Comparison of lanthanum substituted bismuth titanate (BLT) thin films deposited by sputtering and pulsed laser deposition

被引:31
|
作者
Besland, MP
Aissa, HDA
Barroy, PRJ
Lafane, S
Tessier, PY
Angleraud, B
Richard-Plouet, M
Brohan, L
Djouadi, MA
机构
[1] Univ Nantes, Inst Mat Jean Rouxel, CNRS, UMR 6502, F-44322 Nantes, France
[2] CDTA, Div Milieux Lonises & Lasers, Algiers, Algeria
关键词
thin films deposition; PVD magnetron; PLD; aurivillius phase; BLT oxide;
D O I
10.1016/j.tsf.2005.08.154
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Bi4-xLaxTi3O12 (BLTx), (x=0 to 1) thin films were grown on silicon (100) and platinized substrates Pt/TiO2/SiO2/Si using RF diode sputtering, magnetron sputtering and pulsed laser deposition (PLD). Stoichiometric home-synthesized targets were used. Reactive sputtering was investigated in argon/oxygen gas mixture, with a pressure ranging from 0.33 to 10 Pa without heating the substrate. PLD was investigated in pure oxygen, at a chamber pressure of 20 Pa for a substrate temperature of 400-440 degrees C. Comparative structural, chemical, optical and morphological characterizations of BLT thin films have been performed by X-ray diffraction (XRD), Scanning Electron Microscopy (SEM), Energy Dispersive Spectroscopy (EDS), X-Ray Photoelectron Spectroscopy (XPS), Spectro-ellipsometric measurements (SE) and Atomic Force Microscopy (AFM). Both sputtering techniques allow to obtain uniform films with thickness ranging from 200 to 1000 nm and chemical composition varying from (Bi,La)(2) Ti-3 O-12 to (Bi,La)(4.5)Ti3O12, depending on deposition pressure and RF power. In addition, BLT films deposited by magnetron sputtering, at a pressure deposition ranging from 1.1 to 5 Pa, were well-crystallized after a post-deposition annealing at 650 C in oxygen. They exhibit a refractive index and optical band gap of 2.7 and 3.15 eV, respectively. Regarding PLD, single phase and well-crystallized, 100-200 nm thick BLT films with a stoichiometric (Bi,La)(4)Ti3O12 chemical composition were obtained, exhibiting in addition a preferential orientation along (200). It is worth noting that BLT films deposited by magnetron sputtering are as well-crystallized than PLD ones. (c) 2005 Elsevier B.V All rights reserved.
引用
收藏
页码:86 / 91
页数:6
相关论文
共 50 条
  • [21] Dielectric properties of lead lanthanum zirconate stanate titanate antiferroelectric thin films prepared by pulsed laser deposition
    Yao, YB
    Zhai, JW
    Chen, HD
    JOURNAL OF APPLIED PHYSICS, 2004, 95 (11) : 6341 - 6346
  • [22] Microwave dielectric properties of bismuth zinc niobate thin films deposited on alumina by pulsed laser deposition
    Wang, Zhao
    Ren, Wei
    Zhang, Xiaohua
    Shi, Peng
    Wu, Xiaoqing
    Chen, Xiaofeng
    CERAMICS INTERNATIONAL, 2013, 39 : S491 - S495
  • [23] Yttria-stabilized zirconia thin films deposited by pulsed-laser deposition and magnetron sputtering
    Hidalgo, H.
    Reguzina, E.
    Millon, E.
    Thomann, A. -L.
    Mathias, J.
    Boulmer-Leborgne, C.
    Sauvage, T.
    Brault, P.
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (19): : 4495 - 4499
  • [24] Characterization of zirconium thin films deposited by pulsed laser deposition
    刘伟
    万竟平
    蔡吴鹏
    梁建华
    周晓松
    龙兴贵
    Chinese Physics B, 2014, (09) : 500 - 505
  • [25] Transparent PLT thin films deposited by pulsed laser deposition
    Xiong, S.B.
    Liu, Z.G.
    Xu, N.
    Ferroelectrics, 1997, 195 (1 -4 pt 1): : 171 - 174
  • [26] Characterization of zirconium thin films deposited by pulsed laser deposition
    Liu Wei
    Wan Jing-Ping
    Cai Wu-Peng
    Liang Jian-Hua
    Zhou Xiao-Song
    Long Xing-Gui
    CHINESE PHYSICS B, 2014, 23 (09)
  • [27] Transparent PLT thin films deposited by pulsed laser deposition
    Xiong, SB
    Liu, ZG
    Xu, N
    FERROELECTRICS, 1997, 195 (1-4) : 171 - 174
  • [28] ITO thin films deposited by advanced pulsed laser deposition
    Viespe, Cristian
    Nicolae, Ionut
    Sima, Comelia
    Grigorlu, Constantin
    Medianu, Rares
    THIN SOLID FILMS, 2007, 515 (24) : 8771 - 8775
  • [29] Optical Properties of Nitrogen-Substituted Strontium Titanate Thin Films Prepared by Pulsed Laser Deposition
    Marozau, Ivan
    Shkabko, Andrey
    Doebeli, Max
    Lippert, Thomas
    Logvinovich, Dimitri
    Mallepell, Marc
    Schneider, Christof W.
    Weidenkaff, Anke
    Wokaun, Alexander
    MATERIALS, 2009, 2 (03) : 1388 - 1401
  • [30] Pulsed laser deposition of lanthanum monosulfide thin films on silicon substrates
    Fairchild, S
    Jones, J
    Cahay, M
    Garre, K
    Draviam, P
    Boolchand, P
    Wu, X
    Lockwood, DJ
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 2005, 23 (01): : 318 - 321