Protection of γ-based TiAl against high temperature oxidation using ion implantation of chlorine

被引:22
|
作者
Hornauer, U
Günzel, R
Reuther, H
Richter, E
Wieser, E
Möller, W
Schumacher, G
Dettenwanger, F
Schütze, M
机构
[1] Forschungszentrum Rossendorf EV, FWII, D-01314 Dresden, Germany
[2] DECHEMA eV, Karl Winnacker Inst, D-60486 Frankfurt, Germany
来源
SURFACE & COATINGS TECHNOLOGY | 2000年 / 125卷 / 1-3期
关键词
chlorine; implantation; oxidation; plasma immersion; TiAl;
D O I
10.1016/S0257-8972(99)00544-7
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of ion beam implantation and plasma immersion ion implantation of chlorine on the high temperature oxidation of titanium aluminides above 800 degrees C in air was investigated. Thermogravimetric oxidation tests (TGA) were performed to examine the long term protection. Depth profiling with Auger electron spectroscopy (AES) was used to investigate Cl diffusion and oxide formation during the first stage of oxidation. A microscopic model of the 'Cl-effect' will be discussed. A systematic variation of the implantation energy and fluence shows that there is a narrow regime of Cl concentration for optimum protective effect. The time to form a protective Al2O3 layer depends on the local Cl concentration. The oxidation rate after this incubation time is reduced by about two orders of magnitude compared to untreated Ti50Al and is nearly independent of the fluence. The implantation energy is not a sensitive parameter because the implanted chlorine profile changes very quickly during high temperature oxidation. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:89 / 93
页数:5
相关论文
共 50 条
  • [21] Influence of Nb-ion implantation upon high temperature oxidation behavior of γ-TiAl under thermal cycling condition
    Wang, W
    Zhang, YG
    Ji, V
    Shi, JY
    Chen, CQ
    GAMMA TITANIUM ALUMINIDES 1999, 1999, : 799 - 804
  • [22] High temperature oxidation behaviour of TiAl-based intermetallics
    Stroosnijder, MF
    Sunderkotter, JD
    Haanappel, VAC
    DESIGN FUNDAMENTALS OF HIGH TEMPERATURE COMPOSITES, INTERMETALLICS, AND METAL-CERAMICS SYSTEMS, 1996, : 287 - 293
  • [23] The improvement of the oxidation resistance of TiAl alloys by fluorine plasma-based ion implantation
    Zhu, YC
    Li, XY
    Fujita, K
    Iwamoto, N
    Matsunaga, Y
    Nakagawa, K
    Taniguchi, S
    SURFACE & COATINGS TECHNOLOGY, 2002, 158 : 503 - 507
  • [24] The effect of niobium ion implantation on the oxidation behavior of a gamma-TiAl-based intermetallic
    Stroosnijder, MF
    Zheng, N
    Quadakkers, WJ
    Hofman, R
    Gil, A
    Lanza, F
    OXIDATION OF METALS, 1996, 46 (1-2): : 19 - 35
  • [25] Influence of ion implantation of several elements on oxidation behavior of TiAl
    Yoshihara, M.
    Taniguchi, S.
    Furumaki, D.
    Aono, M.
    HIGH-TEMPERATURE OXIDATION AND CORROSION 2005, 2006, 522-523 : 633 - 640
  • [26] Effect of Nb-ion implantation on the oxidation resistance of TiAl
    Taniguchi, S
    Shibata, T
    Saeki, T
    Zhang, HX
    Liu, XH
    MATERIALS TRANSACTIONS JIM, 1996, 37 (05): : 998 - 1003
  • [27] The Use of Fluorine to Protect β-Solidifying γ-TiAl-Based Alloys against High-Temperature Oxidation
    Alexander Donchev
    Mathias Galetz
    Svea Mayer
    Helmut Clemens
    Michael Schütze
    MRS Advances, 2017, 2 (25) : 1361 - 1367
  • [28] Improvement of the oxidation resistance of gamma titanium aluminides by microalloying with chlorine using ion implantation
    Schumacher, G
    Lang, C
    Schütze, M
    Hornauer, U
    Richter, E
    Wieser, E
    Möller, W
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1999, 50 (03): : 162 - 165
  • [29] Improvement of the oxidation resistance of TiAl alloys by using the chlorine effect
    Karl-Winnacker-Inst der DECHEMA e.V., Frankfurt am Main, Germany
    Mater Sci Eng A Struct Mater Prop Microstruct Process, (847-858):
  • [30] Improvement of the oxidation resistance of TiAl alloys by using the chlorine effect
    Schutze, M
    Hald, M
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 240 : 847 - 858