摘要
An indentation technique using a conventional Vickers microhardness tester was used to evaluate fatigue properties of lead-alkali and soda-lime silica glasses. The specimens were indented repeatedly at the same point with subcritical loads until radial cracks were initiated. The number of cycles to initiate the cracks at different subcritical loads demonstrated typical fatigue curves for both glasses. The uniqueness of the experiment was that the diagonal lengths of the deformed cavity were observed to increase with the number of cycles. This increase of the deformed cavity for a certain number of cycles prior to the visibility of crack initiation was analyzed, correlating the elastic-plastic phenomenon and the accumulation of the residual stress in each cycle.
引用
收藏
页码:2722 / 2724
页数:3
相关论文
共 50 条
  • [21] Quantification of crack volumes in dynamically damaged soda-lime glass
    Bauer, Steffen
    Butz, Ines
    Strassburger, Elmar
    Sauer, Martin
    Hiermaier, Stefan
    GLASS STRUCTURES & ENGINEERING, 2022, 7 (04) : 569 - 602
  • [22] Statistical analysis of fracture toughness of soda-lime glass determined by indentation
    Gong, JH
    Chen, YF
    Li, CY
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2001, 279 (2-3) : 219 - 223
  • [23] Quantification of crack volumes in dynamically damaged soda-lime glass
    Steffen Bauer
    Ines Butz
    Elmar Strassburger
    Martin Sauer
    Stefan Hiermaier
    Glass Structures & Engineering, 2022, 7 : 569 - 602
  • [24] Internal friction at crack tip of soda-lime silicate glass
    Huang, Zhenhan
    Tomozawa, Minoru
    JOURNAL OF NON-CRYSTALLINE SOLIDS-X, 2025, 25
  • [25] Prevention of exit crack in mirco drilling of soda-lime glass
    Park, BJ
    Choi, YJ
    Chu, CN
    CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2002, 51 (01): : 347 - 350
  • [26] INFLUENCE OF WATER VAPOR ON CRACK PROPAGATION IN SODA-LIME GLASS
    WIEDERHORN, SM
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1967, 50 (08) : 407 - +
  • [27] ENVIRONMENTALLY ENHANCED CRACK-GROWTH IN SODA-LIME GLASS
    FREIMAN, SW
    WHITE, GS
    FULLER, ER
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (03) : 108 - 112
  • [28] INFLUENCE OF WATER VAPOR ON CRACK PROPAGATION IN SODA-LIME GLASS
    WIEDERHO.SM
    AMERICAN CERAMIC SOCIETY BULLETIN, 1966, 45 (04): : 433 - &
  • [29] The analysis of soda-lime glass
    Lundell, GEF
    Knowles, HB
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1927, 10 (11) : 829 - 849
  • [30] HYDRATION OF SODA-LIME GLASS
    LANFORD, WA
    DAVIS, K
    LAMARCHE, P
    LAURSEN, T
    GROLEAU, R
    DOREMUS, RH
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1979, 33 (02) : 249 - 266