In-Situ saxs/waxd analysis on structural evolution in peek irradiated by 1 MeV electrons during tensile deformation

被引:3
|
作者
Li, Hongxia [1 ]
Yang, Jianqun [1 ]
Lv, Gang [1 ]
Dong, Saisai [1 ]
Tian, Feng [2 ]
Dong, Shangli [1 ]
Li, Xingji [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Chinese Acad Sci, Shanghai Adv Res Inst, Zhangjiang Lab, Shanghai Synchrotron Radiat Facil, Shanghai 201204, Peoples R China
基金
中国国家自然科学基金;
关键词
Peek; Electron irradiation; Mechanical property; Saxs; WAXD; MECHANICAL-PROPERTIES; POLYETHERETHERKETONE PEEK; POLYETHYLENE; STRAIN; SAXS; FILM;
D O I
10.1016/j.polymdegradstab.2020.109350
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polyether ether ketone (PEEK) is widely used as an electrical insulation material in aerospace field due to its excellent thermal and electrical properties. The changes in micro structure of the PEEK irradiated by 1 MeV electrons are studied by in-situ analysis of synchronous small-angle X-ray scattering (SAXS) and wide-angle X-ray diffraction (WAXD) during tensile deformation at room temperature. The tensile strength and the elongation at break of the irradiated PEEK decrease obviously, which is compared with the pristine one. The differential scanning calorimetry (DSC) analysis shows that the pristine PEEK begins to melt at 334.8 degrees C, the melting peak T-n, appears at 339.7 degrees C and a deeper exothermic crystallization peak T-n appears at 297.8 degrees C during the cooling process. The crystallization peak temperature decreases with the increase of the irradiation fluences. The pristine PEEK has a significant scattering peak along the meridian direction of the SAXS pattern, which indicates that the crystal lamellae of the material exhibits a certain orientation, and the position of the scattering peak changes little after irradiation. The intensity of SAXS decreases with the increasing of stretching strains, and the descent rate increases with the increasing of the irradiation fluences. According to the WAXD analysis, the width at half height of the diffraction peak increases with the increasing of the stretching strain, and the peak tends to disappear during tensile deformation. The diffraction peak disappearance rate increases with the increasing of the irradiation fluences. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:11
相关论文
共 31 条
  • [21] An investigation on microstructure evolution and deformation mechanism of Ti-5Al-5Mo-5V-1Cr-1Fe alloy during in-situ tensile
    Li, Wei
    Wang, Lei
    Wang, Jinhui
    Jin, Peipeng
    Luan, Shiyu
    Li, Deqing
    Zhu, Lin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 489 - 502
  • [22] Structural evolution of poly(ether-b-amide12) elastomers during uniaxial drawing studied using in-situ synchrotron WAXS and SAXS
    Park, Soo-Young
    Kamal, Tahseen
    Chang, Young-Wook
    ACTA CRYSTALLOGRAPHICA A-FOUNDATION AND ADVANCES, 2011, 67 : C260 - C260
  • [23] In-situ analysis of microstress and texture development during tensile deformation of MMCs at room temperature and at elevated temperatures using synchrotron radiation
    Pyzalla, A
    Reetz, B
    Wegener, J
    Jacques, A
    Ferry, O
    Feiereisen, JP
    Buslaps, T
    ECRS 6: PROCEEDINGS OF THE 6TH EUROPEAN CONFERENCE ON RESIDUAL STRESSES, 2002, 404-7 : 535 - 540
  • [24] Synchrotron X-ray line-profile analysis experiments for the in-situ microstructural characterisation of SPD nanometals during tensile deformation
    Kerber, Michael B.
    Schafler, Erhard
    Wieczorek, Arkadiusz K.
    Ribarik, Gabor
    Bernstorff, Sigrid
    Ungar, Tamas
    Zehetbauer, Michael J.
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2009, 100 (06) : 770 - 774
  • [25] Analysis of the dynamic evolution behavior of radial deformation and cracks during in-service welding instability based on quasi-in-situ and in-situ experiments
    Han, Tao
    Han, Laihui
    Wu, Qian
    Xu, Shikai
    Sun, Jianbo
    Wang, Yong
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2023, 206
  • [26] Bayesian analysis reveals the impact of load partitioning on microstructural evolution in Ti-6Al-4V during in-situ tensile loading
    Armstrong, N.
    Lynch, P. A.
    Cizek, P.
    Kada, S. R.
    Slater, S.
    Antoniou, R. A.
    MATERIALIA, 2021, 15
  • [27] Structural evolution of cellulose triacetate film during stretching deformation: An in-situ synchrotron radiation wide-angle X-Ray scattering study
    An, Minfang
    Zhang, Qianlei
    Ye, Ke
    Lin, Yuanfei
    Wang, Daoliang
    Chen, Wei
    Yin, Panchao
    Meng, Lingpu
    Li, Liangbin
    POLYMER, 2019, 182
  • [28] In-situ X-ray tomography analysis of the evolution of pores during deformation of a Cu-Sn alloy fabricated by selective laser melting
    Samei, Javad
    Amirmaleki, Maedeh
    Ventura, Anthony P.
    Pawlikowski, Gregory T.
    Bayes, Martin
    Misiolek, Wojciech Z.
    Wilkinson, David S.
    ADDITIVE MANUFACTURING, 2020, 34
  • [29] In-situ X-ray tomography analysis of the evolution of pores during deformation of AlSi10Mg fabricated by selective laser melting
    Samei, Javad
    Amirmaleki, Maedeh
    Dastgiri, Mohammad Shirinzadeh
    Marinelli, Carlo
    Green, Daniel E.
    MATERIALS LETTERS, 2019, 255
  • [30] In-situ analysis of the slip activity during tensile deformation of cast and extruded Mg-10Gd-3Y-0.5Zr (wt.%) at 250 °C
    Wang, H.
    Boehlert, C. J.
    Wang, Q. D.
    Yin, D. D.
    Ding, W. J.
    MATERIALS CHARACTERIZATION, 2016, 116 : 8 - 17