Phase formation and stability of polycrystalline NaxGa4+xTi1-xO8, (x∼0.7)

被引:4
|
作者
Amoroso, Jake W. [1 ]
Edwards, Doreen D. [1 ]
机构
[1] Alfred Univ, Sch Engn, NYS Coll Ceram, Alfred, NY 14802 USA
关键词
sodium gallium titanate; 1-D conductors; beta-gallia-rutile intergrowths; alkali-ion conductors;
D O I
10.1016/j.ssi.2008.01.062
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The formation and stability of polycrystalline NaxGa4+xTi1-xO8, (x similar to 0.7) was examined. High temperature x-ray diffraction (HTXRD) showed that NaxGa4+xTi1-xO8, (x similar to 0.7), begins to form from component oxides and carbonates at similar to 950 degrees C and shows complete reaction within 24 h while being held at 1050 degrees C. The desired Na0.7Ga4.7Ti0.3O8 phase remains only nominally phase pure with residual gallium oxide identifiable. Further heating of the reacted material results in the decomposition of the material beginning at similar to 1200 degrees C in which Ga2O3 and other intermediate phases are seen in the diffraction pattern. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:878 / 880
页数:3
相关论文
共 50 条
  • [31] Preparation and structural analysis of Fe2+xTi1-x thin films in the C14 Laves phase stability range
    Köble, J
    Huth, M
    JOURNAL OF CRYSTAL GROWTH, 2002, 234 (04) : 666 - 678
  • [32] LATTICE INSTABILITIES IN SINGLE-PHASE POLYCRYSTALLINE Y1-XCAXBA2CU4O8 (X=0, 0.005, 0.1)
    WU, T
    FOSSHEIM, K
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1993, 6 (12): : 827 - 836
  • [33] Li1+xFe1-3xTi1+2xO4 (0.0 ≤ x ≤ 0.33) based spinels:: Possible negative electrode materials for future Li-ion batteries
    Robertson, AD
    Tukamoto, H
    Irvine, JTS
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (11) : 3958 - 3962
  • [34] FORMATION OF A HEAVY FERMION PHASE IN UCU4+XAL8-X BY VARIATION OF STOICHIOMETRY
    GEIBEL, C
    AHLHEIM, U
    GIORGI, AL
    SPARN, G
    SPILLE, H
    STEGLICH, F
    SUSKI, W
    PHYSICA B, 1990, 163 (1-3): : 194 - 196
  • [35] Determination of Structuralers of Type Solid Solutions Ba1-3XGd2XTi1-3XEu4XO3. (X=0.1, 0.15, 0.3, and 0.6% by Weight)
    Martinez Lopez, Ricardo
    Perez Labra, Miguel
    Barrientos Hernandez, Francisco Raul
    Reyes Perez, Martin
    Juarez Tapia, Julio Cesar
    Teja Ruiz, Aislinn Michelle
    Reyes Cruz, Victor Esteban
    Cobos Murcia, Jose Angel
    TMS 2022 151ST ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2022, : 579 - 586
  • [36] Electrical and magnetic properties of spinel solid solutions Mg2-xTi1+xO4; 0 [less-than or equal to] x [less-than or equal to] 1
    Universität Konstanz, Fakultät für Physik, Postfach 5560, D-78434 Konstanz, Germany
    不详
    J. Solid State Chem., 2 (216-223):
  • [37] Li conductivity in Li1+xTi2-xAlx(PO4)3 (0.3 ≤ x ≤ 0.7) ceramics prepared from sol-gel precursors
    Jimenez, R.
    Sobrados, I.
    Martinez, S.
    Criado, M.
    Perea, B.
    Sanz, J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 844 (844)
  • [38] Incommensurate modulations in a hollandite phase Bax(Al,Fe)2xTi8-2xO16 intended for the storage of radioactive wastes:: a (3+1) dimension structure determination
    Aubin-Chevaldonnet, Virginie
    Deniard, Philippe
    Evain, Michel
    Leinekugel-Le-Cocq-Errien, Aude Ysoline
    Jobic, Stephane
    Caurant, Daniel
    Petricek, Vaclav
    Advocat, Thierry
    ZEITSCHRIFT FUR KRISTALLOGRAPHIE, 2007, 222 (08): : 383 - 390
  • [39] Electrical conductivity and thermal stability of (1-x)CsH2PO4/xSiPyOz (x=0.2-0.7) composites
    Ponomareva, V. G.
    Shutova, E. S.
    Lavrova, G. V.
    INORGANIC MATERIALS, 2008, 44 (09) : 1009 - 1014
  • [40] Phase Formation, Microstructure, Magnetic and Electrical Properties of (1-x)Mg0.7Zn0.3Fe2O4-xBa0.7Sr0.3TiO3 Ceramics Composite
    Rittidech, Aurawan
    Sutthapintu, Aekkasit
    FERROELECTRICS, 2014, 458 (01) : 227 - 233