Effect of Molybdenum Content on Heat Treatment Behavior of Multi-Alloyed White Cast Iron

被引:13
|
作者
Meebupha, Thanit [1 ]
Inthidec, Sudsakorn [2 ]
Sricharoenchai, Prasonk [1 ]
Matsubara, Yasuhiro [3 ]
机构
[1] Chulalongkorn Univ, Dept Met Engn, Fac Engn, Bangkok 10330, Thailand
[2] Mahasarakham Univ, Dept Mfg Engn, Fac Engn, Maha Sarakham 44150, Thailand
[3] Kurume Coll, Natl Inst Technol, Fukuoka 8308555, Japan
关键词
multi-alloyed white cast iron; heat treatment; hardness; volume fraction of retained austenite; molybdenum effect; CARBON;
D O I
10.2320/matertrans.M2016396
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of the Molybdenum (Mo) content on the heat treatment behavior of multi-alloyed white cast iron was investigated. The cast iron with varying Mo contents from 0.12 to 7.66% under the basic alloy composition of 5% Cr, W and V each was prepared. After annealing at 1223 K for 18 ks, the test specimens were austenitized at 1373 K for 3.6 ks in a vacuum furnace and subsequently hardened by a jet-spray of liquid nitrogen. The tempering was carried out at temperatures from 673 to 873 K at 50 K intervals for 12 ks. It was found that the hardness in the as-hardened state was increased progressively with an increase in the Mo content. The volume fraction of the retained austenite (V.) decreased markedly when the Mo content was increased over 1.17%. In the tempered state, the hardness curve showed clear secondary hardening due to the precipitation of fine secondary carbides and a reduction of the V.. The V. value in each specimen decreased gradually as the tempering temperature was elevated, but reduced greatly when tempered at 748 to 823 K. The maximum tempered hardness (HTmax) was obtained in the specimen tempered at 798 K where the V. was less than 10%. The HTmax increased first, and then subsequently decreased with an increase in the Mo content. The highest HTmax value, 946 HV30, was obtained in the specimen with 4.98% Mo. It was found that the 15-37% V. in the as-hardened state was necessary to get the hardness over 900 HV30 by tempering. The degree of secondary hardening (Delta Hs) increased as the Mo content rose from 0.12 to 4.98% where the difference between the V-gamma in the as-hardened state and that at HTmax (Delta V-gamma) was 22-23%.
引用
收藏
页码:655 / 662
页数:8
相关论文
共 50 条
  • [22] Effect of pulsed laser treatment on the structure of alloyed cast iron
    V. V. Girzhon
    D. I. Anpilogov
    Metal Science and Heat Treatment, 1997, 39 : 144 - 145
  • [23] Effect of pulsed laser treatment on the structure of alloyed cast iron
    Girzhon, VV
    Anpilogov, DI
    METAL SCIENCE AND HEAT TREATMENT, 1997, 39 (3-4) : 144 - 145
  • [24] Heat treatment of novel low-carbon multi-alloyed anti-wear marine steel
    Jiang, Jing-hua
    Wang, Qiu-yue
    Ma, Ai-bin
    Shi, Jun
    Zhang, Liu-yan
    Yang, Hui-dong
    Lu, Fu-min
    Zhou, Qi
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2011, 21 (03) : 254 - 261
  • [25] Heat treatment of novel low-carbon multi-alloyed anti-wear marine steel
    Jing-hua JIANG~(1
    2.College of Mechanics and Materials
    3.Department of Mechanical and Aerospace Engineering
    Progress in Natural Science:Materials International, 2011, 21 (03) : 254 - 261
  • [26] Effect of Molybdenum Content, Pouring Temperature and Cooling Rate on the Casting Defects of High Chromium White Cast Iron
    Dugic, Izudin
    TMS 2017 146TH ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2017, : 475 - 482
  • [27] Effect of Boron and Heat Treatment on Mechanical Properties of White Cast Iron for Mining Application
    Havva Kazdal Zeytin
    Hakan Yildirim
    Banu Berme
    Selim Duduoglu
    Gürkan Kazdal
    Adem Deniz
    Journal of Iron and Steel Research(International), 2011, 18 (11) : 31 - 39
  • [28] Effect of Boron and Heat Treatment on Mechanical Properties of White Cast Iron for Mining Application
    Zeytin, Havva Kazdal
    Yildirim, Hakan
    Berme, Banu
    Duduoglu, Selim
    Kazdal, Gurkan
    Deniz, Adem
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 (11) : 31 - 39
  • [29] Effect of Boron and Heat Treatment on Mechanical Properties of White Cast Iron for Mining Application
    Havva Kazdal Zeytin
    Hakan Yildirim
    Banu Berme
    Selim Duduoĝlu
    Gürkan Kazdal
    Adem Deniz
    Journal of Iron and Steel Research International, 2011, 18 : 31 - 39
  • [30] Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron
    Chen Xiang
    Li Yanxiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (02): : 770 - 775