Preparation of a Calcium Titanium Phosphate Glass-Ceramic with Improved Chemical Durability

被引:14
|
作者
Kasuga, Toshihiro [1 ]
Kimata, Takafumi [1 ]
Obata, Akiko [1 ]
机构
[1] Nagoya Inst Technol, Grad Sch Engn, Dept Frontier Mat, Showa Ku, Nagoya, Aichi 4668555, Japan
关键词
APATITE; SPECTROSCOPY; FLUORAPATITE; FRACTURE; SYSTEM; RAMAN;
D O I
10.1111/j.1551-2916.2009.03107.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A calcium titanium phosphate glass-ceramic for use as a dental material with excellent chemical durability was derived from a mother glass with a small amount of fluorine. The laser Raman spectroscopic analysis showed that 35CaO-10CaF(2)-30P(2)O(5)-25TiO(2) glass, as the nominal composition, consists of ortho-, pyro-, and meta-phosphate groups. On heating the glass at 865 degrees C, orthophosphate crystals, such as fluorine-containing oxyapatite (Ca(10)(PO(4))(6)(O,F(2))) and the Nasicon-type phase (CaTi(4)(PO(4))(6)), were preferentially precipitated; the apatite particles of several tens of nanometers in size were embedded in the CaTi(4)(PO(4))(6) phase. The pale bluish color of the glass-ceramic indicated that titanium ions were included in the residual glassy phase. When the glass-ceramic was treated with dilute hydrochloric acid, only the apatite particles at the surface were leached out, while no CaTi(4)(PO(4))(6) phase was etched; the dissolution of the glass-ceramic was effectively controlled. Almost no dissolution of ions from the glass-ceramic occurred in water. It was suggested that the behavior is a result of the microstructure of the glass-ceramic, which consists of crystalline and glassy phases with excellent chemical durability.
引用
收藏
页码:1709 / 1712
页数:4
相关论文
共 50 条
  • [21] Fabrication of a new porous glass-ceramic monolith using vanadium(III) calcium phosphate glass as precursor
    Mazali, IO
    Alves, OL
    JOURNAL OF THE BRAZILIAN CHEMICAL SOCIETY, 2004, 15 (04) : 464 - 467
  • [22] CALCIUM-PHOSPHATE GLASS-CERAMIC CROWN PREPARED BY LOST-WAX TECHNIQUE
    KIHARA, S
    WATANABE, A
    ABE, Y
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1984, 67 (06) : C100 - C101
  • [23] Enhancement of biomimetic apatite forming ability of calcium phosphate glass-ceramic by a hydrothermal treatment
    Kasuga, T
    Fujimoto, T
    Nogami, M
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2003, 111 (09) : 633 - 635
  • [24] Preparation, thermal characterisation and chemical durability of calcium iron phosphate glasses
    Metcalfe, BL
    Fong, SK
    Donald, IW
    GLASS TECHNOLOGY, 2005, 46 (02): : 130 - 133
  • [25] Preparation and Characterization of Glass-Ceramic Basalt Fiber
    Lida Luo
    Tan Yan
    Jin Liu
    Linfeng Ding
    Qingwei Wang
    Wan Jiang
    JournalofHarbinInstituteofTechnology(NewSeries), 2022, 29 (06) : 27 - 33
  • [26] Improved glass-ceramic envelope for vacuum interrupters
    Parashar, R. S.
    25TH INTERNATIONAL SYMPOSIUM ON DISCHARGES AND ELECTRICAL INSULATION IN VACUUM (ISDEIV 2012), 2012, : 449 - 452
  • [27] Preparation of self-cleaning glass-ceramic
    Hou, Tie-Cui
    Li, Ming-Liang
    Wang, Hai-Long
    Zhang, Rui
    Lu, Hong-Xia
    Chen, De-Liang
    Xu, Hong-Liang
    Huaxue Gongcheng/Chemical Engineering (China), 2008, 36 (09): : 58 - 62
  • [28] CHEMICAL DURABILITY OF PHOSPHATE-GLASS
    JOHNSTONE, JK
    WILDER, JA
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 375 - 375
  • [29] BIOCOMPATIBLE GLASS-CERAMIC COATINGS FOR TITANIUM-ALLOYS
    VLASOV, AS
    LUDANOVA, OV
    GLASS AND CERAMICS, 1995, 52 (3-4) : 99 - 101
  • [30] INTERFACIAL EQUILIBRIA IN TITANIUM PARTICLE GLASS-CERAMIC COMPOSITES
    FERRARIS, M
    BADINI, C
    COUZINET, B
    COMPOSITES, 1994, 25 (07): : 494 - 498