Physical Properties of a Hybrid and a Nanohybrid Dental Light-Cured Resin Composite

被引:10
|
作者
Sideridou, Irini D. [1 ]
Karabela, Maria M. [1 ]
Micheliou, Christina N. [1 ]
Karagiannidis, Panagiotis G. [2 ]
Logothetidis, Stergios [2 ]
机构
[1] Aristotle Univ Thessaloniki, Dept Chem, Lab Organ Chem Technol, GR-5412 Thessaloniki, Greece
[2] Aristotle Univ Thessaloniki, Dept Phys, Lab Thin Films Nanosyst & Nanometrol, GR-54124 Thessaloniki, Greece
关键词
Dental composites; degree of conversion; flexural properties; thermogravimetric analysis; sorption solubility; volumetric change; surface morphology; AFM; DIMETHACRYLATE RESINS; SORPTION; CONVERSION; ETHANOL; WATER;
D O I
10.1163/156856208X386435
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This work was aimed at the study of some physical properties of two current light-cured dental resin composites, Rok (hybrid) and Ice (nanohydrid). As filler they both contain strontium aluminosilicate particles, however, with different size distribution, 40 nm-2.5 mu m for Rok and 10 nm-1 mu m for Ice. The resin matrix of Rok consists of UDMA, that of Ice of UDMA, Bis-EMA and TEGDMA. Degree of conversion was determined by FT-IR analysis. The flexural strength and modulus were measured using a three-point bending set-up according to the ISO-4049 specification. Sorption, solubility and volumetric change were measured after storage of composites in water or ethanol/water (75 vol%) for 1 day, 7 or 30 days. Thermogravimetric analysis was performed in air and nitrogen atmosphere from 30 to 700 degrees C. Surface roughness and morphology of the composites was studied by atomic force microscopy (AFM). The degree of conversion was found to be 56.9% for Rok and 61.0% for Ice. The flexural strength of Rok does not significantly differ from that of Ice, while the flexural modulus of Rok is higher than that of Ice. The flexural strengths of Rok and Ice did not show any significant change after immersion in water or ethanol solution for 30 days. The flexural modulus of Rok and Ice did not show any significant change either after immersion in water for 30 days, while it decreased significantly, even after 1 day immersion, in ethanol solution. Ice sorbed a higher amount of water and ethanol solution than Rok and showed a higher volume increase. Thermogravimetric analysis showed that Rok contains about 80 wt% inorganic filler and Ice about 75 wt%. (C) Koninklijke Brill NV, Leiden, 2009
引用
收藏
页码:1831 / 1844
页数:14
相关论文
共 50 条
  • [41] EFFECTS OF DILUENTS ON PHYSICAL-PROPERTIES OF A LIGHT-CURED COMPOSITE (PRISMA-FIL)
    CAUGHMAN, WF
    COMER, RW
    ZARDIACKAS, LD
    OPERATIVE DENTISTRY, 1984, 9 (03) : 82 - 85
  • [42] PHOTOCALORIMETRY OF LIGHT-CURED DENTAL COMPOSITES
    ABADIE, MJM
    APPELT, BK
    DENTAL MATERIALS, 1989, 5 (01) : 6 - 9
  • [43] Effect of porous glass-ceramic fillers on mechanical properties of light-cured dental resin composites
    Liu, Yong
    Tan, Yanni
    Lei, Ting
    Xiang, Qijun
    Han, Yunjuan
    Huang, Baiyun
    DENTAL MATERIALS, 2009, 25 (06) : 709 - 715
  • [44] Evaluation of the Degree of Conversion, Residual Monomers and Mechanical Properties of Some Light-Cured Dental Resin Composites
    Moldovan, Marioara
    Balazsi, Robert
    Soanca, Andrada
    Roman, Alexandra
    Sarosi, Codruta
    Prodan, Doina
    Vlassa, Mihaela
    Cojocaru, Ileana
    Saceleanu, Vicentiu
    Cristescu, Ioan
    MATERIALS, 2019, 12 (13)
  • [45] The Influence of Amorphous Calcium Phosphate Addition on Mechanical Properties of the Experimental Light-Cured Dental Composite
    Drzewiecka, Karolina
    Kleczewska, Joanna
    Krasowski, Michal
    Lapinska, Barbara
    Sokolowski, Jerzy
    DENTAL AND MEDICAL PROBLEMS, 2016, 53 (01) : 34 - 40
  • [46] The effect of total light energy on the polymerization of light-cured composite resin and composites.
    Hwang, KL
    Lee, YK
    Lim, BS
    Kim, CW
    JOURNAL OF DENTAL RESEARCH, 2001, 80 (04) : 1349 - 1349
  • [47] Surface hardness of light-cured composite resin using three light guides.
    Dannheimer, MFG
    Marais, JT
    Borman, JW
    Germishuys, PJ
    Nel, JC
    JOURNAL OF DENTAL RESEARCH, 1996, 75 (05) : 1307 - 1307
  • [48] MECHANICAL-PROPERTIES OF LIGHT-CURED AND DARK-CURED HYBRID IONOMERS
    MCCRARY, BR
    POWERS, JM
    LADD, GD
    JOURNAL OF DENTAL RESEARCH, 1994, 73 : 219 - 219
  • [49] Influence of three curing techniques on the polymerization of a light-cured composite resin.
    Pereira, TF
    Campos, VF
    Coviello, RC
    Silva, EM
    Guimaraes, JGA
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 180 - 180
  • [50] Shear bond strength of immediately repaired light-cured composite resin restorations
    Lewis, G
    Johnson, W
    Martin, W
    Canerdy, A
    Claburn, C
    Collier, M
    OPERATIVE DENTISTRY, 1998, 23 (03) : 121 - 127