A XANES determination of the oxidation state of chromium in silicate glasses

被引:0
|
作者
Berry, AJ [1 ]
O'Neill, HSC [1 ]
机构
[1] Australian Natl Univ, Res Sch Earth Sci, Canberra, ACT 0200, Australia
关键词
D O I
暂无
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
Cr K-edge X-ray absorption near-edge structure (XANES) spectra were recorded for silicate glasses of various compositions in the system CaO + MgO + Al2O3 + SiO2 +/- TiO2, quenched from melts equilibrated as a function of oxygen fugacity (fo(2)) at 1400 degreesC. The spectra vary systematically with fo(2) (logfo(2) similar to 0 to -16) indicating changes in the Cr oxidation state. The intensity of a shoulder on the absorption edge (attributed to the 1s --> 4s transition) was quantified using the corresponding peak in the XANES derivative spectrum and used to determine Cr2+/SigmaCr. The resulting Cr2+/SigmaCr values are in agreement with the theoretical dependence on logfo(2) suggesting that the 1s --> 4s feature is diagnostic of Cr2+ in a silicate glass and sigma(Cr2+/SigmaCr) = +/- 0.015. The Cr2+/SigmaCr ratio for a given logfo(2) changes with the glass composition which may reflect the ability of the melt to accommodate the Jahn-Teller distorted coordination geometry which stabilizes Cr2+.Cr2+/SigmaCr varies between similar to 0.3 and 0.8 over the logfo(2) range bounded by the Ni/NiO and Fe/FeO fo(2) buffers, suggesting that Cr2+ may be important in natural melts even though this oxidation state has never been identified in a terrestrial material. The development of a methodology for determining Cr2+/SigmaCr from XANES spectra of quenched glasses is an essential precursor to in situ experiments on Fe-bearing silicate melts at high temperature.
引用
收藏
页码:790 / 798
页数:9
相关论文
共 50 条
  • [41] Oxidation state of chromium in ferropericlase inclusions in lower mantle diamonds determined with micro-XANES measurements
    Odake, S.
    Kagi, H.
    Arakawa, M.
    Ohta, A.
    Harte, B.
    GEOCHIMICA ET COSMOCHIMICA ACTA, 2009, 73 (13) : A962 - A962
  • [42] Si K-edge EXAFS/XANES study of sodium silicate glasses
    Henderson, G.S.
    Journal of Non-Crystalline Solids, 1995, 183 (1-2):
  • [43] Kinetics and mechanisms of Iron redox reactions in silicate glasses and melts: A XANES study
    Cochain, B.
    Neuville, D. R.
    de Ligny, D.
    Cormier, L.
    Roux, J.
    Baudelet, F.
    Pinet, O.
    Richet, P.
    GEOCHIMICA ET COSMOCHIMICA ACTA, 2008, 72 (12) : A170 - A170
  • [44] OXIDATION-STATE OF COPPER IONS IN SILICATE-GLASSES PREPARED BY DIFFERENT METHODS
    YOKO, T
    KAMIYA, K
    SAKKA, S
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1985, 71 (1-3) : 245 - 251
  • [45] OXIDATION-STATE AND OPTICAL-ABSORPTION OF RHODIUM IN BORATE AND SILICATE-GLASSES
    PAUL, A
    PARKER, JM
    PHYSICS AND CHEMISTRY OF GLASSES, 1975, 16 (05): : 103 - 107
  • [46] The state of magnesium in silicate glasses and melts
    Kuryaeva, R. G.
    GLASS PHYSICS AND CHEMISTRY, 2009, 35 (04) : 378 - 383
  • [47] The state of magnesium in silicate glasses and melts
    R. G. Kuryaeva
    Glass Physics and Chemistry, 2009, 35 : 378 - 383
  • [48] Cr oxidation state in periclase by XANES spectroscopy
    Eeckhout, SG
    Bolfan-Casanova, N
    GEOCHIMICA ET COSMOCHIMICA ACTA, 2005, 69 (10) : A255 - A255
  • [49] DETERMINATION OF CHROMIUM IN GLASSES BY PHOTOMETRIC TITRATION
    CHESNOKOVA, SM
    ABRAMOV, VV
    SMIRNOVA, LN
    ANDREEV, PA
    GLASS AND CERAMICS, 1981, 38 (11-1) : 600 - 602
  • [50] The effect of chromium oxide on optical spectroscopy of sodium silicate glasses
    Mirhadi, Bahman
    Mehdikhani, Behzad
    JOURNAL OF OPTOELECTRONICS AND ADVANCED MATERIALS, 2011, 13 (9-10): : 1067 - 1070