Effect of different preparation designs and all ceramic materials on fracture strength of molar endocrowns

被引:21
|
作者
Haralur, Satheesh B. [1 ]
Alamrey, Alaa Ali [2 ]
Alshehri, Shatha Abdulrahman [2 ]
Alzahrani, Danyah Saeed [2 ]
Alfarsi, Mohammed [1 ]
机构
[1] King Khalid Univ, Coll Dent, Dept Prosthodont, Abha 62529, Saudi Arabia
[2] King Khalid Univ, Coll Dent, Abha, Saudi Arabia
关键词
Endocrowns; lithium disilicate ceramic; polymer infiltrated hybrid ceramic; high translucency zirconia; fracture resistance; ENDODONTICALLY TREATED TEETH; LOAD-BEARING CAPACITY; LITHIUM DISILICATE; FAILURE MODES; CROWNS; RESISTANCE; THICKNESS; POST; RESTORATIONS; PREMOLARS;
D O I
10.1177/2280800020947329
中图分类号
Q6 [生物物理学];
学科分类号
071011 ;
摘要
Objective: The aim was to compare the fracture strength of Molar endocrowns fabricated from different all-ceramic materials and various preparation designs. Materials and methods: Ninety extracted human molar teeth were root canal treated and randomly divided into three groups according to the all ceramic materials used for fabrication of the endocrowns (n = 30): (1) Lithium disilicate (IPS e.max Press); (2) Polymer infiltrated ceramic (Vita Enamic); (3) High translucency zirconia (Ceramill Zolid HT). Each group was subdivided into 3 subgroups (n = 10) according to the preparation design as 2 mm occlusal reduction, 4.5 mm occlusal reduction, and 4.5 mm occlusal reduction with 2 mm radicular extension. The endocrowns from each material were fabricated and surface treated according to the manufacturer's recommendations. After cementation with self-adhesive resin luting cement, the specimens were stored in a humid environment for 72 hours and subsequently subjected to 5000 thermal cycles. After, a compressive, static-axial load was applied using a universal testing machine until failure. Load-to-failure was recorded (N) and the specimens were examined under a stereomicroscope to determine the failure type. The data was statistically analyzed using One-way ANOVA and Tukey HSD tests at p < 0.05. Results: The Lithium Disilicate endocrowns recorded the higher mean fracture strength for 4.5 mm occlusal thickness and 2 mm radicular extension at 3770.28 N and 3877.40 correspondingly. The High translucency zirconia endocrowns at conventional 2 mm thickness showed the highest mean fracture load (3533.34 N). Even though polymer infiltrated ceramic endocrowns displayed comparatively lesser fracture load; they recorded the predominantly favorable fractures. Conclusions: Increased occlusal thickness showed a significant improvement in fracture strength of lithium disilicate and polymer infiltrated ceramic molar endocrowns. Although the 2 mm radicular extension had the substantial enhancement of fracture strength in high translucency zirconia, it resulted in more unfavorable failure types.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Effect of a DPSS laser on the shear bond strength of ceramic brackets with different base designs
    Mi-Gyoung Park
    Jung-Hoon Ro
    Jeong-Kil Park
    Ching-Chang Ko
    Yong Hoon Kwon
    Lasers in Medical Science, 2013, 28 : 1461 - 1466
  • [42] Effect of a DPSS laser on the shear bond strength of ceramic brackets with different base designs
    Park, Mi-Gyoung
    Ro, Jung-Hoon
    Park, Jeong-Kil
    Ko, Ching-Chang
    Kwon, Yong Hoon
    LASERS IN MEDICAL SCIENCE, 2013, 28 (06) : 1461 - 1466
  • [43] The Effect of Different Materials and Techniques on Stress Distribution in CAD/CAM Endocrowns
    Eskitascioglu, M.
    Kucuk, O.
    Eskitascioglu, G.
    Eraslan, O.
    Belli, S.
    STRENGTH OF MATERIALS, 2020, 52 (05) : 812 - 819
  • [44] In vitro fracture strength of teeth restored with different procera all-ceramic crowns.
    Potiket, N.
    Chiche, G. J.
    Finger, I. M.
    Mercante, D.
    Blatz, M. B.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B182 - B182
  • [45] Temperature dependence of the fracture strength of porous ceramic materials
    Wang, Ruzhuan
    Wang, Shu
    Li, Dingyu
    Li, Weiguo
    Zhang, Chuanzeng
    CERAMICS INTERNATIONAL, 2020, 46 (08) : 11311 - 11316
  • [46] Comparison of Fracture Strength of Modified PEEK, Nanohybrid Ceramic, Monolithic Zirconium Endocrowns Produced with CAD/CAM System
    Ciris, Gulsum Sena
    Altintas, Eyyup
    MEANDROS MEDICAL AND DENTAL JOURNAL, 2022, 23 (03): : 393 - 399
  • [47] The fracture strength of endocrowns manufactured from different hybrid blocks under axial and lateral forces
    Acar, Duygu Hazal
    Kalyoncuoglu, Elif
    CLINICAL ORAL INVESTIGATIONS, 2021, 25 (04) : 1889 - 1897
  • [48] The fracture strength of endocrowns manufactured from different hybrid blocks under axial and lateral forces
    Duygu Hazal Acar
    Elif Kalyoncuoğlu
    Clinical Oral Investigations, 2021, 25 : 1889 - 1897
  • [49] Correction: Effect of proximal box elevation on fracture resistance and microleakage of premolars restored with ceramic endocrowns
    Zhang, Hong
    Li, He
    Cong, Qian
    Zhang, Zhimin
    Du, Aobo
    Wang, Ying
    PLOS ONE, 2021, 16 (09):
  • [50] The effect of preparation design on the fracture strength of resin-bonded ceramic restorations.
    Teo, P
    Baratieri, LN
    Van Noort, R
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A421 - A421