Effect of nanocrystallization on sulfur segregation in Fe-Cr-Al alloy during oxidation at 1000°C

被引:12
|
作者
Yang, Songlan
Wang, Fuhui
机构
[1] Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Peoples R China
[2] Univ Saskatchewan, Dept Mech Engn, Saskatoon, SK S7N 5A9, Canada
来源
OXIDATION OF METALS | 2006年 / 65卷 / 3-4期
基金
中国国家自然科学基金;
关键词
nanocrystallization; oxidation; scale adhesion; sulfur segregation;
D O I
10.1007/s11085-006-9014-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
From the 1980's a theory named "the sulfur effect" has been applied to explain the scale adhesion and the reactive-element effect (REE) during high-temperature oxidation. It claims that the bond between the oxide scale and the metal substrate is intrinsically strong and that impurity sulfur in the metal segregates at the oxide scale/substrate interface and weakens the bond, and that REs getter the sulfur impurity and prevent it from segregating to the interface. In the present study, a cast polycrystalline sulfur-containing Fe-25Cr-5Al-1S (wt.%) alloy and its magnetron-sputtered nanocrystalline coating were oxidized at 1000 degrees C, and the specimens were examined by XRD and SEM. The scale formed on the cast alloy was cracked and detached from the substrate even after isothermal exposure, and obvious sulfur enrichment was detectable at the scale/substrate interface. While, the scale formed on the nanocrystalline coating was very adherent after 100 cycles oxidation. Here, sulfur was preferentially distributed in the outer scale and internal oxides rather than at the scale/substrate interface. These results provide evidence that nanocrystallization can prevent sulfur segregation at the scale/substrate interface, hence enhance scale adhesion.
引用
收藏
页码:195 / 205
页数:11
相关论文
共 50 条
  • [41] Kinetics and Mechanism of Sulfur Corrosion of Fe-Cr-Al Alloys.
    Mrowec, Stanislaw
    Wsolek, Malgorzata
    Polska Akademia Nauk, Oddzial W Krakowie, Prace Komisji Metalorgiczno-Odlewniczej, Metalurgia, 1983, (31): : 7 - 55
  • [42] EFFECT OF ALUMINUM IN THERMAL-OXIDATION OF FE-CR-AL CONVERSION COATING FOR CATALYSIS
    ARIES, L
    ROY, J
    NABOULSI, B
    BOUISSOU, T
    SEMPERE, R
    MATERIALS SCIENCE AND TECHNOLOGY, 1991, 7 (08) : 757 - 760
  • [43] Fabrication of Fe-Cr-Al base alloy strips by melt dragging and their oxidation resistance at elevated temperature
    Namkung, J
    Kim, MC
    Park, WW
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 115 (03) : 391 - 395
  • [44] INFLUENCE OF THERMAL CYCLING ON THE OXIDATION BEHAVIOR OF FE-CR-AL AND FE-CR-AL-Y ALLOYS AT 1200-DEGREES-C
    STOTT, FH
    GOLIGHTLY, FA
    WOOD, GC
    CORROSION SCIENCE, 1979, 19 (11) : 889 - 906
  • [45] Kinetics of oxidation of Fe-Cr-Al alloy Characterization by electrochemical spectroscopy of impedance in a 3% medium NaCl
    Chadli, H.
    Retima, M.
    Khenioui, Y.
    PROCEEDINGS OF THE JMSM 2008 CONFERENCE, 2009, 2 (03): : 1015 - 1020
  • [46] Microstructure evolution and properties of Fe-Cr-Al alloy in the process of annealing
    Tang, D. (tangdi@nercar.ustb.edu.cn), 1600, Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China (34):
  • [47] Preparation and properties of the anodized film on Fe-Cr-Al alloy surface
    Yang, Jialin
    Guo, Yunting
    Zai, Wei
    Ma, Siyuan
    Dong, Liang
    Li, Guangyu
    ANTI-CORROSION METHODS AND MATERIALS, 2020, 67 (04) : 379 - 386
  • [48] Influences of yttrium on adhesion of oxide scale of Fe-Cr-Al alloy
    Xin, L
    Li, MS
    Zhou, LJ
    Wang, FH
    Li, TF
    JOURNAL OF RARE EARTHS, 2001, 19 (02) : 117 - 121
  • [49] PROPAGATION CHARACTERISTICS OF ACOUSTIC SHOCK PULSE IN FE-CR-AL ALLOY
    YASUMOTO, Y
    TAKEUCHI, R
    JOURNAL OF THE ACOUSTICAL SOCIETY OF AMERICA, 1978, 64 : S32 - S32
  • [50] Highly heat-resistant powder Fe-Cr-Al alloy
    TsNIIchermet, Moscow, Russia
    Stal', 2002, (01): : 75 - 76