Influence of heat treatment on tribological properties of electroless Ni-P and Ni-P-Al2O3 coatings on Al-Si casting alloy

被引:54
|
作者
Novak, M. [1 ]
Vojtech, D. [1 ]
Vitu, T. [2 ]
机构
[1] Inst Chem Technol, Dept Met & Corros Engn, CR-16628 Prague 6, Czech Republic
[2] Czech Tech Univ, Dept Phys, CR-16628 Prague 6, Czech Republic
关键词
Al-Si alloy; Electroless coating; Heat treatment; Wear testing; WEAR PERFORMANCE;
D O I
10.1016/j.apsusc.2009.11.057
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Evolution of tribological properties of electroless Ni-P and Ni-P-Al2O3 coating on an Al-10Si-0.3Mg casting alloy during heat treatment is investigated in this work. The pre-treated substrate was plated using a bath containing nickel hypophosphite, nickel lactate and lactic acid. For preparation of fiber-reinforced coating Al2O3 Saffil fibers pre-treated in demineralised water were used. The coated samples were heat treated at 400-550 degrees C/1-8 h. Tribological properties were studied using the pin-on-disc method. It is found that the best coating performance is obtained using optimal heat treatment regime (400 degrees C/1 h). Annealing at higher temperatures (450 degrees C and above) leads to the formation of intermetallic compounds that reduce the coating wear resistance. The reason is that the intermetallic phases adversely affect the coating adherence to the substrate. The analysis of wear tracks proves that abrasion is major wear mechanism, however due to the formed intermetallic sub-layers, partial coating delamination may occur during the pin-on-disc test on the samples annealed at 450 degrees C and above. It was found that fiber reinforcement reduces this scaling and increases wear resistance of coatings as compared to the non-reinforced Ni-P coatings. (C) 2009 Elsevier B. V. All rights reserved.
引用
收藏
页码:2956 / 2960
页数:5
相关论文
共 50 条
  • [41] Duplex electroless Ni-P/Ni-P-W coatings: Effect of heat treatment on tribological and corrosion performance
    Biswas, Palash
    Das, Suman Kalyan
    Sahoo, Prasanta
    MATERIALS TODAY-PROCEEDINGS, 2022, 66 : 2237 - 2244
  • [42] Effect of Annealing Temperature and Alumina Particles on Mechanical and Tribological Properties of Ni-P-Al2O3 Composite Coatings
    Prasanna Gadhari
    Prasanta Sahoo
    Silicon, 2017, 9 : 761 - 774
  • [43] Effect of Electroless Ni-P Plating on the Fatigue Strength of Dilute Al-Si Alloys
    Nagata, Norihito
    Kanadani, Teruto
    Fukuhara, Minoru
    Hino, Makoto
    Murakami, Koji
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 290 - +
  • [44] Effect of pH on mechanical, physical and tribological properties of electroless Ni-P-Al2O3 composite deposits for marine applications
    Julka S.
    Ansari M.I.
    Thakur D.G.
    Journal of Marine Science and Application, 2016, 15 (4) : 484 - 492
  • [45] Effect of Annealing Temperature and Alumina Particles on Mechanical and Tribological Properties of Ni-P-Al2O3 Composite Coatings
    Gadhari, Prasanna
    Sahoo, Prasanta
    SILICON, 2017, 9 (05) : 761 - 774
  • [46] Effect of glycine as a complex agent on the surface and corrosion properties of Ni-P and Ni-P/Al2O3 electroless coating
    Omar, Refaie
    Oraby, Elsayed
    Abdelrhman, Yasser
    Aboraia, Mohammed
    ANTI-CORROSION METHODS AND MATERIALS, 2020, 67 (06) : 593 - 603
  • [47] Ni-P-Al2O3复合镀层
    张翼
    沈光伟
    李亚文
    周雅萍
    安志勇
    大庆石油学院学报, 1998, (02) : 34 - 36+92
  • [48] Electrodeposition of Ni-P-Al2O3 deposits
    Sheffield Hallam Univ, Sheffield, United Kingdom
    Surf Coat Technol, 2-3 (353-358):
  • [49] Effects of Content of Al2O3 Particles and Heat Treatment on Corrosion Resistance of Ni-P-Al2O3 Composite Coatings
    Lu, Jian-hua
    Sun, Wan-chang
    Zhu, Ming
    Tan, Ming-feng
    Zhou, Quan
    CHINESE CERAMICS COMMUNICATIONS, 2010, 105-106 : 441 - 443
  • [50] Effect of alumina content on surface morphology and hardness of Ni-P-Al2O3(α) electroless composite coatings
    Alirezaei, S
    Monirvaghefi, SM
    Salehi, M
    Saatchi, A
    SURFACE & COATINGS TECHNOLOGY, 2004, 184 (2-3): : 170 - 175