Fabrication, mechanical properties, and tribological behaviors of Ti2AlC and Ti2AlSn0.2C solid solutions

被引:46
|
作者
Cai, Leping [1 ]
Huang, Zhenying [1 ,2 ]
Hu, Wenqiang [1 ]
Hao, Suming [1 ]
Zhai, Hongxiang [1 ]
Zhou, Yang [1 ]
机构
[1] Beijing Jiaotong Univ, Ctr Mat Sci & Engn, Sch Mech & Elect Control Engn, Beijing 100044, Peoples R China
[2] Beijing Jiaotong Univ, Minist Educ, Key Lab Vehicle Adv Mfg Measuring & Control Techn, Beijing, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti2AlC; Ti2AlSn0.2C; microstructure; mechanical property; tribological behavior; GRAIN-SIZE; TI3ALC2; MICROSTRUCTURE; OXIDATION; COMPOSITES; FRICTION; SURFACE; PHASES;
D O I
10.1007/s40145-017-0221-9
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Highly pure and dense Ti2AlC and Ti2AlSn0.2C bulks were prepared by hot pressing with molar ratios of 1:1.1:0.9 and 1:0.9:0.2:0.85, respectively, at 1450 degrees C for 30 min with 28 MPa in Ar atmosphere. The phase compositions were investigated by X-ray diffraction (XRD); the surface morphology and topography of the crystal grains were also analyzed by scanning electron microscopy (SEM). The flexural strengths of Ti2AlC and Ti2AlSn0.2C have been measured as 430 and 410 MPa, respectively. Both Vickers hardness decreased slowly as the load increased. The tribological behavior was investigated by dry sliding a low-carbon steel under normal load of 20-80 N and sliding speed of 10-30 m/s. Ti2AlC bulk has a friction coefficient of 0.3-0.45 and a wear rate of (1.64-2.97)x10(-6) mm(3)/(N.m), while Ti2AlSn0.2C bulk has a friction coefficient of 0.25-0.35 and a wear rate of (2.5-4.31) x10(-6) mm(3)/(N.m). The influences of Sn incorporation on the microstructure and properties of Ti2AlC have also been discussed.
引用
收藏
页码:90 / 99
页数:10
相关论文
共 50 条
  • [21] Preparation and properties of Ti2AlC/TiAl composites
    School of Materials Science and Engineering, Shaanxi University of Technology, Hanzhong, China
    Rengong Jingti Xuebao, (275-279):
  • [22] Synthesis of Ti2AlC by hot pressing and its mechanical and electrical properties
    王苹
    梅炳初
    洪小林
    周卫兵
    Transactions of Nonferrous Metals Society of China, 2007, (05) : 1001 - 1004
  • [23] Physicomechanical Properties of Coatings Based on Max Ti2AlC and (Ti, Nb)2AlC Phases at 20°C and 500°C
    Podhurska, V. Ya.
    Kuprin, O. S.
    Chepil, R. V.
    Ostash, O. P.
    Prikhna, T. O.
    Sverdun, V. B.
    Bortnytska, M. O.
    MATERIALS SCIENCE, 2023, 59 (01) : 10 - 17
  • [24] Physicomechanical Properties of Coatings Based on Max Ti2AlC and (Ti, Nb)2AlC Phases at 20°C and 500°C
    V. Ya. Podhurska
    O. S. Kuprin
    R. V. Chepil
    O. P. Ostash
    T. O. Prikhna
    V. B. Sverdun
    M. O. Bortnytska
    Materials Science, 2023, 59 (1) : 10 - 17
  • [25] Strengthening of Ti2AlC by substituting Ti with V
    Meng, FL
    Zhou, YC
    Wang, JY
    SCRIPTA MATERIALIA, 2005, 53 (12) : 1369 - 1372
  • [26] Anisotropic corrosion of Ti2AlC and Ti3AlC2 in supercritical water at 500 °C
    Du, Yina
    Liu, Ji-Xuan
    Gu, Yifeng
    Wang, Xin-Gang
    Xu, Fangfang
    Zhang, Guo-Jun
    CERAMICS INTERNATIONAL, 2017, 43 (09) : 7166 - 7171
  • [27] Mechanical and oxidation behavior of textured Ti2AlC and Ti3AlC2 MAX phase materials
    Li, Xiaoqiang
    Xie, Xi
    Gonzalez-Julian, Jesus
    Malzbender, Juergen
    Yang, Rui
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (15) : 5258 - 5271
  • [28] On the interactions of Ti2AlC, Ti3AlC2, Ti3SiC2 and Cr2AlC with palladium at 900 °C
    Bentzel, G. W.
    Sokol, M.
    Griggs, J.
    Lang, A. C.
    Barsoum, M. W.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 771 : 1103 - 1110
  • [29] Fabrication and characterization of NiTi/Ti3SiC2 and NiTi/Ti2AlC composites
    Hu, Liangfa
    Kothalkar, Ankush
    Proust, Gwénaëlle
    Karaman, Ibrahim
    Radovic, Miladin
    Journal of Alloys and Compounds, 2014, 610 : 635 - 644
  • [30] Fabrication and characterization of NiTi/Ti3SiC2 and NiTi/Ti2AlC composites
    Hu, Liangfa
    Kothalkar, Ankush
    Proust, Gwenaelle
    Karaman, Ibrahim
    Radovic, Miladin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 610 : 635 - 644