Study of Deformation Stability during Semi-Dieless Drawing of Ti-6Al-4V Alloy Wire

被引:3
|
作者
Li, Kaisong [1 ]
Wang, Zhangke [1 ]
Liu, Xuefeng [1 ,2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Dept Mat Proc Engn, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Beijing Lab Metall Mat & Proc Modern Transportat, Beijing 100083, Peoples R China
来源
MATERIALS | 2019年 / 12卷 / 08期
基金
中国国家自然科学基金;
关键词
Ti-6Al-4V alloy wire; semi-dieless drawing; stability; BEHAVIOR; DESIGN;
D O I
10.3390/ma12081320
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A semi-dieless drawing technology has the advantages of producing a large deformation in a single pass and achieving high-precision dimensions of the finished products. However, instabilities can easily occur in a technique with a large amount of deformation, resulting in its failure. Herein, the deformation behavior of a wire during semi-dieless drawing is studied by finite element simulations. The instability mechanism of the semi-dieless drawing is proposed and validated by experiments. The experiments are conducted under the following conditions: a heating temperature of 950 degrees C; a distance between the die and heating coil of 20 mm; a feeding speed of 0.25 mm/s; a drawing speed range of 0.38-0.53 mm/s, and a die diameter range of 1.8-2.4 mm. The results show that by increasing the drawing speed or decreasing die diameter, the diameter fluctuation of the dieless drawn wire increases, and the semi-dieless drawing process easily becomes unstable. The diameter of the entering wire shows a fluctuating increasing trend owing to the variation in the drawing speed, which results in the instability during the semi-dieless drawing. The validity of the finite element model is verified by comparing the numerically predicted value and experimentally measured value of the drawn wire diameter.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Oxidation of Ti-6Al-4V alloy
    Guleryuz, Hasan
    Cimenoglu, Huseyin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 472 (1-2) : 241 - 246
  • [32] Microstructural evolution in Ti-6Al-4V during hot deformation
    Gartside, MB
    ADVANCES IN THE SCIENCE AND TECHNOLOGY OF TITANIUM ALLOY PROCESSING, 1996, : 101 - 108
  • [33] ACOUSTIC-EMISSION DURING DEFORMATION OF TI-6AL-4V
    KENNEDY, JR
    SCRIPTA METALLURGICA, 1982, 16 (05): : 525 - 530
  • [34] Microstructure refinement in Ti-6Al-4V during warm deformation
    Zherebtsov, S.
    Murzinova, M.
    Mironov, S.
    SaIishchev, G.
    Semiatin, S. L.
    TMS 2008 ANNUAL MEETING SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND PROPERTIES, 2008, : 211 - +
  • [35] On characterization of deformation microstructure in Boron modified Ti-6Al-4V alloy
    Roy, Shibayan
    Sarkar, Apu
    Suwas, Satyam
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (01): : 449 - 458
  • [36] Characteristic of deformation of Ti-6Al-4V alloy with hydrogen at high temperature
    Li, Zhong-Hua
    Wang, Qing
    Sun, Dong-Li
    Zhang, Li-Ping
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 683 - +
  • [37] Failure and formability studies in warm deep drawing of Ti-6Al-4V alloy
    Kotkunde, Nitin
    Deole, Aditya D.
    Gupta, Amit Kumar
    Singh, Swadesh Kumar
    Adity, B.
    MATERIALS & DESIGN, 2014, 60 : 540 - 547
  • [38] Experimental study on chip deformation of Ti-6Al-4V titanium alloy in cryogenic cutting
    Gong, Le (legong@nuaa.edu.cn), 1600, Springer London (96): : 9 - 12
  • [39] Effect of hot deformation on the tribological behaviour of Ti-6Al-4V alloy
    Ismail, A.
    Abdel-Aziz, M.
    El-Morsy, A.
    El-Bitar, T.
    CANADIAN METALLURGICAL QUARTERLY, 2006, 45 (04) : 469 - 473
  • [40] Deformation behavior in the isothermal compression of hydrogenated Ti-6Al-4V alloy
    Zhang, Wei-Fu
    Li, Miao-Quan
    Lin, Ying-Ying
    Suxing Gongcheng Xuebao/Journal of Plasticity Engineering, 2008, 15 (06): : 107 - 112