Enhancing tensile strength of styrene butadiene rubber using alkanolamide

被引:3
|
作者
Surya, Indra [1 ]
Ismail, H. [2 ]
机构
[1] Univ Sumatera Utara, Chem Engn Dept, Medan, Indonesia
[2] Univ Sains Malaysia, Sch Mat & Mineral Resources Engn, Engn Campus, Nibong Tebal, Penang, Indonesia
关键词
EPOXIDIZED NATURAL-RUBBER; SILICA; REINFORCEMENT;
D O I
10.1088/1757-899X/509/1/012053
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Enhancing the carbon black (CB) dispersion and tensile strength of composites of styrene-butadiene rubber (SBR) using bio compatibilizer-alkanolamide (BALK) was carried out. The raw SBR was filled by N330 type of CB at a fixed concentration (thirty parts per hundred rubbers, phr). The BALK was Refined Bleached Deodorized Palm Stearin (RBDPS)-based additive, loaded into the composites at 1, 3, 5 and 7 phr. The BALK enhanced not only degree of CB dispersion but also tensile properties. It exhibited tensile and modulus enhancements, especially up to a five phr of addition. The morphological study proved that the five phr was the optimum BALK addition where the fractured surface of composites of SBR with five phr of BALK showed the greatest surface roughness and matrix tearing line.
引用
收藏
页数:6
相关论文
共 50 条
  • [31] Enhancing the Properties of Styrene-Butadiene Rubber by Adding Borax Particles of Different Sizes
    Salih, Habeeb A.
    Ali, Hasan S.
    Talu, S.
    Jawad, Akram J.
    IRANIAN JOURNAL OF CHEMISTRY & CHEMICAL ENGINEERING-INTERNATIONAL ENGLISH EDITION, 2021, 40 (05): : 1616 - 1629
  • [32] Tech service: Determination of the styrene content of styrene-butadiene rubber using TGA
    Shield, Stephanie R.
    Ghebrehiwet, N.
    Rubber World, 2000, 223 (02): : 24 - 33
  • [33] Tensile Strength and Flexural Strength Testing of Acrylonitrile Butadiene Styrene (ABS) Materials for Biomimetic robotic Applications
    Tran Linh Khuong
    Gang, Zhao
    Farid, Muhammad
    Yu, Rao
    Sun, Zhuang-Zhi
    Rizwan, Muhammad
    JOURNAL OF BIOMIMETICS BIOMATERIALS AND BIOMEDICAL ENGINEERING, 2014, 20 : 11 - 21
  • [34] Improvement in compressive strength of Styrene-Butadiene-Rubber (SBR) modified mortars by using powder form and nanoparticles
    Idrees, Maria
    Saeed, Farhan
    Amin, Abreeza
    Hussain, Tousif
    JOURNAL OF BUILDING ENGINEERING, 2021, 44
  • [35] Dynamic mechanical properties of filled styrene butadiene rubber compounds:: comparison of tensile and shear data
    Konecny, P.
    Cerny, M.
    Voldanova, J.
    Malac, J.
    Simonik, J.
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2007, 18 (02) : 122 - 127
  • [36] Structural morphology and properties of star styrene-isoprene-butadiene rubber and natural rubber/star styrene-butadiene rubber blends
    Zhao, SH
    Zou, H
    Zhang, XY
    JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 93 (01) : 336 - 341
  • [37] THE EFFECTS OF LIGHT AND HEAT ON THE RUBBER CONTENT AND IMPACT STRENGTH OF ACRYLONITRILE-BUTADIENE-STYRENE
    BAIR, HE
    BOYLE, DJ
    KELLEHER, PG
    POLYMER ENGINEERING AND SCIENCE, 1980, 20 (15): : 995 - 1001
  • [38] The effect of alkanolamide addition on cure and tensile properties of unfilled natural rubber compounds
    Surya, I.
    Siregar, S. F.
    Ismail, H.
    INNOVATION IN POLYMER SCIENCE AND TECHNOLOGY 2016 (IPST 2016), 2017, 223
  • [39] Improvement of properties of silica-filled styrene-butadiene rubber compounds using acrylonitrile-butadiene rubber
    Choi, SS
    JOURNAL OF APPLIED POLYMER SCIENCE, 2001, 79 (06) : 1127 - 1133
  • [40] Strength and transport properties of concrete with styrene butadiene rubber latex modified lightweight aggregate
    Patel, Jignesh
    Patil, Hemant
    Patil, Yogesh
    Vesmawala, Gaurang
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 195 : 459 - 467