Ytterbium disilicate-based glass-ceramic as joining material for ceramic matrix composites

被引:15
|
作者
Smeacetto, Federico [1 ]
D'Isanto, Fabiana [1 ]
Casalegno, Valentina [1 ]
Tatarko, Peter [2 ]
Salvo, Milena [1 ]
机构
[1] Politecn Torino, DISAT, Dept Appl Sci & Technol, Corso Duca Abruzzi 24, I-10129 Turin, Italy
[2] Slovak Acad Sci, Inst Inorgan Chem, Dubravska Cesta 9, Bratislava 84536, Slovakia
关键词
Joining; Glass; Ceramic matrix composites; INTERLAYER;
D O I
10.1016/j.jeurceramsoc.2020.10.022
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A key aspect of ceramic matrix composites integration is related to a reliable joining technique. An ytterbium disilicate based glass-ceramic material is processed by reactive viscous flow sintering between a barium aluminium borosilicate glass and ytterbium oxide and it is used to join SiC/SiC and C/SiC composites. The joining temperature and the in situ formation of the Yb2Si2O7 is optimised at 1200 degrees C without pressure, on the basis of the sintering and crystallisation mechanisms. The mechanical characterization of SiC/SiC and C/SiC joined with the ytterbium disilicate-based glass-ceramic, tested by single-lap offset at RT, exhibits an apparent shear strength of 35 MPa, similar to their interlaminar shear strength. The proposed system displays self-healing behaviour at 1000 degrees C and 1150 degrees C, as demonstrated by the partial and complete sealing of induced cracks by Vickers indentation on its surface at different loads, thus suggesting that it can effectively be used as promising joining material for CMCs.
引用
收藏
页码:1099 / 1106
页数:8
相关论文
共 50 条
  • [21] Fiber-Matrix Compatibility in LZSA Glass-Ceramic Matrix Composites
    Goushegir, S. M.
    Guglielmi, P. O.
    Oliveira, A. P. N.
    Hotza, D.
    Janssen, R.
    ADVANCED POWDER TECHNOLOGY VIII, PTS 1 AND 2, 2012, 727-728 : 562 - +
  • [22] The preparation of the lithium disilicate glass-ceramic with high translucency
    Bai, Yang
    Peng, Lian
    Zhu, Qingshan
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2017, 457 : 129 - 134
  • [23] Strengthening of a lithium disilicate glass-ceramic by rapid cooling
    Li, D.
    Li, X. C.
    Meng, M.
    Wei, R.
    He, L.
    Zhang, S. F.
    CERAMICS INTERNATIONAL, 2018, 44 (10) : 11650 - 11657
  • [24] Joining of silicon carbide with a cordierite glass-ceramic
    Perham, TJ
    De Jonghe, LC
    MoberlyChan, WJ
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (02) : 297 - 305
  • [25] Joining properties of a composite glass-ceramic sealant
    Gross, Sonja M.
    Koppitz, Thomas
    Remmel, Josef
    Bouche, Jean-Bernard
    Reisgen, Uwe
    Fuel Cells Bulletin, 2006, 2006 (09) : 12 - 15
  • [26] CHARACTERIZATION OF OXYNITRIDE GLASS-CERAMIC MATRIX SIC FIBER COMPOSITES
    HERRON, MA
    RISBUD, SH
    BRENNAN, JJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1984, 63 (12): : 1475 - 1475
  • [27] GLASS-CERAMIC MATRIX COMPOSITES WITH HIGH OXIDATION EMBRITTLEMENT RESISTANCE
    GADKAREE, KP
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (09) : 2417 - 2424
  • [28] Work of adhesion of resin on treated lithia disilicate-based ceramic
    Della Bona, A
    Shen, CY
    Anusavice, KJ
    DENTAL MATERIALS, 2004, 20 (04) : 338 - 344
  • [29] INTERFACIAL CHARACTERISTICS OF GLASS-CERAMIC MATRIX SIC FIBER COMPOSITES
    BRENNAN, JJ
    JOURNAL DE PHYSIQUE, 1988, 49 (C-5): : 791 - 809
  • [30] Glass-ceramic matrix composites made from industrial waste
    Rozenstrauha, I
    Cimdins, R
    Berzina, L
    Bajare, D
    Bossert, J
    Boccaccini, AR
    EURO CERAMICS VII, PT 1-3, 2002, 206-2 : 867 - 870