Enhancing Wear Resistance of A356 Alloy by Adding CNFs Based on Ultrasonic Vibration Casting

被引:9
|
作者
Wu, Qing-Jie [1 ,2 ]
Yan, Hong [1 ,2 ]
Zhang, Peng-Xiang [1 ,2 ]
Zhu, Xue-Qin [1 ,2 ]
Nie, Qiao [3 ]
机构
[1] Nanchang Univ, Sch Mech & Elect Engn, Nanchang 330031, Jiangxi, Peoples R China
[2] Key Lab Light Alloy Preparat & Proc Nanchang City, Nanchang 330031, Jiangxi, Peoples R China
[3] Jiangxi Ling Ge Nonferrous Met Proc Co Ltd, Nanchang 330008, Jiangxi, Peoples R China
基金
中国国家自然科学基金;
关键词
A356 matrix composites; Carbon nanofibers; Wear testing; MATRIX COMPOSITES; MECHANICAL-PROPERTIES; CARBON NANOTUBES; DRY WEAR; FRICTION; BEHAVIOR; MICROSTRUCTURE;
D O I
10.1007/s40195-017-0680-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A356-carbon nanofibers (CNFs) composites with different contents of CNFs were fabricated by ultrasonic vibration casting to investigate the effect of CNFs in the matrix on the mechanical properties and wear resistance. The worn surfaces were investigated using scanning electron microscopy (SEM). As the CNFs content was increased, strength, hardness and wear resistance were significantly enhanced and the coefficient of friction was extremely reduced. The nanocomposite containing 1.2 wt% of CNFs exhibited more than 109 HV in hardness and less than 0.35 in the coefficient of friction. Compared with the as-cast matrix, the wear rate of the optimal composite was less than one-third of the matrix sample and the microhardness exhibited about 47% enhancement of the matrix. Meanwhile, steadier and lower friction coefficient was also achieved by the composite. CNFs were observed to be either partially or fully crushed forming a carbon film that covered the surface and acted as a solid lubricant, enhancing the wear behavior significantly.
引用
收藏
页码:523 / 532
页数:10
相关论文
共 50 条
  • [41] Enhancement of wear and corrosion resistance of cast A356 aluminium alloy using friction stir processing
    Reddy G.M.
    Rao K.S.
    Transactions of the Indian Institute of Metals, 2010, 63 (5) : 793 - 798
  • [42] The Effects of Molding Materials on Microstructure and Wear Behavior of A356 Alloy
    Yildirim, Musa
    Ozyurek, Dursun
    Tuncay, Tansel
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2017, 36 (05) : 515 - 521
  • [43] Enhancement of wear and corrosion resistance of cast A356 aluminium alloy using friction stir processing
    Reddy, G. Madhusudhan
    Rao, K. Srinivasa
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2010, 63 (05) : 793 - 798
  • [44] The effect of ultrasonic injection on the microstructure and mechanical properties of A356 alloy
    Kang, Byoung-Il
    Ko, Dae-Gyun
    Youn, Jeong-Il
    Kim, Young-Jig
    THERMEC 2009 SUPPLEMENT: 6TH INTERNATIONAL CONFERENCE ON PROCESSING & MANUFACTURING OF ADVANCED MATERIALS, 2010, 89-91 : 285 - +
  • [45] Refinement of eutectic silicon phase of aluminum A356 alloy using high-intensity ultrasonic vibration
    Jian, X
    Meek, TT
    Han, Q
    SCRIPTA MATERIALIA, 2006, 54 (05) : 893 - 896
  • [46] The effect of ultrasonic injection on the microstructure and mechanical properties of A356 alloy
    Kang, Byoung-Il
    Ko, Dae-Gyun
    Youn, Jeong-Il
    Kim, Young-Jig
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 3960 - 3965
  • [47] MECHANICAL PROPERTIES AND MICROSTRUCTURES OF A356 ALLOY PREPARED BY CASTING COMBINED WITH FORGING
    Liang, Zhenglong
    Zhang, Qi
    PROCEEDINGS OF THE ASME 12TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE - 2017, VOL 1, 2017,
  • [48] Investigation of Simultaneous Effects of Cooling Slope Casting and Mold Vibration on Mechanical and Microstructural Properties of A356 Aluminum Alloy
    Mahdieh Jahanbakhshi
    Salman Nourouzi
    Reza Naseri
    Kourosh Esfandiari
    Metals and Materials International, 2022, 28 : 1508 - 1516
  • [49] Investigation of Simultaneous Effects of Cooling Slope Casting and Mold Vibration on Mechanical and Microstructural Properties of A356 Aluminum Alloy
    Jahanbakhshi, Mahdieh
    Nourouzi, Salman
    Naseri, Reza
    Esfandiari, Kourosh
    METALS AND MATERIALS INTERNATIONAL, 2022, 28 (06) : 1508 - 1516
  • [50] Liquidus semi-continuous casting and thixoforming of the aluminum alloy A356
    Wang, P
    Lu, GM
    Cui, JZ
    RARE METAL MATERIALS AND ENGINEERING, 2002, 31 (05) : 382 - 384