Mechanical, structural and dissolution properties of heat treated thin-film phosphate based glasses

被引:17
|
作者
Stuart, Bryan W. [1 ]
Gimeno-Fabra, Miquel [1 ]
Segal, Joel [1 ]
Ahmed, Ifty [1 ]
Grant, David M. [1 ]
机构
[1] Univ Nottingham, Adv Mat Res Grp, Fac Engn, Nottingham, England
基金
英国工程与自然科学研究理事会;
关键词
Heat treatment; Phosphate glass; Mechanical properties; Ion leaching; Osseointegration; Thin films; BIOACTIVE GLASS; IN-VITRO; OXIDATION; COATINGS; DIFFERENTIATION; DEGRADATION; LAYERS;
D O I
10.1016/j.apsusc.2017.04.110
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Here we show the deposition of 2.7 mu m thick phosphate based glass films produced by magnetron sputtering, followed by post heat treatments at 500 C-omicron. Variations in degradation properties pre and post heat treatment were attributed to the formation of Hematite crystals within a glass matrix, iron oxidation and the depletion of hydrophilic P-O-P bonds within the surface layer. As deposited and heat treated coatings showed interfacial tensile adhesion in excess of 73.6 MPa; which surpassed ISO and FDA requirements for HA coatings. Scratch testing of coatings on polished substrates revealed brittle failure mechanisms, amplified due to heat treatment and interfacial failure occurring from 2.3 to 5.0 N. Coatings that were deposited onto sandblasted substrates to mimic commercial implant surfaces, did not suffer from tensile cracking or trackside delamination showing substantial interfacial improvements to between 8.6 and 11.3 N. An exponential dissolution rate was observed from 0 to 2 h for as deposited coatings, which was eliminated via heat treatment. From 2 to 24 h ion release rates ordered P > Na > Mg > Ca > Fe whilst all coatings exhibited linear degradation rates, which reduced by factors of 2.4-3.0 following heat treatments. (C) 2017 The Author(s). Published by Elsevier B.V.
引用
收藏
页码:605 / 617
页数:13
相关论文
共 50 条
  • [31] THIN-FILM DEPOSITION INVESTIGATION ON TEX GLASSES
    ZHANG, XH
    FONTENEAU, G
    LUCAS, J
    PERRIN, A
    LI, ZZ
    SERGENT, M
    HALIDE GLASSES V, 1988, 32 : 453 - 456
  • [32] THIN-FILM DIODES ON BASE OF CHALCOGENIDE GLASSES
    GAMAN, VI
    BAZAROV, VD
    IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII FIZIKA, 1967, (09): : 80 - &
  • [33] OPTICAL-STRUCTURAL PROPERTIES OF GEASTE THIN-FILM ALLOYS
    ONTON, A
    HUNTER, S
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1981, 26 (03): : 393 - 393
  • [34] Magnetic and structural properties of CoCrTaNiPt longitudinal thin-film media
    Yoshimura, Satoru
    Djayaprawira, D.D.
    Shoji, Hiroki
    Takahashi, Migaku
    1600, Am Inst Phys, Woodbury, NY, USA (87):
  • [35] Structural and Magnetic Properties of Thin-film ScFeO3
    Kim, Kwang-Joo
    Park, Jongho
    Park, Jae-Yun
    JOURNAL OF MAGNETICS, 2022, 27 (01) : 96 - 99
  • [36] VIBRATIONAL AND STRUCTURAL-PROPERTIES OF THIN-FILM AMORPHOUS PHOSPHORUS
    SHANABROOK, BV
    LANNIN, JS
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1980, 25 (03): : 166 - 166
  • [37] Magnetic and structural properties of CoCrTaNiPt longitudinal thin-film media
    Yoshimura, S
    Djayaprawira, DD
    Shoji, H
    Takahashi, M
    JOURNAL OF APPLIED PHYSICS, 2000, 87 (09) : 6866 - 6868
  • [38] Influence of post-heat treatment over structural network and mechanical properties of carbon (C)-incorporated CVD TiCN thin-film coating
    Das, Soham
    Guha, Spandan
    Ghadai, Ranjan Kr.
    CARBON LETTERS, 2023, 33 (04) : 1073 - 1094
  • [39] Influence of post-heat treatment over structural network and mechanical properties of carbon (C)-incorporated CVD TiCN thin-film coating
    Soham Das
    Spandan Guha
    Ranjan Kr. Ghadai
    Carbon Letters, 2023, 33 : 1073 - 1094
  • [40] Mechanical deformation on nanoparticle-based thin-film transistors
    Vidor, Fabio F.
    Meyers, Thorsten
    Reker, Julia
    Mueller, Kathrin
    Wirth, Gilson I.
    Hilleringmann, Ulrich
    FIFTH CONFERENCE ON SENSORS, MEMS, AND ELECTRO-OPTIC SYSTEMS, 2019, 11043