Evaluation of Mn substitution for Ni in alumina-forming austenitic stainless steels

被引:55
|
作者
Yamamoto, Y. [1 ,2 ]
Santella, M. L. [1 ,2 ]
Liu, C. T. [2 ]
Evans, N. D. [1 ]
Maziasz, P. J. [1 ]
Brady, M. P. [1 ]
机构
[1] Oak Ridge Natl Lab, Mat Sci & Technol Div, Oak Ridge, TN 37831 USA
[2] Univ Tennessee, Dept Mat Sci & Engn, Knoxville, TN 37996 USA
基金
美国能源部;
关键词
Austenitic stainless steels; Alumina-forming; High-Mn containing alloys; HIGH-TEMPERATURE OXIDATION; CREEP-RESISTANT; SCALE FORMATION; WATER-VAPOR; ALLOYS; ADDITIONS; PHASE;
D O I
10.1016/j.msea.2009.06.043
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
There has been increasing interest in the substitution of low-cost Mn for Ni in austenitic stainless steels due to the rising price of Ni. This paper investigates the possibility of such a substitution approach for the recently developed alumina (Al2O3)-forming austenitic (AFA) class of heat-resistant stainless steels. Computational thermodynamic tools were utilized to predict the alloy composition range to maintain an austenitic matrix microstructure when Mn is substituted for Ni in the presence of Al, which is a strong body-centered-cubic (BCC) phase stabilizer. Phase equilibria, oxidation behavior, and creep properties of Fe-(10-14)Cr-(5-15)Mn-(4-12)Ni-(2.5-3)Al-Cu-Nb-C-B (in weight percent) based alloys were studied. The alloys based on Fe-14Cr-2.5Al-(5-9)Mm-(10-12)Ni exhibited the best balance of oxidation and creep resistance, which represents approximately 50% reduction in Ni content compared to previously developed AFA alloys. These low-Ni, high-Mn AFA alloys formed protective Al2O3 scales up to 973-1073 K in air and at 923 K in air with 10% water vapor. Creep-rupture lives of the alloys under a severe screening condition of 1023 K and 100 MPa were in the 7.2 x 10(5)-1.8 x 10(6) s (200-500 h) range, which is comparable to or somewhat improved over that of type 347 stainless steel (Fe-18Cr-11Ni base). (C) 2009 Elsevier B.V. All rights reserved.
引用
下载
收藏
页码:176 / 185
页数:10
相关论文
共 50 条
  • [21] The negative effect of Zr addition on the high temperature strength in alumina-forming austenitic stainless steels
    Moon, Joonoh
    Jang, Min-Ho
    Kang, Jun-Yun
    Lee, Tae-Ho
    MATERIALS CHARACTERIZATION, 2014, 87 : 12 - 18
  • [22] Effect of Mn content on the high-temperature oxidation behaviors of Mn-substituted-for-Ni alumina-forming austenitic stainless steel
    Zhao, Yanjun
    Chen, Peilin
    Wen, Weiying
    Deng, Yongjie
    Peng, Kaiwei
    Liu, Yafei
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 7816 - 7828
  • [23] Compatibility of Alumina-Forming Austenitic Steels in Static and Flowing Pb
    Bruce A. Pint
    Yi-Feng Su
    Michael P. Brady
    Yukinori Yamamoto
    Jiheon Jun
    Michael R. Ickes
    JOM, 2021, 73 : 4016 - 4022
  • [24] Compatibility of Alumina-Forming Austenitic Steels in Static and Flowing Pb
    Pint, Bruce A.
    Su, Yi-Feng
    Brady, Michael P.
    Yamamoto, Yukinori
    Jun, Jiheon
    Ickes, Michael R.
    JOM, 2021, 73 (12) : 4016 - 4022
  • [25] Modelling internal nitridation in an alumina-forming austenitic stainless steel
    Elger, R.
    Magnusson, H.
    Frisk, K.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2017, 68 (02): : 143 - 150
  • [26] Effect of tungsten on the oxidation of alumina-forming austenitic stainless steel
    Kang J.-Y.
    Ha H.-Y.
    Kim S.-D.
    Park J.Y.
    Jang M.-H.
    Lee T.-H.
    Applied Microscopy, 2019, 49 (01)
  • [27] Effect of cold rolling and annealing on the microstructure and mechanical properties of Mn-substituted-for-Ni alumina-forming austenitic stainless steel
    Wen, Weiying
    Zhao, Yanjun
    Chen, Peilin
    Deng, Yongjie
    Peng, Kaiwei
    Liu, Yafei
    MATERIALS TODAY COMMUNICATIONS, 2023, 35
  • [28] Overview of Strategies for High-Temperature Creep and Oxidation Resistance of Alumina-Forming Austenitic Stainless Steels
    Y. Yamamoto
    M.P. Brady
    M.L. Santella
    H. Bei
    P.J. Maziasz
    B.A. Pint
    Metallurgical and Materials Transactions A, 2011, 42 : 922 - 931
  • [29] The Effects of Cold Work on the Microstructure and Mechanical Properties of Intermetallic Strengthened Alumina-Forming Austenitic Stainless Steels
    Hu, B.
    Trotter, G.
    Baker, Ian
    Miller, M. K.
    Yao, L.
    Chen, S.
    Cai, Z.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (08): : 3773 - 3785
  • [30] Composition, Microstructure, and Water Vapor Effects on Internal/External Oxidation of Alumina-Forming Austenitic Stainless Steels
    M. P. Brady
    Y. Yamamoto
    M. L. Santella
    L. R. Walker
    Oxidation of Metals, 2009, 72 : 311 - 333