Measurement of the maximum charge and discharge powers of a nickel metal hydride battery for hybrid electric vehicles

被引:14
|
作者
Yang, YF [1 ]
机构
[1] Toyota Motor Corp, Mat Engn Div 1, Toyota, Aichi 4718572, Japan
关键词
nickel oxide electrode; metal hydride electrode; battery; charge and discharge; hybrid electric vehicle;
D O I
10.1016/S0378-7753(98)00078-0
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The determination of the maximum acceptable charge power and power output is of special significance in the development of hybrid electric vehicles. Theoretically, the maximum acceptable charge power and the power output can be defined as those relating to the maximum current levels before the occurrence of any side reaction. A new method has been developed to measure these maximum currents for nickel/metal hydride batteries used in hybrid electric vehicles. The method involves three step: (i) measurement of the transient voltage vs. current relation during charge or discharge by a sequence of pulse currents; (ii) calculation of the overall battery internal impedance at different times and current magnitudes; (iii) determination of the maximum current from the minimum point of the internal impedance. This method is based on the principle that, with increasing current level, mass transport becomes the rate-limiting step. Any extra increase in current can only cause the occurrence of a side reaction which will result in an increase in the battery internal impedance. The maximum current can thus be determined by the minimum internal impedance from a plot of this parameter against current. Experimental results show that the maximum current strongly depends on battery state-of-charge and also, battery structure. Increase in the surface area of the battery plates is an efficient way to increase the charge-acceptance and power output of the battery, and also to reduce the internal impedance. (C) 1998 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:19 / 27
页数:9
相关论文
共 50 条
  • [41] Intelligent control technology of charge and discharge for Ni-MH battery of electric vehicles
    Xie, Qinghua
    Lu, Yong
    Zhang, Qi
    Jixie Gongcheng Xuebao/Chinese Journal of Mechanical Engineering, 2008, 44 (08): : 185 - 189
  • [42] DESCRIPTION OF HYSTERESIS OF NICKEL METAL HYDRIDE BATTERY
    Trapanese, Marco
    Franzitta, Vincenzo
    Viola, Alessia
    38TH ANNUAL CONFERENCE ON IEEE INDUSTRIAL ELECTRONICS SOCIETY (IECON 2012), 2012, : 967 - 970
  • [44] THE NICKEL-ZINC BATTERY FOR ELECTRIC VEHICLES
    REASBECK, P
    PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1981, 302 (1468): : 351 - 360
  • [45] Battery and battery management for hybrid electric vehicles: a review
    Conte, F. V.
    ELEKTROTECHNIK UND INFORMATIONSTECHNIK, 2006, 123 (10): : 424 - 431
  • [46] Environmental optimization of the charge of battery electric vehicles
    Zacharopoulos, Leon
    Thonemann, Nils
    Dumeier, Marcel
    Geldermann, Jutta
    APPLIED ENERGY, 2023, 329
  • [47] REPURPOSING OF A HYBRID VEHICLE NICKEL METAL HYDRIDE BATTERY PACK FOR ELECTRICAL GRID STORAGE
    Balderston, Dayton
    Kelley, John Eric
    Crowder, James
    DeAgostino, Thomas
    Depcik, Christopher
    PROCEEDINGS OF THE ASME INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, 2017 VOL 6, 2018,
  • [48] Battery wiring module for electric and hybrid electric vehicles
    Shimoda, Hiroki
    Takahashi, Hideo
    Nakayama, Osamu
    Takase, Shinichi
    Tanaka, Tetsuji
    Uchita, Yoshifumi
    SEI Technical Review, 2019, (88): : 35 - 38
  • [49] Life Cycle Environmental Assessment of Lithium-Ion and Nickel Metal Hydride Batteries for Plug-In Hybrid and Battery Electric Vehicles (vol 45, pg 4548, 2011)
    Majeau-Bettez, Guillaume
    Hawkins, Troy R.
    Stromman, Anders Hammer
    ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2011, 45 (12) : 5454 - 5454
  • [50] Self-discharge mechanism of sealed-type nickel/metal-hydride battery
    Ikoma, M
    Hoshina, Y
    Matsumoto, I
    Iwakura, C
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (06) : 1904 - 1907