Tribology characteristics of in-situ laser deposition of Fe-TiC

被引:49
|
作者
Emamian, Ali [1 ]
Corbin, Stephen F. [2 ]
Khajepour, Amir [1 ]
机构
[1] Univ Waterloo, Dept Mech & Mechatron Engn, Waterloo, ON N2L 3G1, Canada
[2] Dalhousie Univ, Univ Waterloo, Dept PEAS Adjunct Prof, Mat Engn Dept,Civil & Resource Engn Cross Appoint, Halifax, NS, Canada
来源
SURFACE & COATINGS TECHNOLOGY | 2012年 / 206卷 / 22期
基金
加拿大自然科学与工程研究理事会;
关键词
In-situ laser cladding; Abrasive wear resistance; Fe-TiC; COMPOSITE COATINGS; WEAR-RESISTANCE; ABRASIVE WEAR; PARTICLE COMPOSITES; MATRIX COMPOSITES; MICROSTRUCTURE; SIZE; PERFORMANCE; MECHANICS; ALLOYS;
D O I
10.1016/j.surfcoat.2012.01.051
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, the effects of TIC morphology and TiC volume fraction on wear resistance of the laser deposited Fe-TIC were studied. In-situ Fe-TIC clad layers were deposited on an AISI 1030 steel substrate with a fiber laser using dynamic blow technique. Two laser conditions along with two atomic percent ratios, 45:55 and 55: 45, were selected for C:Ti, and Fe percentages were explored with 70, 60,50 and 10 wt.%. Results showed that TIC morphology was affected by laser process parameters and powder composition. Optimum wear resistance was found among the samples by conducting wear tests with the ASTM G65-04, dry sand/rubber wheel, low-stress, coarse and abrasive (three-body) test methods. The abrasive characteristics of TiC were compared to WC-12wt.% Ni deposited on a similar substrate measured under identical test conditions. Results showed excellent wear resistance of in-situ TiC. The clad layer's abrasive wear resistance was a factor of 50-70 and 1.2 times higher than that of AISI 1030 steel and WC-12% Ni, respectively. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:4495 / 4501
页数:7
相关论文
共 50 条
  • [21] Microstructure and wear properties of Fe-TiC surface composite coating by laser cladding
    Qu, Shiyao
    Wang, Xinhong
    Zhang, Min
    Zou, Zengda
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (05) : 1546 - 1551
  • [22] Rapidly solidified Fe-TiC composites: Thermodynamics and the peculiarities of microstructure formation in situ
    Popov, AA
    Gasik, MM
    SCRIPTA MATERIALIA, 1996, 35 (05) : 629 - 634
  • [23] In situ production of Fe-VC and Fe-TiC surface composites by cast-sintering
    Wang, YS
    Zhang, XY
    Zeng, GT
    Li, FC
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2001, 32 (02) : 281 - 286
  • [24] Correlation between temperature distribution and in situ formed microstructure of Fe-TiC deposited on carbon steel using laser cladding
    Emamian, Ali
    Alimardani, Masoud
    Khajepour, Amir
    APPLIED SURFACE SCIENCE, 2012, 258 (22) : 9025 - 9031
  • [25] Synthesis of Fe-TiC Hard Coating From Ilmenite Via Laser Cladding
    Khalili, A.
    Mojtahedi, M.
    Goodarzi, M.
    Torkamany, M. J.
    IRANIAN JOURNAL OF MATERIALS SCIENCE AND ENGINEERING, 2019, 16 (03) : 75 - 86
  • [26] LASER SURFACE-TREATMENT OF PSEUDO-BINARY FE-TIC ALLOYS
    GILBERT, D
    STRUTT, PR
    NOWOTNY, H
    JOURNAL OF METALS, 1979, 31 (08): : F63 - F63
  • [27] Study on microstructure and wear-resistance of in situ synthesized Fe-TiC surface composites
    Cheng Fengjun
    Wang Yisan
    Zhang Xinyuan
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 : 470 - 474
  • [28] Evaluation of Centrifugal Casting Process Parameters for In Situ Fabricated Functionally Gradient Fe-TiC Composite
    Rahimipour, Mohammad Reza
    Sobhani, Manoochehr
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2013, 44 (05): : 1120 - 1123
  • [29] In-situ synthesis and characteristics of TiC−Fe cermet graded composite coating on a steel substrate
    Yan You-wei
    Fu Zheng-yi
    Yuan Run-zhang
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2003, 18 (4): : 14 - 17
  • [30] Evaluation of Centrifugal Casting Process Parameters for In Situ Fabricated Functionally Gradient Fe-TiC Composite
    Mohammad Reza Rahimipour
    Manoochehr Sobhani
    Metallurgical and Materials Transactions B, 2013, 44 : 1120 - 1123