Corrosion of a 3D-C/SiC composite in salt vapor environments

被引:23
|
作者
Cheng, LF [1 ]
Xu, YD [1 ]
Zhang, LT [1 ]
Luan, XG [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
carbon composites; oxidation; activation energy;
D O I
10.1016/S0008-6223(01)00203-2
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Corrosion behavior of the three-dimensional C/SiC composite was investigated in a Na2SO4 vapor environment at temperatures from 1000 to 1500degreesC. The degradation mechanisms for the C/SiC composite could be determined by dividing a complicated function describing the weight change of the composite with temperature into several monotone functions describing the mechanisms, and then identified by the strength change of the composite with temperature. There were three reactions between the C/SiC composite and the Na2SO4 vapor. The First one was the passive oxidation of the CND SiC, leading a small weight gain. The second one was the oxidation of the carbon phases, leading a small weight loss. The third one was the active oxidation of the CVD SiC, leading a large weight loss. The threshold temperature for these reactions was, respectively, 1080, 1100 and 1300degreesC. The transition temperature from passive to active was 1200degreesC. The activation energy for these reactions was, respectively, calculated by the weight chance with temperature to be 114, 105 and 112 kcal/mol. The flexural strength loss of the composite reached its minimum value when the weight gain of the composite reached its maximum value at 1200degreesC. Below 1200degreesC, the C/SiC composite had a higher corrosion resistance to the Na2SO4 vapor. Above 1300degreesC, the poor corrosion resistance of the CVD SiC made the composite having a poor corrosion resistance to the Na2SO4 vapor. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:877 / 882
页数:6
相关论文
共 50 条
  • [31] Oxidation behavior from room temperature to 1500°C of 3D-C/SiC composites with different coatings
    Cheng, Laifei
    Xu, Yongdong
    Zhang, Litong
    Yin, Xiaowei
    1600, American Ceramic Society (85):
  • [32] Oxidation behavior from room temperature to 1500°C of 3D-C/SiC composites with different coatings
    Cheng, LF
    Xu, YD
    Zhang, LT
    Yin, XW
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (04) : 989 - 991
  • [33] 热处理对3D-C/PyC/SiC力学性能的影响
    董宁
    张立同
    徐永东
    成来飞
    范尚武
    固体火箭技术, 2008, (02) : 188 - 192+197
  • [34] PROCESSING AND FRICTION PROPERTIES OF 3D-C/C-SiC MODEL COMPOSITES WITH A MULTILAYERED C-SiC MATRIX ENGINEERED AT THE NANOMETER SCALE
    Fillion, A.
    Naslain, R.
    Pailler, R.
    Bourrat, X.
    Robin-Brosse, C.
    Brendle, M.
    DEVELOPMENTS IN ADVANCED CERAMICS AND COMPOSITES, 2005, 26 (08): : 179 - 186
  • [35] Biaxial testing of 3D-C/C composite materials by a special frame system on universal tester
    Guanhu, H.
    Hongyu, F.
    Heng, W.
    Shuqing, D.
    Zihua, Z.
    Benlian, Z.
    1993, 6
  • [36] Corrosion of Si, C, and SiC in molten salt
    Xi, Jianqi
    Jiang, Hao
    Liu, Cheng
    Morgan, Dane
    Szlufarska, Izabela
    CORROSION SCIENCE, 2019, 146 : 1 - 9
  • [37] Corrosion of C/SiC composite in water vapor and Na2SO4 vapour
    Dong, Ning
    Luan, Xin'gang
    Cheng, Laifei
    SCIENCE AND ENGINEERING OF COMPOSITE MATERIALS, 2008, 15 (02): : 121 - 129
  • [38] Bending damage behavior of 3D-C/C-TiC-Cu composite based on acoustic emission technology
    Wang, Xianghong
    Dong, Xinlei
    Tong, Yonggang
    Hu, Hongwei
    Liu, Wenzheng
    APPLIED ACOUSTICS, 2024, 220
  • [39] 加载速率对3D-C/SiC不同温度拉伸性能的影响
    罗国清
    乔生儒
    材料工程, 2003, (10) : 9 - 10+39
  • [40] 预疲劳对3D-C/SiC复合材料拉伸性能的影响
    杜双明
    西安科技大学学报, 2009, 29 (01) : 97 - 100