The influence of simulated masticatory loading regimes on the bi-axial flexure strength and reliability of a Y-TZP dental ceramic

被引:48
|
作者
Curtis, Andrew R.
Wright, Adrian J.
Fleming, Garry J. P.
机构
[1] Dublin Dent Sch & Hosp, Dept Restorat Dent & Periodontol, Dublin 2, Ireland
[2] Univ Birmingham, Sch Dent, Biomat Unit, Birmingham B4 6NN, W Midlands, England
[3] Univ Birmingham, Sch Chem, Birmingham B15 2TT, W Midlands, England
关键词
Y-TZP; zirconia; CAD/CAM; Weibull analysis; bi-axial flexure strength; simulated masticatory loading; Vickers hardness;
D O I
10.1016/j.jdent.2005.07.009
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: The purpose of the current study was to examine the influence of simulated masticatory loading regimes, to which all-ceramic crown or bridge restorations will routinely be subjected during their service-life, on the performance of a yttria-stabilised tetragonal zirconia polycrystalline (Y-TZP) dental ceramic. Methods: Ten sets of 30 Y-TZP ceramic discs (13 mm diameter, 1.48-1.54 mm thickness) supplied by the manufacturer were randomly selected. Six groups were loaded for 2000 cycles at 500 N (383-420 MPa), 700N (536-588 MPa) and 800 N (613672 MPa) with three groups maintained dry and the remaining three groups loaded while immersed in water at 37+/-1 degrees C. A further two groups underwent extended simulated masticatory loading regimes at 80 N (61-67 MPa) for 104 and 1 05 cycles under dry conditions. The mean bi-axial flexure strengths, standard deviations and dssociated Weibull moduli (m) were determined. The surface hardness was also determined using the Vickers hardness indentation technique. Results: No significant difference (P>0.05) was identified in the bi-axial flexure strength of the simulated masticatory loading regimes and the control specimens loaded dry or wet. A significant increase in m was identified for the Y-TZP specimens following loading while immersed in water (8.6+/-1.6, 8.5 +/- 1.6 and 10.3 +/- 1.9) compared with the control (7.1 +/- 1.3). However, the extended loading regime to 105 cycles resulted in a significant reduction in the m of the Y-TZP specimens (5.3 +/- 1.0) compared with the control. Localised areas of increased surface hardness were identified to occur directly beneath the spherical indenter. Conclusions: The occurrence of localised areas of increased surface hardness could be the result of either a transformation toughening mechanism or crushing and densification of the material beneath the indentor manifested as the formation of a surface layer of compressive stresses that counteracted the tensile field generated at the tip of a propagating crack which increased the Weibull modulus of the Y-TZP specimens. The reduced reliability of the Y-TZP specimens loaded to 80 N for 10(5) cycles was associated with the accumulation of subcritical damage as a result of the extended nature of loading. (C) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:317 / 325
页数:9
相关论文
共 23 条
  • [21] An assessment of the influence of mixing induced variability on the bi-axial flexure strength of dentine porcelain discs and the implications for laboratory testing of porcelain specimens
    Fleming, GJP
    Shaini, FJ
    Marquis, PM
    DENTAL MATERIALS, 2000, 16 (02) : 114 - 119
  • [22] Fracture strength of all-ceramic (Y-TZP) three- and four-unit fixed dental prostheses with different connector design and production history
    Mahmood, Deyar Jallal Hadi
    Linderoth, Ewa H.
    von Steyern, Per Vult
    Wennerberg, Ann
    SWEDISH DENTAL JOURNAL, 2013, 37 (04) : 179 - 188
  • [23] Influence of nano-structured alumina coating on shear bond strength between Y-TZP ceramic and various dual-cured resin cements
    Lee, Jung-Jin
    Choi, Jung-Yun
    Seo, Jae-Min
    JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (02): : 130 - 137