Study of microstructure and mechanical properties of aluminum 7075 alloy extruded in a semi-solid state

被引:0
|
作者
Hajihassani, Kamran [1 ]
Pouyafar, Vahid [1 ]
Sadough, Seyed Ali [2 ]
机构
[1] Univ Tabriz, Dept Mech Engn, Tabriz 5166616471, Iran
[2] Amirkabir Univ Technol, Tehran Polytech, Dept Mech Engn, Tehran 15914, Iran
来源
MATERIALS RESEARCH EXPRESS | 2019年 / 6卷 / 11期
关键词
Semi-solid process; 7075 aluminum alloy; forward extrusion; AZ91D ALLOY; EVOLUTION;
D O I
10.1088/2053-1591/ab4c5b
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, the effect of strain-induced melt activation process parameters and the effect of forward extrusion parameters on the semi-solid state in the microstructures and the mechanical properties of aluminum 7075 alloy are investigated. The isothermal holding time, isothermal temperature, and predeformation ratio-which are parameters of strain-induced melt activation method-have been selected at 5-20 min, 590-620 degrees C and 10%-40% respectively. Also, the extrusion ratio is 68%-89% and the extrusion speed is 0.05-0.5 m/s; the parameters are driven from forward extrusion. Samples at an extrusion ratio of 68%, 75%, and 82% were extruded defectively. Sound products were obtained at an extrusion ratio of 89%. So among these stated parameters, it was derived that the extrusion ratio has the greatest effect on obtaining sound products. At predeformation ratios higher than 30%, the shape factor decreased, and the grain size increased, it was clear that a predeformation ratio higher than 30% is inefficient for the process. The yield and ultimate stress for thixo-extruded samples were higher than for hot extruded samples. As expected, most of the mechanical properties in between sound samples (yield stress of 327 MPa, ultimate stress of 459.5 MPa, and elongation 14%) were related to the sample of finest-grained microstructures. The finest-grained sample (25.85 mu m) was achieved at isothermal holding time, isothermal temperature, predeformation ratio, and extrusion rate equal to, 20 min, 590 degrees C, 30%, 0.2 m/s respectively.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Microstructure evolution and thixoforming behavior of 7075 aluminum alloy in the semi-solid state prepared by RAP method
    Jin-long Fu
    Kai-kun Wang
    Xiao-wei Li
    Hai-kuan Zhang
    [J]. International Journal of Minerals, Metallurgy, and Materials, 2016, 23 : 1404 - 1415
  • [22] The Preparation and Microstructure of Semi-Solid 7075 Alloy Slurry
    Gan, G-S.
    Yang, B.
    Bei, S. -Y.
    Mei, H.
    [J]. ACTA PHYSICA POLONICA A, 2012, 122 (03) : 565 - 568
  • [23] Influencing factors of the coarsening behaviors for 7075 aluminum alloy in the semi-solid state
    Fu, Jinlong
    Wang, Shuxian
    Wang, Kaikun
    [J]. JOURNAL OF MATERIALS SCIENCE, 2018, 53 (13) : 9790 - 9805
  • [24] Influencing factors of the coarsening behaviors for 7075 aluminum alloy in the semi-solid state
    Jinlong Fu
    Shuxian Wang
    Kaikun Wang
    [J]. Journal of Materials Science, 2018, 53 : 9790 - 9805
  • [25] Investigation of microstructure and mechanical properties of semi-solid state joining of SSM aluminum alloys
    Petkhwan, Apirit
    Muangjunburee, Prapas
    Wannasin, Jessada
    [J]. FRONTIERS OF MANUFACTURING AND DESIGN SCIENCE IV, PTS 1-5, 2014, 496-500 : 371 - 375
  • [26] Recrystallisation in the Semi-Solid State in 7075 Aluminium Alloy
    H. V. Atkinson
    K. Burke
    G. Vaneetveld
    [J]. International Journal of Material Forming, 2008, 1 : 973 - 976
  • [27] Recrystallisation in the semi-solid state in 7075 aluminium alloy
    Atkinson, H. V.
    Burke, K.
    Vaneetveld, G.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 490 (1-2): : 266 - 276
  • [28] Recrystallisation in the Semi-Solid State in 7075 Aluminium Alloy
    Atkinson, H. V.
    Burke, K.
    Vaneetveld, G.
    [J]. INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2008, 1 (Suppl 1) : 973 - 976
  • [29] Microstructure and rheology of an AA2024 aluminium alloy in the semi-solid state, and mechanical properties of a back-extruded part
    de Freitas, ER
    Ferracini, E
    Ferrante, A
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2004, 146 (02) : 241 - 249
  • [30] Compressive mechanical properties of aluminum alloy in the semi-solid state at dynamic strain rate
    Nakano, S
    Mukai, T
    Higashi, K
    [J]. PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 2599 - 2602