Effect of Quenching Medium on the Microstructure of Hot Rolled Ti-6Al-6Nb Alloy for Medical Application

被引:3
|
作者
Sutowo, Cahya [1 ]
Alhamidi, A. Ali [2 ]
Basir, Muh Idrus Abdul [2 ]
Rokhmanto, Fendy [1 ]
机构
[1] Indonesia Inst Sci, Res Ctr Met & Mat, Kawasan Puspiptek, Gd 470, Thngerang Selatan, Indonesia
[2] Univ Sultan Ageng Tirtayasa, Fac Engn, Dept Met & Mat, Cilegon, Banten, Indonesia
关键词
D O I
10.1063/1.5038327
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The Ti-6Al-6Nb alloy has been used as hone plate in biomedical application. But, its modulus elasticity still lies above its cortical-bone, which causes stress shielding. An alternative process for reduce modulus of elasticity by means of treatment solutions with heating beta-transus temperature follows with rapid cooling for obtaining high % intensity of beta-phase fractions. In this study the Ti-6Al-6Nb as-cast alloys were homogenized at 1050 degrees C for 12 hours, then hot rolled with a reduction 60% (from 10mm to 4 mm thickness) at 1000 degrees C and then dissolved at 1100 degrees C for 2 hours and then cooled by water, oil and air. The microstructural observations were performed with OM and SEM-EDS. The phase analyzes were observed by XRD test and mechanical properties observed by Ultrasonic test. The observation result shows the elasticity modulus value in alloys which being ST with cooling is 106,71 GPa. This is consistent with the observation of the microstructure that the presence of beta-transformed and it is also in accordance with the XRD analysis and the intensity of the phase fraction, where the peak and% intensity of the beta (35%) phase fraction increase in alloys which ST and oil quench.
引用
收藏
页数:8
相关论文
共 50 条
  • [31] On restructuring the microstructure of Ti-6Al-7Nb alloy before surface engineering
    Shen, Xiaojun
    Shukla, Pratik
    Sharma, Deepak
    Zammit, Ann
    Swanson, Philip
    Jiao, Yang
    Lawrence, Jonathan
    MATERIALS CHARACTERIZATION, 2020, 169
  • [32] Microstructure and properties of composite polyetheretherketone/Bioglass® coatings deposited on Ti-6Al-7Nb alloy for medical applications
    Moskalewicz, Tomasz
    Seuss, Sigrid
    Boccaccini, Aldo R.
    APPLIED SURFACE SCIENCE, 2013, 273 : 62 - 67
  • [33] Effect of Al content on the hot deformation behavior and microstructure evolution of TiAl-6(Cr, Nb, Ta) alloy
    Liu, Hongwu
    Gao, Fan
    Feng, Xiangzheng
    Li, Zhenxi
    MATERIALS RESEARCH EXPRESS, 2020, 7 (07)
  • [34] The effect of Nb and Si on the hot corrosion behaviors of TiAl coatings on a Ti-6Al-4V alloy
    Dai, Jingjie
    Zhang, Hongxia
    Sun, Caixia
    Li, Shouying
    Chen, Chuanzhong
    Yang, Yong
    CORROSION SCIENCE, 2020, 168
  • [35] Effect of microstructure on small fatigue crack initiation and propagation characteristics of Ti-6Al-7Nb alloy
    Toyohashi Univ of Technology, Toyohashi, Japan
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1998, 62 (10): : 952 - 960
  • [36] Effect of microstructure on small fatigue crack initiation and propagation characteristics of Ti-6Al-7Nb alloy
    Akahori, T
    Niinomi, M
    Ozeki, A
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1998, 62 (10) : 952 - 960
  • [37] Effect of LaB6 on the microstructure evolution and mechanical properties of Ti-45Al-8Nb alloy
    Fang, Yingchun
    Jin, Kaihang
    Liu, Cheng
    Wang, Haiwen
    Wei, Xiao
    Ding, Qingqing
    Bei, Hongbin
    Zhao, Xinbao
    Zhang, Ze
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 938
  • [38] INFLUENCE OF INITIAL MICROSTRUCTURE ON HOT WORKABILITY OF Ti-6Al-4V ALLOY
    Yeom, Jong-Taek
    Kim, Jeoung Han
    Hong, Jae-Keun
    Park, Nho-Kwang
    Lee, Chong Soo
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2009, 23 (6-7): : 808 - 813
  • [39] Effect of Growth Rate on Microstructure Evolution and Hardness in Directionally Solidified Ti-50Al-6Nb Alloy
    Liu Guohuai
    Zhang Yuan
    Li Xinzhong
    Chen Ruirun
    Su Yanqing
    Guo Jingjie
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (07) : 1655 - 1660
  • [40] Microstructure of Hot Isostatically Pressed Ti-6Al-4V Alloy after Hot Deformation
    Zhang Zhimin
    Ren Luying
    Xue Yong
    Wu Yaojin
    Wang Qiang
    Xu Jian
    Zhang Huifang
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (03) : 820 - 826