Factors affecting aluminum depletion during cyclic oxidation of Fe-base alumina-forming alloys

被引:9
|
作者
Pint, B. A. [1 ]
Walker, L. R. [1 ]
Wright, I. G. [1 ]
机构
[1] Oak Ridge Natl Lab, Div Mat Sci & Technol, Oak Ridge, TN 37831 USA
关键词
alumina-formers; breakaway oxidation; oxide dispersion strengthened; lifetime model; HIGH-TEMPERATURE OXIDATION; BREAKAWAY OXIDATION; HEAT-EXCHANGER; GROWTH-RATES; LIFETIME; BEHAVIOR; SCALES; PERFORMANCE;
D O I
10.3184/096034009X464401
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to develop an improved oxidation-limited lifetime model, experiments are being conducted to assess the critical factors that affect the rate of Al loss from Fe-base alumina-forming alloys during cyclic oxidation. Both wrought and dispersion strengthened ferritic and intermetallic Fe-Al +/- Cr alloys are being investigated at exposure temperatures from 1100-1300 degrees C. Higher temperatures, thinner specimens and cycle frequency are used to accelerate degradation during oxidation. However, the effects of these experimental choices often have not been critically assessed in prior work. Electron probe microanalysis has been used to measure the residual Al Content under various conditions and at various stages of life. For 0.5-2 mm thick specimens, lifetime repeatedly showed a linear relationship to thickness. Increasing the oxidation temperature appears to be the most viable strategy to accelerate the evaluation of oxidation resistance for comparing and developing alloys.
引用
收藏
页码:211 / U2