Effect of rheocast and thixocast characteristics of eutectic Lead-Tin alloy sheet on deep drawing

被引:1
|
作者
Kalaichelvan, K [1 ]
Sivaramakrishnan, R
Saravanakumar, VP
Stanley, AJ
Venkataswamy, S
机构
[1] Anna Univ, Dept Prod Technol, MIT, Madras 600044, Tamil Nadu, India
[2] Anna Univ, Dept Aeronaut Engn, MIT, Madras 600044, Tamil Nadu, India
关键词
rheocast; thixocast; Erichsen number;
D O I
10.1016/j.jmatprotec.2004.04.127
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Semisolid metal processing is a relatively new technology in metal forming. It is different from conventional metal forming technology, which use either solid metals or liquid metals as starting material. Semisolid metal processing deals with semisolid slurries in which non-dendritic solid particles are dispersed in a liquid matrix. This work involves the developing of an alloy sheet blank with a structure, which is non-dendritic, irregularly spherical solid solution by rheocasting and thixocasting techniques. This alloy sheet blank was used to form simple cup by deep drawing process. The formability of this alloy, reduction in applied load, strength of the alloy and the surface strain parameters were studied using Erichsen cupping test, tensile test and grid marking the blank surface. The above parameters were compared for each of these casting processes and the effective method of processing was identified. Thixocast components were found to have good qualities than the conventionally cast and rheocast components. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:637 / 642
页数:6
相关论文
共 50 条
  • [31] Lead-tin alloy coating-thickness monitoring
    Bliznikas, Z.A., 1600, (54):
  • [32] LEAD-TIN EMBRITTLEMENT OF LOW-ALLOY STEELS
    BALAGUER, JP
    DUQUETTE, DJ
    STOLOFF, NS
    SIKORA, RB
    MOTYL, MJ
    JOURNAL OF METALS, 1988, 40 (07): : A28 - A28
  • [33] DIFFUSION OF CD-IN ALLOY INTO LEAD-TIN TELLURIDE
    LANIR, M
    LEVINSTEIN, H
    INFRARED PHYSICS, 1978, 18 (04): : 259 - 266
  • [34] INTERDENDRITIC FLUID-FLOW IN A LEAD-TIN ALLOY
    STREAT, N
    WEINBERG, F
    METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1976, 7 (03): : 417 - 423
  • [35] Gravitational macrosegregation in unidirectionally solidified lead-tin alloy
    Wang, L.
    Laxmanan, V.
    Wallace, J.F.
    Metallurgical transactions. A, Physical metallurgy and materials science, 1988, 19 A (11): : 2687 - 2694
  • [36] GRAVITATIONAL MACROSEGREGATION IN UNIDIRECTIONALLY SOLIDIFIED LEAD-TIN ALLOY
    WANG, L
    LAXMANAN, V
    WALLACE, JF
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (11): : 2687 - 2694
  • [37] LEAD-TIN ALLOY COATING-THICKNESS MONITORING
    BLIZNIKAS, ZA
    SKOMINAS, VJ
    INDUSTRIAL LABORATORY, 1988, 54 (07): : 751 - 753
  • [38] EFFECT OF FREQUENCY ON THE CYCLIC CREEP AND FRACTURE OF A LEAD-RICH LEAD-TIN SOLDER ALLOY
    WEINBEL, RC
    SCHWARZKOPF, EA
    TIEN, JK
    SCRIPTA METALLURGICA, 1987, 21 (09): : 1165 - 1168
  • [39] Effect of temperature and drawing speed on warm deep drawing characteristics of AZ31 magnesium alloy sheet
    Department of Mechanical Engineering, Tokyo Metropolitan University, 1-1 Minamiosawa, Hachioji-shi, Tokyo 192-0397
    不详
    Keikinzoku J Jpn Inst Light Met, 2006, 10 (521-526):
  • [40] DEEP ENERGY-LEVELS IN LEAD-TIN TELLURIDE
    CHASHCHIN, SP
    GUZHOVA, IP
    BARYSHEV, NS
    KHARIONOVSKII, YS
    EZHOVA, LN
    ANDRAMONOV, VS
    SOVIET PHYSICS SEMICONDUCTORS-USSR, 1977, 11 (05): : 579 - 579