Effect of ultrasonic vibration on the wetting behavior of molten tin on copper substrate

被引:5
|
作者
Sun, Xuemin [1 ]
Yu, Weiyuan [1 ]
Wang, Fengfeng [1 ]
Wang, Yanhong [2 ]
机构
[1] Lanzhou Univ Technol, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Peoples R China
[2] Lanzhou Univ Technol, Sch Civil Engn, Lanzhou 730050, Peoples R China
基金
中国国家自然科学基金;
关键词
CU; SN; DEFORMATION; MORPHOLOGY; INTERFACE; ALLOYS;
D O I
10.1007/s10854-020-04882-7
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The wetting behavior of molten tin solder on copper substrate under ultrasonic vibrations was investigated by the wetting balance method at 250 degrees C. The cross-section morphology and microstructure of the specimen were analyzed after the wetting test. The grain size and thickness of intermetallic compounds (IMCs) at the interface were measured by an image-pro software. The ultrasonic sound pressure distribution in the molten tin solder was simulated by finite element analysis. The results showed significant effect of ultrasonic vibrations on the wettability of the molten tin solder on the copper substrate. The wettability was conjunctively determined by the driving and additional forces caused by an interfacial reaction and acoustic streaming, respectively. Acoustic cavitation expedited the interaction of interfacial atoms and facilitated the interfacial reaction, resulting in an increased driving force that contributed to the spreading of the molten tin solder on the copper substrate.
引用
收藏
页码:1073 / 1079
页数:7
相关论文
共 50 条
  • [21] Spreading and wetting behavior of al-based brazing filler metal on TiNi shape memory alloy substrate by coupled effect of ultrasonic vibration and laser heating
    Li H.
    Tao B.-H.
    Li Z.-X.
    Guo F.
    Li, Hong (hongli@bjut.edu.cn), 1600, Beijing Institute of Aeronautical Materials (BIAM) (44): : 66 - 71
  • [22] EFFECT OF VIBRATION ON THE SOLIDIFICATION OF COPPER-TIN ALLOYS
    SARKAR, S
    BANERJEE, MK
    SEAL, AK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1985, 38 (02): : 139 - 146
  • [23] Effect of nano-metallic coating on the wetting of silicon by molten tin at 800 °C
    Lin, Qiaoli
    Lai, Jinxin
    SURFACE & COATINGS TECHNOLOGY, 2024, 492
  • [24] Wetting Behavior of Carbon in Molten Carbonate
    Chen, Chia-Chin
    Maruyama, Toru
    Hsieh, Ping-Hsun
    Selman, J. Robert
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2012, 159 (10) : D597 - D604
  • [25] The wetting and spontaneous infiltration of ceramics by molten copper
    A. R. Kennedy
    J. D. Wood
    B. M. Weager
    Journal of Materials Science, 2000, 35 : 2909 - 2912
  • [26] The wetting and spontaneous infiltration of ceramics by molten copper
    Kennedy, AR
    Wood, JD
    Weager, BM
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (12) : 2909 - 2912
  • [27] EFFECT OF SODIUM SULFIDE ON REMOVAL OF COPPER AND TIN FROM MOLTEN IRON
    LIU, X
    JEFFES, JHE
    IRONMAKING & STEELMAKING, 1985, 12 (06) : 293 - 294
  • [28] Effects of direct current on the wetting behavior and interfacial morphology between molten Sn and Cu substrate
    Gu, Yan
    Shen, Ping
    Yang, Nan-Nan
    Cao, Kang-Zhan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 586 : 80 - 86
  • [30] Instrument to characterize the wetting behavior of molten metal on a solid substrate under high magnetic field
    Xiao, Yubao
    Liu, Tie
    Lu, Zhengyang
    Yuan, Shuang
    Li, Guojian
    Dong, Shulin
    Wang, Qiang
    REVIEW OF SCIENTIFIC INSTRUMENTS, 2019, 90 (06):