Effect of fatigue on biaxial flexural strength of bilayered porcelain/zirconia (Y-TZP) dental ceramics

被引:31
|
作者
Yilmaz, Handan [1 ]
Nemli, Secil Karakoca [1 ]
Aydin, Cemal [1 ]
Bal, Bilge Turhan [1 ]
Tiras, Tulay [2 ]
机构
[1] Gazi Univ, Dept Prosthodont, Fac Dent, TR-06510 Ankara, Turkey
[2] Anadolu Univ, Dept Phys, Fac Sci, Eskisehir, Turkey
关键词
Zirconia; Bilayer; Fatigue; Biaxial flexural strength; Formulas; Raman spectroscopy; FIXED PARTIAL DENTURES; LOAD-BEARING CAPACITY; SURFACE CHARACTERIZATION; MECHANICAL-PROPERTIES; PHASE-TRANSFORMATION; STABILIZED ZIRCONIA; RAMAN-SPECTROSCOPY; FRACTURE SURFACE; BRIDGES; WATER;
D O I
10.1016/j.dental.2011.03.019
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The aim of this study was to evaluate the effect of fatigue on biaxial flexural strength of bilayered disks of two Y-TZP cores. Methods. Twenty bilayered veneer/zirconia disks were fabricated from each material (Lava veneer + core, 3 M/ESPE, and Cercon veneer + core, Densply). Ten specimens from each material were tested for biaxial flexural strength either with or without being subjected to fatigue (20,000 cycles, 2 Hz, 200 N load) in a universal testing machine (1 mm/min). Stresses generated at the core and the veneer, at the top and the bottom surfaces, and the interface of bilayered disk were calculated using Huesh's solutions. Data were statistically analyzed using Weibull statistics. The fractured core was also examined via Raman spectroscopy and the monoclinic fraction was calculated at the top, the middle of thickness, and the bottom of the cross-section of fractured core. The results of monoclinic fraction were statistically analyzed by Three-Factor ANOVA with Repeated Measures on One Factor. Results. Weibull modulus (m) of Cercon control (CC), Cercon fatigue (CF), Lava control (LC) and Lava fatigue (LF) were between 11.8 and 14.3, 7.1 and 13.1, 9.4 and 13, and 7.1 and 8.2, respectively. There were no significant differences between characteristic strength (sigma(0)) of CC (970.9 MPa) and CF (947.7 MPa) (p > 0.05). For Lava, sigma(0) of LF (1444.8 MPa) was significantly higher than LC (1240.5 MPa) (p < 0.05). At the interfaces, sigma(0) values of CC and CF groups were not significantly different while LF showed significantly higher sigma(0) than LC. The monoclinic zirconia was significantly lower for CF than CC and significantly higher for LF than LC. Significance. Fatigue showed different effects on the strength of Cercon and Lava ceramic systems. Decreases in m values were observed at the interfaces of two materials after fatigue. (C) 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:786 / 795
页数:10
相关论文
共 50 条
  • [21] Influence of Low Temperature Aging on the Flexural Strength of Y-TZP Ceramics
    Wang, Chen
    Dong, Limin
    Yi, Yuanfu
    Wen, Ning
    Zan, Qingfeng
    Tian, Jiemo
    HIGH-PERFORMANCE CERAMICS VII, PTS 1 AND 2, 2012, 512-515 : 1756 - +
  • [22] Biaxial flexural strength of the bilayered disk composed of ceria-stabilized zirconia/alumina nanocomposite (Ce-TZP/A) and veneering porcelain
    Sawada, Tomofumi
    Schille, Christine
    Wagner, Verena
    Spintzyk, Sebastian
    Schweizer, Ernst
    Geis-Gerstorfer, Juergen
    DENTAL MATERIALS, 2018, 34 (08) : 1199 - 1210
  • [23] Effects of Pretreatment, Specimen Thickness, and Artificial Aging on Biaxial Flexural Strength of Two Types of Y-TZP Ceramics
    Sundh, A.
    Kou, W.
    Sjogren, G.
    OPERATIVE DENTISTRY, 2019, 44 (06) : 615 - 624
  • [24] Effect of anelasticity on fatigue behavior in Y-TZP ceramics
    Horibe, S
    FATIGUE '99: PROCEEDINGS OF THE SEVENTH INTERNATIONAL FATIGUE CONGRESS, VOLS 1-4, 1999, : 1521 - 1526
  • [25] Ageing and fatigue behaviour of surface treated Y-TZP dental ceramics
    Kosmac, Tomaz
    Oblak, Cedomir
    BIOCERAMICS, VOL 20, PTS 1 AND 2, 2008, 361-363 : 817 - +
  • [26] Effect of surface treatments and aging on phase transformation and flexural strength of different Y-TZP ceramics
    Okutan, Yener
    Yucel, Munir T.
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2019, 16 (04) : 1425 - 1440
  • [27] The effect of zirconia thickness on the biaxial flexural strength of zirconia-ceramic bilayered discs
    Sinmazisik, Gulden
    Tarcin, Bilge
    Demirbas, Bulent
    Gulmez, Turgut
    Bor, Emire
    Ozer, Fusun
    DENTAL MATERIALS JOURNAL, 2015, 34 (05) : 640 - 647
  • [28] Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    Guazzato, M
    Quach, L
    Albakry, M
    Swain, MV
    JOURNAL OF DENTISTRY, 2005, 33 (01) : 9 - 18
  • [29] Flexural Strength, Fatigue Life, and Stress-Induced Phase Transformation Study of Y-TZP Dental Ceramic
    Pittayachawan, Piyapanna
    McDonald, Ailbhe
    Young, Anne
    Knowles, Jonathan C.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2009, 88B (02) : 366 - 377
  • [30] Effects of core-to-dentin thickness ratio on the biaxial flexural strength, reliability, and fracture mode of bilayered materials of zirconia core (Y-TZP) and veneer indirect composite resins
    Su, Naichuan
    Liao, Yunmao
    Zhang, Hai
    Yue, Li
    Lu, Xiaowen
    Shen, Jiefei
    Wang, Hang
    JOURNAL OF PROSTHETIC DENTISTRY, 2017, 117 (01): : 150 - 157