摘要
Steel Ladle in Bhilai Steel Plant, SAIL, India, passes through VAD & LF-RH route and this exposes refractory lining to a severe operating conditions. Ladles are lined with in-house manufactured MgO-C refractories. Lining life used to be 35 heats, out of which 18-20 heats were through VAD/LF-RH, hence, ladle availability had become a constraint. Laboratory studies were carried-out to optimize granulometry and composition. Gramilometry was developed by adopting Andearssen packing model. A suitable plasiticiser was identified to eliminate inconsistency caused due to variation in resin quality and weather condition. It reduced variation in green bulk density from 6 to 1.3%. Abrasion and slag erosion studies were conducted, which shows that with increase of carbon, abrasion resistance decreases and corrosion resistance improves. Based on these studies, graphite in slag zone was increased from 10 to 12.5% and in metal zone it was reduced to 7.5%. Different process parameters of brick making were optimized to make MgO-C bricks of maximum bulk density with reduced coke porosity. Modified bricks have bulk density of 2.99-3.02 g/cc and coke porosity of 9.5-10.5%. Further, shape of the bricks were changed from side arch to mini keys and thickness was increased from 80 to 100 mm. Mini key bricks are pressed from sides, thus eliminating variation in thickness which is critical dimension for dry joints. These modifications improved average lining life of steel ladies to 64 heats, which includes 37-40 secondary heats. Maximum life obtained is 87 heats.
引用
收藏
页码:343 / +
页数:2
相关论文
共 50 条
  • [31] IMPROVING THE FIRING OF PLATES FOR STEEL-TEEMING LADLE SLIDE GATES
    GLAZMAN, MS
    ABBAKUMOV, VG
    KARAS, GE
    IVANOVA, MY
    REFRACTORIES, 1986, 27 (1-2): : 59 - 61
  • [32] Design and implementation of ergonomic performance measurement system at a steel plant in India
    Ray, Pradip Kumar
    Tewari, V. K.
    WORK-A JOURNAL OF PREVENTION ASSESSMENT & REHABILITATION, 2012, 41 : 5943 - 5949
  • [34] Artificial Intelligence Approaches For The Ladle Predictive Maintenance In Electric Steel Plant
    Vannucci, Marco
    Colla, Valentina
    Chini, Matteo
    Gaspardo, Daniele
    Palm, Birgit
    IFAC PAPERSONLINE, 2022, 55 (02): : 331 - 336
  • [35] MATHEMATICAL-MODEL OF THERMAL PERFORMANCE OF STEEL POURING LADLE
    SHKLYAR, FR
    MALKIN, VM
    KORSHUNOV, VA
    SOVETKIN, VL
    STEEL IN THE USSR, 1991, 21 (02): : 68 - 70
  • [36] LADLE FURNACE REFINING (APC) AT LE-CREUSOT STEEL PLANT
    CAUMONT, F
    DOR, P
    DELAVAREILLE, A
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 1981, 78 (11): : E171 - E172
  • [37] Improvement of the refractory and ladle maintenance concept at the ThyssenKrupp steel plant Bruckhausen
    Ploch, Andreas
    Lindner, Chris
    Schuetz, Carl Heinz
    STAHL UND EISEN, 2006, 126 (09): : 35 - 38
  • [38] Steel ladle treatment section
    Smirnov, N.A.
    Stal', 2001, (01): : 23 - 24
  • [39] Desulfurization of Steel in the Ladle.
    Brazzoduro, L.
    Metallurgia Italiana, 1980, 72 (10): : 409 - 422
  • [40] STEEL LADLE REFRACTORY ZONING
    PHELPS, LR
    GEISLER, TA
    GREEN, ME
    AMERICAN CERAMIC SOCIETY BULLETIN, 1982, 61 (08): : 830 - 830