Ageing effects on the nanoindentation response of sub-micrometric 3Y-TZP ceramics

被引:25
|
作者
Guicciardi, Stefano
Shimozono, Takayoshi
Pezzotti, Giuseppe
机构
[1] CNR, ISTEC, Inst Sci & Technol Ceram, I-48018 Faenza, Italy
[2] Kyoto Inst Technol, Ceram Phys La, Sakyo Ku, Kyoto 6068585, Japan
[3] Kyoto Inst Technol, RIN, Sakyo Ku, Kyoto 6068585, Japan
关键词
D O I
10.1007/s10853-006-1177-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The surface mechanical response, specifically hardness and Young's modulus, of two thermally aged 3Y-TZP ceramics with different grain size was evaluated by depth-sensing indentation tests. The ageing treatment were carried out in autoclave at 121°C with a water vapor pressure of 0.235 MPa for different times. The depth-sensing indentation tests were carried out using a Berkovich diamond tip on a commercial nanoindenter. The presence of microcracking in the transformed layer have been formulated only on the basis of the nanoindentation outcomes. The surface mechanical behavior of aged zirconia ceramics was influenced, at different sampling depths, by ageing time and mean grain size. Ageing treatment have been shown to replicate the transformation effects observed in retrieved prostheses and the assessment of the surface mechanical behavior gives useful information about the wear and contact properties of these aged ceramics.
引用
收藏
页码:718 / 722
页数:5
相关论文
共 50 条
  • [31] Subcritical crack propagation in 3Y-TZP ceramics: Static and cyclic fatigue
    Chevalier, J
    Olagnon, C
    Fantozzi, G
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (11) : 3129 - 3138
  • [32] The Effects of Sintering Additives on the Sintering of 3Y-TZP Ceramic
    Theenagaran, S.
    Ting, C. H.
    Chin, K. L.
    Yeo, W. H.
    Ng, C. K.
    Ramesh, S.
    Teng, W. D.
    INTERNATIONAL CONFERENCE ON ADVANCED ENGINEERING AND TECHNOLOGY (ICAET 2020), 2021, 1117
  • [33] Porosity-dependence of elastic moduli and hardness of 3Y-TZP ceramics
    Luo, J
    Stevens, R
    CERAMICS INTERNATIONAL, 1999, 25 (03) : 281 - 286
  • [34] Preparation and properties of anti-static coating on the 3Y-TZP ceramics
    Yang, Xianfeng
    Ni, Zhentao
    Yang, Xiaole
    He, Qinglong
    Xie, Hehan
    Xu, Xiewen
    Xie, Zhipeng
    CERAMICS INTERNATIONAL, 2018, 44 (14) : 16459 - 16463
  • [35] Microstructure and mechanical properties of 3Y-TZP ceramics by low temperature sintering
    Sun, Yihai
    Zhang, Yufeng
    Guo, Jingkun
    Kuei Suan Jen Hsueh Pao/ Journal of the Chinese Ceramic Society, 2002, 30 (03): : 267 - 271
  • [36] Effects of Composition and Additives on the Mechanical Characteristics of 3Y-TZP
    Park, Mi-Jung
    Yang, Seong-Koo
    Kang, Jong-Bong
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2006, 43 (10) : 640 - 645
  • [37] Towards the prediction of hydrothermal ageing of 3Y-TZP bioceramics from processing parameters
    Wei, Chong
    Gremillard, Laurent
    ACTA MATERIALIA, 2018, 144 : 245 - 256
  • [38] Stability of 3Y-TZP nano zirconia powder after hydrothermal ageing treatment
    Ahmed, Shafique
    Zou, Lifong
    Yan, Haixue
    ADVANCES IN APPLIED CERAMICS, 2022, 121 (5-8) : 159 - 165
  • [39] In vivo ageing of zirconia dental ceramics - Part II: Highly-translucent and rapid-sintered 3Y-TZP
    Cotic, Jasna
    Kocjan, Andraz
    Panchevska, Sanja
    Kosmac, Tomaz
    Jevnikar, Peter
    DENTAL MATERIALS, 2021, 37 (03) : 454 - 463
  • [40] Characterisation of Ce0.8Gd0.2O1.9/3Y-TZP composite electrolytes—Effects of 3Y-TZP particle treatment
    R. J. Ball
    R. Stevens
    Journal of Materials Science, 2002, 37 : 4137 - 4144