Corrosion Testing of CrNx-Coated 310 H Stainless Steel under Simulated Supercritical Water Conditions

被引:4
|
作者
Tudose, Aurelia Elena [1 ,2 ]
Golgovici, Florentina [2 ]
Anghel, Alexandru [3 ]
Fulger, Manuela [1 ]
Demetrescu, Ioana [2 ,4 ]
机构
[1] Inst Nucl Res Pitesti, Pob 78,Campului St 1, Mioveni 115400, Romania
[2] Univ Politech Bucharest, Dept Gen Chem, Splaiul Independentei St 313, Bucharest 060042, Romania
[3] Natl Inst Laser Plasma & Radiat Phys, Atomistilor St, Magurele 077126, Romania
[4] Acad Romanian Scientists, 3 Ilfov, Bucharest 050094, Romania
关键词
corrosion; oxidation; CrNx coating; SEM; XRD; EIS; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; NACL AQUEOUS-SOLUTION; MECHANICAL-PROPERTIES; NITRIDE COATINGS; CHROMIUM NITRIDE; ARC PLASMA; BEHAVIOR; RESISTANCE; PVD; TIN;
D O I
10.3390/ma15165489
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The paper's aim is the assessment of corrosion behaviour of a CrNx-coated 310 H stainless steel under simulated supercritical water conditions (550 degrees C and 25 MPa) for up to 2160 h. The CrNx coating was obtained by the thermionic vacuum arc (TVA) method. The oxides grown on this coating were characterized using metallographic and gravimetric analysis, SEM with EDS, and grazing incidence X-ray diffraction (GIXRD). A diffusion mechanism drives oxidation kinetics because it follows a parabolic law. By XRD analysis, the presence of Cr2O3 and Fe3O4 on the surface of the autoclaved CrNx-coated 310 H samples were highlighted. Corrosion susceptibility assessment was performed by electrochemical impedance spectroscopy (EIS) and linear potentiodynamic polarization. EIS impedance spectra show the presence of two capacitive semicircles in the Nyquist diagram, highlighting both the presence of the CrNx coating and the oxide film formed during autoclaving on the 310 H stainless steel. Very low corrosion rates, with values up to 11 nm x year(-1), obtained in the case of autoclaved for 2160 h, CrNx-coated samples indicated that the oxides formed on these samples are protective and provide better corrosion resistance. The determination of micro hardness Vickers completed the above investigation.
引用
收藏
页数:18
相关论文
共 50 条
  • [41] Effect of Working Medium Pressure and Creep on the Stress Corrosion Cracking Behavior of Cold Deformed 310S Stainless Steel in Supercritical Water Environment
    Su H.
    Wang P.
    Zhang L.
    [J]. Hedongli Gongcheng/Nuclear Power Engineering, 2022, 43 (06): : 108 - 116
  • [42] Erosion corrosion in stainless steel pipe under water vapour two-phase flow conditions
    Koike, MH
    [J]. CORROSION SCIENCE, 2006, 48 (03) : 617 - 624
  • [43] Corrosion studies of stainless steel 316L, modified by ion beam techniques, under simulated physiological conditions
    Meinert, K
    Wolf, GK
    [J]. SURFACE & COATINGS TECHNOLOGY, 1998, 98 (1-3): : 1148 - 1156
  • [44] Oxidation behavior of Incoloy 800 under simulated supercritical water conditions
    Fulger, M.
    Ohai, D.
    Mihalache, M.
    Pantiru, M.
    Malinovschi, V.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2009, 385 (02) : 288 - 293
  • [45] Corrosion studies of stainless steel 316L, modified by ion beam techniques, under simulated physiological conditions
    Universität Heidelberg, Phys. Chemisches Inst./Radiochemie, Im Neuenheimer Feld 500, 69120 Heidelberg, Germany
    [J]. Surf. Coat. Technol., 1-3 (1148-1156):
  • [46] Corrosion of Weathering Steel under Light Illumination and Simulated Atmospheric Conditions
    Qiu, Xiangxiao
    Li, Jifeng
    Liu, Zhanqing
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (04): : 3236 - 3244
  • [47] Preparation of Different Coatings on 316 L Stainless Steel and their Corrosion Performance in Supercritical Water
    Wang Y.-Z.
    Gao F.
    Yang J.-Q.
    Li J.
    Zhu Y.-T.
    Fang C.-Q.
    Wang S.-Z.
    [J]. Wang, Yu-Zhen (yzwang@xaut.edu.cn), 1600, Zhejiang University (31): : 1177 - 1185
  • [48] Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water
    Du, Donghai
    Chen, Kai
    Zhang, Lefu
    Shen, Zhao
    [J]. CORROSION SCIENCE, 2020, 170
  • [49] CORROSION BEHAVIORS OF NUCLEAR-GRADE STAINLESS STEEL AND FERRITIC-MARTENSITIC STEEL IN SUPERCRITICAL WATER
    Zhong Xiangyu
    Wu Xinqiang
    Han En-Hou
    [J]. ACTA METALLURGICA SINICA, 2011, 47 (07) : 932 - 938
  • [50] Oxidation Behavior of Austenitic Stainless Steel 316L and 310S in Air and Supercritical Water
    Nezakat, Majid
    Akhiani, Hamed
    Penttila, Sami
    Szpunar, Jerzy
    [J]. JOURNAL OF NUCLEAR ENGINEERING AND RADIATION SCIENCE, 2016, 2 (02):