Overview of interfacial fracture energy predictions for stacked thin films using a four-point bending framework

被引:13
|
作者
Lee, Chang-Chun [1 ]
机构
[1] Chung Yuan Christian Univ, Inst Biomed Technol, Dept Mech Engn, Res & Dev Ctr Microsyst Reliabil, Chungli 32023, Taoyuan County, Taiwan
来源
关键词
Interfacial adhesion; Four-point bending test; J-integral; Virtual crack closure technique; Finite element analysis (FEA); LASER SPALLATION TECHNIQUE; ADHESION MEASUREMENTS; BIMATERIAL INTERFACE; MECHANICS ANALYSIS; CRACK-PROPAGATION; HARD COATINGS; TOUGHNESS; DELAMINATION; PENETRATION; DEFLECTION;
D O I
10.1016/j.surfcoat.2013.06.127
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Developing a robust predicting methodology on the interfacial fracture energy of dissimilar materials is urgently needed to meet the mechanical strength requirements for investigating novel materials and subsequent device structures with the bonded types of multi thin films. Thus, this paper provides an overview of useful approaches according to linear-elastic interfacial fracture mechanics, such as J-integral method, modified virtual crack closure technique (MVCCT), and analytical solutions derived from the relationship between the stress field of delaminated tip and crack tip opening displacements to compare their estimated capability of cracking energy. A popular technique for determining the interface adhesion of thin coatings is the four-point bending test (4-PBT). The testing vehicles of 4-PBT allow a more thorough validation of the foregoing predicted approaches based on finite element analysis compared with the simulated results with related experimental data. The critical energies of 18 J/m(2), 78.53 J/m(2), 52.01 J/m(2), and 71.02 J/m(2) for the bonded interfaces of SiO2/SiLK, Ta/SiLK, TaN/SiLK, and Si3N4/SiLK stacked nano-scaled thin films are precisely judged, respectively. The predicted results of the J-integral method match well with the MVCCT estimation. The results reveal that the opening fractured mode is dominant at the beginning of the crack advances along the bonded interface of Ta/SiLK, TaN/SiLK, and Si3N4/SiLK stacked films as the interfacial crack length increases. Moreover, the essential trends of dependences for the modulus ratio and thickness ratio of stacked thin films on interfacial energy release rate are logically identified and investigated. Therefore, this paper could be regarded as a design guideline of interfacial fracture behavior for stacked films utilized in the development of advanced device technologies. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:333 / 340
页数:8
相关论文
共 50 条
  • [31] CLEAVAGE FRACTURE ANALYSIS OF CLADDED BEAMS WITH AN EMBEDDED FLAW UNDER FOUR-POINT BENDING
    Yin, Shengjun
    Williams, Paul T.
    Bass, B. Richard
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2008, VOL 6, PT A AND B, 2009, : 103 - 110
  • [32] Elastic and electromagnetic monitoring of TRC sandwich panels in fracture under four-point bending
    Ospitia, Nicolas
    Tsangouri, Eleni
    Pourkazemi, Ali
    Wang, Qinjian
    Keshavarzi, Mohammasadegh
    Stiens, Johan H.
    Aggelis, Dimitrios G.
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 400
  • [33] Shear characterization of sandwich core materials using four-point bending
    Juntikka, Rickard
    Hallstrom, Stefan
    JOURNAL OF SANDWICH STRUCTURES & MATERIALS, 2007, 9 (01) : 67 - 94
  • [34] NUMERICAL SIMULATION OF AN ICE BEAM IN FOUR-POINT BENDING USING SPH
    Das, Jitapriya
    Polic, Drazen
    Ehlers, Soren
    Amdahl, Jorgen
    33RD INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARCTIC ENGINEERING, 2014, VOL 10: POLAR AND ARCTIC SCIENCE AND TECHNOLOGY, 2014,
  • [35] Simulation of Four-Point Bending Fracture Test of Steel-Fiber-Reinforced Concrete
    Kan, Wenguang
    Yang, Zailin
    Yin, Weilong
    MATERIALS, 2022, 15 (20)
  • [36] Adhesion evaluation of thin films to dielectrics in multilayer stacks: A comparison of four-point bending and stressed overlayer technique.
    Lassnig, A.
    Putz, B.
    Hirn, S.
    Többens, D.M.
    Mitterer, C.
    Cordill, M.J.
    Materials and Design, 2021, 200
  • [37] Apparatus for thin-film stress measurement with integrated four-point bending equipment:: Performance and results on Cu films
    Weihnacht, V
    Brückner, W
    Schneider, CM
    REVIEW OF SCIENTIFIC INSTRUMENTS, 2000, 71 (12): : 4479 - 4482
  • [38] Comparison of the telephone cord delamination method for measuring interfacial adhesion with the four-point bending method
    Lee, A
    Litteken, CS
    Dauskardt, RH
    Nix, WD
    ACTA MATERIALIA, 2005, 53 (03) : 609 - 616
  • [39] Development of hybrid four-point bending test for determining mechanical properties of thin films using finite element method and response surface method
    Kinoshita, K.
    FOURTH INTERNATIONAL CONFERENCE ON EXPERIMENTAL MECHANICS, 2010, 7522
  • [40] Determining the fracture toughness of quasi-brittle materials with notched four-point bending tests
    Han, Xiangyu
    Xiao, Qinghua
    Cui, Kai
    Hu, Xiaozhi
    Zhou, Zelin
    ENGINEERING FRACTURE MECHANICS, 2023, 284