Low cycle fatigue behaviour of a ferritic steel strengthened with nano-meter sized precipitates

被引:11
|
作者
Majumdar, S. [1 ]
Gandhi, A. D. [1 ]
Bisht, M. S. [2 ]
机构
[1] Tata Steel Ltd, R&D Div, Jamshedpur 831007, Bihar, India
[2] Natl Inst Technol, Dept Mech Engn, Raipur 492013, Madhya Pradesh, India
关键词
Feeiritic steel; Nanometer-sized precipitates; Low-cycle-Fatigue; Dislocation structure; Coffin-Manson relationship; Microcleavage; COFFIN-MANSON RELATIONSHIP; MECHANICAL-PROPERTIES; GRAIN-SIZE; CROSS-SLIP; MICROSTRUCTURE; DEFORMATION; EVOLUTION; CARBIDES; ALLOYS; SHEETS;
D O I
10.1016/j.msea.2019.04.043
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Low-cycle-fatigue behaviour (Delta epsilon(t)/2 = +/-0.002 to +/-0.01) of a ferritic-steel (tensile strength similar to 800 MPa) strengthened with nano-meter-sized-precipitates has been examined. The selected steel is a hot-rolled Ti-Mo-bearing low-carbon steel (grain size similar to 3 mu m) strengthened predominantly with Ti-Mo-C and Ti-C type precipitates of size <= 30 nm distributed randomly on the grain-boundaries and the matrix. The spread of cyclic-plasticity is negligible in the steel till Delta epsilon(t)/2 = 0.0025 leading to cyclically-stable behaviour and excellent fatigue-life (no failure till 105 loading cycles). At Delta epsilon(t)/2 = 0.003, significant initial-cyclic hardening is noticed followed by minor amount of cyclic-softening. The latter is attributed to formation of low-energy-dislocation-structures e.g. dislocation-walls and channels. At Delta epsilon(t)/2 = 0.004-0.01, predominantly cyclic hardening is noticed till failure; the intensity of hardening increases with increase in Delta epsilon(t)/2. The cyclic-hardening is attributed to increase in dislocation-density and dislocation-precipitate-interaction, formation of subgrains, microbands and dislocation-clusters within both ferrite-grains and microbands. All the above types of dislocation-substructures hinder movement of dislocations and reduce opportunity for cyclic-strain-hardening at Delta epsilon(t)/2 >= 0.004 compared to that at Delta epsilon(t)/2 = 0.002-0.003. This phenomenon leads to two stages of cyclic-hardening with two distinct values of cyclic-strain-hardening-exponents (n(1)' = 0.3 at low Delta epsilon(t)/2 and n(2) = 0.04 at Delta epsilon(t)/2 >= 0.004). Two-stage cyclic-hardening is also reflected in the bilinear Coffin-Manson-relationship and fatigue-fracture. In sharp contrast to fatigue-fracture-surface at Delta epsilon(t)/2 = 0.003, that at Delta epsilon(t)/2 a 0.004 are characterised by multiple-origins of fatigue-crack, absence of fatigue-striations and occurrence of microcleavage/river-pattern indicating faster brittle-fracture at higher Delta epsilon(t)/2.
引用
收藏
页码:198 / 212
页数:15
相关论文
共 50 条
  • [31] Mechanical properties and characteristics of nanometer-sized precipitates in hot-rolled low-carbon ferritic steel
    Xiao-pei Wang
    Ai-min Zhao
    Zheng-zhi Zhao
    Yao Huang
    Liang Li
    Qing He
    International Journal of Minerals Metallurgy and Materials, 2014, 21 (03) : 266 - 272
  • [32] Mechanical properties and characteristics of nanometer-sized precipitates in hot-rolled low-carbon ferritic steel
    Wang, Xiao-pei
    Zhao, Ai-min
    Zhao, Zheng-zhi
    Huang, Yao
    Li, Liang
    He, Qing
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (03) : 266 - 272
  • [33] Low cycle fatigue and cyclic softening behaviour of martensitic cast steel
    Golanski, Grzegorz
    Mrozinski, Stanislaw
    ENGINEERING FAILURE ANALYSIS, 2013, 35 : 692 - 702
  • [34] LOW-CYCLE FATIGUE BEHAVIOUR OF A 5% NICKEL STEEL.
    Ramakrishna Reddy, K.
    Srinivas, M.
    Srinivasa Raghavan, K.
    Radhakrishnan, V.M.
    Transactions of the Indian Institute of Metals, 1984, 37 (04): : 337 - 350
  • [35] Low cycle fatigue behaviour of Grade 92 steel weld joints
    Veerababu, J.
    Goyal, Sunil
    Sandhya, R.
    Laha, K.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 105 : 60 - 70
  • [36] Low-voltage negative-resistance mixers of nano-meter SNS junctions
    Matsui, T
    Ohta, H
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2001, 11 (01) : 191 - 195
  • [37] Low cycle fatigue behaviour of an aluminium alloy with small shearable precipitates: Effect of surface coating
    Khireddine, D
    Khireddine, MH
    INTERNATIONAL JOURNAL OF FATIGUE, 2000, 22 (07) : 585 - 591
  • [38] Fatigue behaviour of ODS ferritic-martensitic Eurofer steel
    Kubena, I.
    Kruml, T.
    Spaetig, P.
    Baluc, N.
    Oksiuta, Z.
    Petrenec, M.
    Obrtlik, K.
    Polak, J.
    FATIGUE 2010, 2010, 2 (01): : 717 - 724
  • [39] Neutron Diffraction Study of Low-Cycle Fatigue Behavior in an Austenitic–Ferritic Stainless Steel
    Ming-Wei Zhu
    Nan Jia
    Feng Shi
    Bj?rn Clausen
    Acta Metallurgica Sinica(English Letters), 2015, 28 (10) : 1247 - 1256
  • [40] Low cycle fatigue behavior of 429EM ferritic stainless steel at elevated temperatures
    Lee, KO
    Yoon, S
    Lee, SB
    Kim, BS
    ADVANCES IN FRACTURE AND FAILURE PREVENTION, PTS 1 AND 2, 2004, 261-263 : 1135 - 1140