Mechanical behavior and failure analysis of granite specimens containing two orthogonal fissures under uniaxial compression

被引:17
|
作者
Yin, Qian [1 ,2 ]
Jing, Hongwen [1 ]
Zhu, Tantan [1 ]
机构
[1] China Univ Min & Technol, State Key Lab Geomech & Deep Underground Engn, Xuzhou 221116, Peoples R China
[2] Univ Western Australia, Sch Civil Environm & Min Engn, Perth, WA 6009, Australia
关键词
Brittle granite; Two orthogonal fissures; Virtual ligament length; Mechanical behavior; Crack initiation stress; Crack coalescence; CRACK-PROPAGATION; COALESCENCE BEHAVIOR; FINITE-ELEMENTS; BRITTLE ROCKS; SANDSTONE; FLAWS; STRESS; MARBLE; GROWTH;
D O I
10.1007/s12517-015-2078-y
中图分类号
P [天文学、地球科学];
学科分类号
07 ;
摘要
The mechanical behavior, crack initiation stress, cracking modes, and crack coalescence process due to uniaxial compressive loading for brittle granite specimens (70x 140x29 mm in size) containing two orthogonal fissures with different "virtual ligament length" were first modeled experimentally. Intact granite specimens present typical axial splitting failure, and the ultimate failure of specimens containing a single fissure results mainly from tensile cracks initiated from the fissure tips. Basically, mechanical parameters of granite specimens containing two orthogonal fissures are lower than the values for intact specimens, and the reduction extent is distinctly related to the virtual ligament length. The uniaxial compressive strength, peak axial strain, Young's modulus, secant Young's modulus, and crack initiation stress of granite specimens containing two orthogonal fissures present the same trend with the increasing virtual ligament length, i.e., first decrease and then increase, finally once again decrease. The effect of virtual ligament length on the crack initiation type and ultimate failure modes of granite specimens containing two orthogonal fissures is analyzed. Crack types based on the fissure geometry and crack propagation mechanism are identified, and three different crack initiation types are summarized. The crack coalescence is observed and characterized from tips of pre-existing fissures. Relation between the real-time cracking process and axial stress-strain curves of granite specimens containing two orthogonal fissures for the entire deformation process is captured, and the corresponding axial stress for crack coalescence is also obtained. Each sharp stress drop in axial stress-strain curves indicates an obvious crack coalescence.
引用
收藏
页码:1 / 15
页数:15
相关论文
共 50 条
  • [41] Experimental study of the mechanical behavior of unfilled rough jointed specimens under uniaxial compression
    Tian, Wen-Ling
    Yang, Sheng-Qi
    Hu, Zhao-Liang
    Lu, Jia-Wei
    ARABIAN JOURNAL OF GEOSCIENCES, 2020, 13 (04)
  • [42] Experimental study of the mechanical behavior of unfilled rough jointed specimens under uniaxial compression
    Wen-Ling Tian
    Sheng-Qi Yang
    Zhao-Liang Hu
    Jia-Wei Lu
    Arabian Journal of Geosciences, 2020, 13
  • [43] Experimental Study of Mechanical and Permeability Behaviors During the Failure of Sandstone Containing Two Preexisting Fissures Under Triaxial Compression
    Du, Yiteng
    Li, Tingchun
    Li, Weiteng
    Ren, Yande
    Wang, Gang
    He, Peng
    ROCK MECHANICS AND ROCK ENGINEERING, 2020, 53 (08) : 3673 - 3697
  • [44] Experimental Study of Mechanical and Permeability Behaviors During the Failure of Sandstone Containing Two Preexisting Fissures Under Triaxial Compression
    Yiteng Du
    Tingchun Li
    Weiteng Li
    Yande Ren
    Gang Wang
    Peng He
    Rock Mechanics and Rock Engineering, 2020, 53 : 3673 - 3697
  • [45] Analysis of Granite Failure Modes and Energy Conversion under Uniaxial Compression at Various Temperatures
    Shah, Kausar Sultan
    Abbas, Naeem
    Kegang, Li
    Hashim, Mohd Hazizan bin Mohd
    Rehman, Hafeezur
    Jadoon, Khan Gul
    JOURNAL OF MINING AND ENVIRONMENT, 2023, 14 (02): : 493 - 506
  • [46] Mechanical properties and failure mechanism of concrete-granite composite specimens under compression load
    Dong, Zhuo
    Lin, Tianran
    Tang, Shibin
    Lang, Yingxian
    Yuan, Ruifu
    Heng, Shuai
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 435
  • [47] Mechanical behavior of sandstone containing double circular cavities under uniaxial compression
    State Key Laboratory for Geomechanics & Deep Underground Engineering, China University of Mining & Technology, Xuzhou
    221116, China
    Yantu Gongcheng Xuebao, 6 (1047-1056):
  • [48] Mechanical properties and fracture evolution of sandstone specimens containing different inclusions under uniaxial compression
    Zhu, Quanqi
    Li, Diyuan
    Han, Zhenyu
    Li, Xibing
    Zhou, Zilong
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2019, 115 (33-47) : 33 - 47
  • [49] Crack evolution of soft–hard composite layered rock-like specimens with two fissures under uniaxial compression
    Dong ZHOU
    Yicheng YE
    Nanyan HU
    Weiqi WANG
    Xianhua WANG
    Frontiers of Structural and Civil Engineering, 2021, (06) : 1372 - 1389
  • [50] Effect of thermal shock on the strength and fracture behavior of pre-flawed granite specimens under uniaxial compression
    Huang, Yan-Hua
    Yang, Sheng-Qi
    Bu, Yi-Shun
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2020, 106