Interfacial reactions and mechanical properties of SiC fiber reinforced Ti3SiC2 and Ti3(SiAl)C2 composites

被引:17
|
作者
He, Guangqi [1 ,2 ]
Xu, Jingjun [2 ]
Zhang, Zerong [2 ]
Qian, Yuhai [2 ]
Zuo, Jun [2 ]
Li, Meishuan [2 ]
Liu, Changsheng [1 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110819, Peoples R China
[2] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2021年 / 827卷
基金
中国国家自然科学基金;
关键词
MAX phase; Composite; SiC fiber; Mechanical properties; PLASMA SINTERED TI3SIC2; CARBON-FIBER; MATRIX COMPOSITES; SILICON-CARBIDE; MICROSTRUCTURE; TEMPERATURE; FABRICATION; DENSIFICATION; SICF/TI3SIC2; CERAMICS;
D O I
10.1016/j.msea.2021.142069
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, SiC fiber (SiCf) reinforced Ti3SiC2 and Ti3(SiAl)C2 composites were fabricated by spark plasma sintering at 1250 degrees C and 1300 degrees C for 10 min, respectively. The interfacial reactions between fibers and matrix, as well as the mechanical properties of the two composites, were investigated. XRD, SEM and TEM were used to characterize the phase compositions and microstructures of the as-synthesized composites. The results showed that no interfacial reaction occurred between SiCf and Ti3SiC2 matrix, while it occurred between SiCf fiber and Ti3(SiAl)C2 matrix. In the latter case, the interfacial reaction layer was mainly composed of SiC, TiC, and TiSi2 phases, and its thickness was about 1.2 mu m. Besides, due to the introduction of SiC fibers, both bending strength and fracture toughness of two composites were improved. Based on the investigation of crack propagation, it was proposed that the main strengthening and toughening mechanism was crack bowing for SiCf/Ti3(SiAl)C2 composite, while was fiber pullout, fiber debonding, and residual thermal stress for SiCf/Ti3SiC2 composite.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Interfacial reactions and mechanical properties of SiC fiber reinforced Ti3SiC2 and Ti3(SiAl)C2 composites
    He, Guangqi
    Xu, Jingjun
    Zhang, Zerong
    Qian, Yuhai
    Zuo, Jun
    Li, Meishuan
    Liu, Changsheng
    Materials Science and Engineering: A, 2021, 827
  • [2] SPS preparation and mechanical properties of Ti3SiC2/SiC composites reinforced with quantitative SiC
    Du, Chengzhi
    Lei, Bo
    Qi, Yajie
    Zhang, Rui
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [3] SPS preparation and mechanical properties of Ti3SiC2/SiC composites reinforced with quantitative SiC
    Zhang, Rui (zhangrui0214@cdu.edu.cn), 1600, Elsevier Ltd (1010):
  • [4] Tribological properties of polycrystalline Ti3SiC2 and Al2O3-reinforced Ti3SiC2 composites
    Hu, Chunfeng
    Zhou, Yanchun
    Bao, Yiwang
    Wan, Detian
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (11) : 3456 - 3461
  • [5] Evaluation of properties of spark plasma sintered Ti3SiC2 and Ti3SiC2/SiC composites
    Islak, Bilge Yaman
    Ayas, Erhan
    CERAMICS INTERNATIONAL, 2019, 45 (09) : 12297 - 12306
  • [6] Microstructural and mechanical properties of Ti3SiC2 composites
    Huang, Jow-Lay
    Lu, Horng-Hwa
    Key Engineering Materials, 2009, 403 : 189 - 192
  • [7] Microstructural and Mechanical Properties of Ti3SiC2 Composites
    Huang, Jow-Lay
    Lu, Horng-Hwa
    SIAIONS AND NON-OXIDES, 2009, 403 : 189 - +
  • [8] Microstructure and Properties of Carbon Fiber Reinforced SiC Matrix Composites Containing Ti3SiC2
    Fan, Xiaomeng
    Yin, Xiaowei
    ADVANCED ENGINEERING MATERIALS, 2014, 16 (06) : 670 - 683
  • [9] Fabrication and Properties of Ti3SiC2/SiC Composites
    YIN Hongfeng
    China'sRefractories, 2008, (01) : 10 - 13
  • [10] Long time oxidation study of Ti3SiC2,Ti3SiC2/SiC, and Ti3SiC2/TiC composites in air
    Barsoum, MW
    Ho-Duc, LH
    Radovic, M
    El-Raghy, T
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (04) : B166 - B175