Fracture Resistance of Various Thickness e.max CAD Lithium Disilicate Crowns Cemented on Different Supporting Substrates: An In Vitro Study

被引:20
|
作者
Chen, Sara Elizabeth [1 ]
Park, Albert Christopher [1 ]
Wang, Jingxu [2 ]
Knoernschild, Kent L. [1 ]
Campbell, Stephen [1 ]
Yang, Bin [1 ]
机构
[1] Univ Illinois Chicago Restorat Dent, Chicago, IL 60612 USA
[2] Guangzhou Med Univ, Dept Stomatol, Affiliated Hosp 1, Guangzhou, Peoples R China
关键词
Monolithic; occlusal thickness; load-bearing capacity; preparation design; all ceramic crown; ultra-thin crown;
D O I
10.1111/jopr.13108
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To investigate the influence of abutment material properties on the fracture resistance and failure mode of lithium disilicate (IPS e.max) CAD/CAM (computer-aided design/manufacturing) crowns on traditionally and minimally prepared simulated tooth substrates. Materials and Methods: Thirty lithium disilicate (IPS e.max) CAD/CAM crowns were divided into three groups (n = 10): TD: traditional thickness crowns cemented on Paradigm MZ100 abutments; MD: minimal thickness crowns cemented on Paradigm MZ100 abutments; ME: minimal thickness crowns cemented on e.max abutments. The 3Shape system was used to scan, design and mill all abutments and crowns with a die space set to 40 mu m. Traditional thickness crowns were designed based on manufacturer guidelines with 1.5 mm occlusal thickness and 1.0 mm margins. Minimal thickness crowns were designed with 0.7 mm occlusal thickness and 0.5 mm margins. MZ100 composite and e.max abutments were selected to simulate dentin and enamel substrates, respectively, based on their elastic-modulus. Variolink Esthetic was used to cement all samples following manufacturer's instructions. A universal testing machine was used to load all specimens to fracture with a 3 mm radius stainless steel hemispherical tip at a crosshead speed 0.5 mm/minute along the longitudinal axis of the abutment with a 1 mm thermoplastic film placed between the loading tip and crown surface. Data was analyzed using ANOVA and Bonferroni post hoc assessment. Fractographic analysis was performed with scanning electron microscopy (SEM). Results: The mean fracture load (standard deviation) was 1499 (241) N for TD; 1228 (287) N for MD; and 1377 (96) N for ME. Statistically significant difference between groups did not exist (p= 0.157, F= 1.995). In groups TD and MD with lowe-modulus abutments, the dispersion of a probability distribution (coefficient of variation: CV) was statistically higher than that of group ME with high e-modulus abutments. SEM illustrated larger micro-fracture dimensions in Group MD than Group ME. Conclusion: Minimal thickness e.max crowns did not demonstrate statistical difference in fracture resistance from traditional thickness crowns. Fracture mechanisms of minimal thickness e.max crowns may be affected by the e-modulus of the substrate. Minimal thickness e.max crowns may be a viable restorative option when supported by high e-modulus materials.
引用
收藏
页码:997 / 1004
页数:8
相关论文
共 50 条
  • [21] RETRACTED: Influence of Resin Cements and Aging on the Fracture Resistance of IPS e.max Press Posterior Crowns (Retracted Article)
    Abou-Madina, Manal M.
    Oezcan, Mutlu
    Abdelaziz, Khalid M.
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2012, 25 (01) : 33 - 35
  • [22] Fracture Resistance of Zirconia-Reinforced Lithium Silicate Ceramic Crowns Cemented with Conventional or Adhesive Systems: An In Vitro Study
    D'Addazio, Gianmaria
    Santilli, Manlio
    Rollo, Marco Lorenzo
    Cardelli, Paolo
    Rexhepi, Imena
    Murmura, Giovanna
    Husain, Nadin Al-Haj
    Sinjari, Bruna
    Traini, Tonino
    Ozcan, Mutlu
    Caputi, Sergio
    MATERIALS, 2020, 13 (09)
  • [23] Fracture resistance of endodontically treated premolars restored with lithium disilicate CAD/CAM crowns or onlays and luted with two luting agents
    Yu, Weiqiang
    Guo, Kewu
    Zhang, Baowei
    Weng, Weimin
    DENTAL MATERIALS JOURNAL, 2014, 33 (03) : 349 - 354
  • [24] Effect of Die Spacer Thickness on the Fracture Resistance of CAD/CAM Lithium Disilicate Veneers on Maxillary First Premolars
    Farag, Sherine Mohamed
    Ghoneim, Mona Mohamed
    Afifi, Rania Reda
    CLINICAL COSMETIC AND INVESTIGATIONAL DENTISTRY, 2021, 13 : 223 - 230
  • [25] Fracture resistance of metal- and galvano-ceramic crowns cemented with different luting cements: In vitro comparative study
    Ghazy, Mohamed H.
    Madina, Manal M. Abo
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2006, 19 (06) : 610 - 612
  • [26] Fracture Resistance of Molar Crowns Fabricated with Monolithic All-Ceramic CAD/CAM Materials Cemented on Titanium Abutments: An In Vitro Study
    Dogan, Derya Ozdemir
    Gorler, Oguzhan
    Mutaf, Burcu
    Ozcan, Mutlu
    Eyuboglu, Gunes Bulut
    Ulgey, Melih
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2017, 26 (04): : 309 - 314
  • [27] Fracture resistance of lithium disilicate restorations after endodontic access preparation: An in vitro study
    Bompolaki, Despoina
    Kontogiorgos, Elias
    Wilson, John B.
    Nagy, William W.
    JOURNAL OF PROSTHETIC DENTISTRY, 2015, 114 (04): : 580 - 586
  • [28] Fracture Resistance of Chairside CAD/CAM Lithium Disilicate- reinforced Ceramic Occlusal Veneers With and Without Margin and Full Coverage Crowns
    Jurado, C. A.
    Lee, D.
    Ramirez, P.
    Cortes-Trevino, D. A.
    Tsujimoto, A.
    OPERATIVE DENTISTRY, 2024, 49 (01) : 84 - 90
  • [29] In vitro study of compressive fracture strength of Empress 2 crowns cemented with various luting agents.
    Kim, MH
    Yang, JH
    JOURNAL OF DENTAL RESEARCH, 2001, 80 (04) : 1350 - 1350
  • [30] Fracture resistance of chairside CAD-CAM lithium disilicate occlusal veneer with various designs after mechanical aging
    Jurado, Carlos A.
    Tsujimoto, Akimasa
    Molisani, Joseph
    Fu, Chin-Chuan
    Sadid-Zadeh, Ramtin
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2025, 34 (03): : 323 - 328