Interfacial tensions between CaO-SiO2-Al2O3 slag and Fe-O-S, Fe-Si, Fe-Al, Fe-C, Fe-Cr or Fe-Ni alloys

被引:0
|
作者
Sun, HP
Yoneda, N
Nakashima, K
Mori, K
机构
关键词
interfacial tension; CaO-SiO2-Al2O3; slag; flux; iron alloy; adsorption of active element;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The interfacial tensions of 35mass%CaO-35mass%SiO2-30mass%Al2O3 slag with Fe-O-S, Fe-Si, Fe-Al, Fe-C, Fe-Cr or Fe-Ni alloys were investigated at 1580 degrees C by the sessile drop method. The interfacial tension for Fe-O-S system decreased with increasing oxygen and/or sulfur contents and their values (sigma) with oxygen and sulfur activities (a) were found to follow the relation, sigma(0)-sigma=0.3241n(1+116a(0)+8.5a(s)) ([S] <1mass%) In evaluating the effect of each alloying element on the interfacial tension, the difference in the oxygen content in each alloy was taken in the consideration. The interfacial tension was increased with increasing aluminum and silicon contents, slightly decreased with increasing carbon or nickel contents, and markedly decreased with increasing sulfur and chromium contents in the melt.
引用
收藏
页码:1 / 6
页数:6
相关论文
共 50 条
  • [41] INFLUENCE OF A MIXED AL2O3 + CR2O3 SUPERFICIAL COATING ON THE NONISOTHERMAL OXIDATION BEHAVIOR OF FE ALLOYS AND FE-CR ALLOYS
    MITRA, SK
    ROY, SK
    BOSE, SK
    OXIDATION OF METALS, 1992, 37 (1-2): : 95 - 108
  • [42] SURFACE TENSIONS OF LIQUID FE-NI, FE-CO AND NI-CO BINARY-ALLOYS AND WETTABILITY OF AL2O3
    OGINO, K
    TAIMATSU, H
    NAKATANI, F
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1982, 46 (11) : 1049 - 1054
  • [43] PHASE RELATIONS IN SYSTEM CAO-AL2O3-SIO2-FE-O .2. SYSTEM CAO-AL2O3-FE2O3-SIO2
    SORRENTINO, FP
    GLASSER, FP
    TRANSACTIONS AND JOURNAL OF THE BRITISH CERAMIC SOCIETY, 1976, 75 (05): : 95 - 103
  • [44] Effect of magnetism on short-range order formation in Fe-Si and Fe-Al alloys
    Gorbatov, Oleg I.
    Gornostyrev, Yuri N.
    Kuznetsov, Andrey R.
    Ruban, Andrei V.
    SOLID-SOLID PHASE TRANSFORMATIONS IN INORGANIC MATERIALS, PTS 1-2, 2011, 172-174 : 618 - +
  • [45] Phase compatibility in the systems CaO-SiO2-Fe2O3-SO3, CaO-Al2O3-Fe2O3-SO3 and SiO2-Al2O3-Fe2O3-SO3
    Strigác, J
    Sahu, S
    Majling, J
    CERAMICS-SILIKATY, 1998, 42 (04) : 141 - 149
  • [46] On the in situ synthesis of (Fe,Cr)Al and (Fe,Cr)Al-Al2O3 nanostructured materials
    Sourani, F.
    Enayati, M. H.
    Ngan, A. H. W.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [47] Numerical analysis on Si deoxidation of molten Fe, Ni, Fe-Ni, Fe-Cr, Fe-Cr-Ni, Ni-Cu and Ni-Co alloys by quadratic formalism
    Miki, T
    Hino, M
    ISIJ INTERNATIONAL, 2005, 45 (12) : 1848 - 1855
  • [48] Fe16Al14B2 phase in Fe-Al alloys
    Chisholm, MF
    Duscher, G
    Pang, LX
    Kumar, KS
    PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 2000, 80 (11): : 2737 - 2745
  • [49] NITROGENATION OF FE-AL ALLOYS .2. ADSORPTION AND SOLUTION OF NITROGEN IN NITROGENATED FE-AL ALLOYS
    PODGURSKI, HH
    ORIANI, RA
    DAVIS, FN
    LI, JCM
    CHOU, YT
    TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1969, 245 (07): : 1603 - +
  • [50] Fe-Si Intermetallics/Al2O3 Composites Formed between Fe-20% Si and Fe-70.5% Si by SHS Metallurgy Method
    Yeh, Chun-Liang
    Lu, Ann
    Liang, Wei-Che
    METALS, 2022, 12 (08)