Marginal Integrity of Turkom-Cera Compared to Other All-Ceramic Materials: Effect of Finish Line
被引:0
|作者:
AL-Makramani, Bandar M. A.
[1
,2
]
Razak, Abdul A. A.
[3
]
Abu-Hassan, Mohamed I.
[4
]
Sulaiman, Eshamsul
[1
]
Loon, Lui Joo
[1
]
Yahya, Noor Azlin
[1
]
机构:
[1] Univ Malaya, Dept Conservat Dent, Fac Dent, Kuala Lumpur, Malaysia
[2] Sanaa Univ, Dept Restorat Dent, Fac Dent, Sanaa, Yemen
[3] Univ Malaya, Fac Dent, Biomat & Dent Technol Unit, Kuala Lumpur, Malaysia
[4] Univ Teknol MARA, Fac Dent, Shah Alam, Malaysia
关键词:
FIT;
CROWNS;
D O I:
暂无
中图分类号:
R78 [口腔科学];
学科分类号:
1003 ;
摘要:
The aim of this study was to evaluate the marginal adaptation of Turkom-Cera all-ceramic crowns compared to In-Ceram and Procera AllCeram systems. The influence of finish line design (chamfer or shoulder) on the marginal adaptation of Turkom-Cera all-ceramic crowns was also investigated. Thirty human premolars were prepared with chamfer margins and assigned to either the Turkom-Cera, In-Ceram, or Procera system group. In addition, 10 premolars were prepared with rounded shoulder finish lines and assigned to an additional Turkom-Cera group. Ceramic copings (0.6-mm thick) were fabricated for each group following the manufacturers' instructions. The copings were seated on abutments using a special holding device that facilitated uniform loading, and marginal adaptation was assessed using a stereomicroscope. Data were analyzed using analysis of variance, the Tukey HSD post hoc test, and an independent samples t test. There was a statistically significant difference regarding marginal adaptation among the three all-ceramic systems (P < .05). There were no significant differences in the mean marginal discrepancies of Turkom-Cera crowns among chamfer and shoulder finish line groups (P > .05). Within the limitations of this study, the marginal discrepancies were all within the clinically acceptable standard. Int J Prosthodont 2011;24:379-381.
引用
收藏
页码:379 / 381