Excellent degradation performance of the Fe78Si11B9P2 metallic glass in azo dye treatment

被引:23
|
作者
Ji, L. [1 ]
Chen, J. W. [1 ]
Zheng, Z. G. [1 ]
Qiu, Z. G. [1 ,3 ]
Peng, S. Y. [2 ]
Zhou, S. H. [1 ,3 ]
Zeng, D. C. [1 ,3 ]
机构
[1] South China Univ Technol, Sch Mat Sci & Engn, Guangzhou 510640, Peoples R China
[2] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Metall M, Guangzhou 510640, Peoples R China
[3] South China Univ Technol, Zhongshan R&D Ctr Mat Surface & Thin Films Techno, Gent Mat Surface Technol Guangzhou Co Ltd, Zhongshan 528437, Peoples R China
基金
中国国家自然科学基金;
关键词
Fe78Si11B9P2 metallic glass; Degradation; Reusability; High COD removal; Wastewater treatment; ZERO-VALENT IRON; FENTON-LIKE CATALYST; WASTE-WATER; REDUCTIVE DEGRADATION; METHYLENE-BLUE; OXIDATION; DECOLORIZATION; EFFICIENT; NANOPARTICLES; MECHANISM;
D O I
10.1016/j.jpcs.2020.109546
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Fe78Si11B9P2 metallic glass (MG) ribbons are proved to exhibit excellent comprehensive ability in azo dye treatment. The Fe(78)Si(11)B(9)P(2 )MG ribbons can degrade the azo dye effectively, which derived from high mass and electron transfer ability due to the cotton-like structure formed during the reaction. The degradation efficiency and reaction rate raise with the decrease of the initial Orange II concentration, the increase of ribbon dosage and the proper addition of H2O2. The Fe78Si11B9P2 MG ribbons are more applicable in acidic and neutral solutions. Compared to the other reported Fe-based metallic glasses for dye degradation, the Fe78Si11B9P2 MG has a lower reaction activation energy and relatively good reusability in treating with azo dye. In addition, the achieved high COD removal indicates that the complex organic structures in azo dye can be decomposed completely by Fe78Si11B9P2 MG ribbons. This work not only provides a new effective and low-cost materials for wastewater treatment, but also promotes the practical applications of Fe-based MGs as functional materials.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] EFFECT OF HYDRIDING ON THE ELECTRON-STRUCTURE OF THE METALLIC GLASSES FE78SI9B13 AND CO78SI9B13
    KOLODZIEJ, HB
    JAKUBCZYK, E
    JAKUBCZYK, M
    TODOROW, B
    CALUSINSKI, B
    MATERIALS CHARACTERIZATION, 1990, 24 (02) : 191 - 198
  • [42] The magnetic structure of Fe78Si9B13 commercial metallic glasses
    Wildes, AR
    Cowlam, N
    Pankhurst, QA
    Al-Heniti, S
    Gibbs, MRJ
    EUROPHYSICS LETTERS, 2004, 68 (04): : 582 - 588
  • [43] DEBYE TEMPERATURE-CHANGE INDUCED BY STRUCTURAL RELAXATION IN FE78B13SI9 METALLIC-GLASS
    PARTITI, CSM
    RECHENBERG, HR
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1994, 145 (01): : K17 - K20
  • [44] Mossbauer spectroscopic study of the effect of annealing on the hyperfine field distributions in Fe78B13Si9 metallic glass
    Bandyopadhyay, D
    SOLID STATE COMMUNICATIONS, 1999, 109 (09) : 611 - 614
  • [45] INVESTIGATION OF THE EFFECT OF CRYSTALLIZATION AND HYDRIDING OF THE FE78SI9B13 METALLIC-GLASS ON ELECTRON-STRUCTURE
    KOLODZIEJ, HB
    CALUSINSKI, B
    JAKUBCZYK, E
    JAKUBCZYK, M
    ACTA PHYSICA POLONICA A, 1988, 74 (01) : 29 - 35
  • [46] Mossbauer spectrometry analysis of Fe78Si9B13 metallic glass prepared with different quenching wheel speed
    Amini, Narges
    Habibi, Safdar
    Dekan, Julius
    Pavuk, Milan
    Novak, Patrik
    Miglierini, Marcel
    JOURNAL OF RADIOANALYTICAL AND NUCLEAR CHEMISTRY, 2017, 314 (03) : 2099 - 2111
  • [47] Features of nanocrystallization of metallic glass Fe78B13Si9 induced by high-current-density electropulsing
    Teng, Gongqing
    Chao, Yuesheng
    Dong, Lin
    Geng, Yan
    Lai, Zuhan
    1996, JJAP, Minato-ku, Japan (35):
  • [48] Features of nanocrystallization of metallic glass Fe78B13Si9 induced by high-current-density electropulsing
    Teng, GQ
    Chao, YS
    Dong, L
    Geng, Y
    Lai, ZH
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 1996, 35 (10): : 5320 - 5325
  • [49] Dynamic fracture behaviour of Fe78Si9B13 metallic glass ribbon under laser shock loading
    Zheng, C.
    Sun, S.
    Ji, Z.
    Song, L.
    Zhang, G.
    Zhang, J.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2014, 37 (05) : 508 - 516
  • [50] Electro-fenton degradation of simulated petroleum wastewater by using Fe78Si9B13 metallic glasses
    Xu, Xiao-Chen
    Shi, Zhong-Ling
    Qiu, Ke-Qiang
    MATERIALS RESEARCH EXPRESS, 2020, 7 (04)