Wear Behaviour of Al-1050 Alloy Processed by Severe Plastic Deformation

被引:18
|
作者
Wang, Chuan Ting [1 ]
Gao, Nong [1 ]
Wood, Robert J. K. [2 ]
Langdon, Terence G. [1 ,3 ,4 ]
机构
[1] Univ Southampton, Sch Engn Sci, Mat Res Grp, Southampton SO17 1BJ, Hants, England
[2] Univ Southampton, Sch Engn Sci, Natl Ctr Adv Tribol, Southampton SO17 1BJ, Hants, England
[3] Univ So Calif, Dept Aerosp & Mech Engn, Los Angeles, CA 90089 USA
[4] Univ So Calif, Dept Mat Sci, Los Angeles, CA 90089 USA
基金
英国工程与自然科学研究理事会;
关键词
Al-1050; ECAP; HPT; wear; wear map; work hardening capacity; HIGH-PRESSURE TORSION;
D O I
10.4028/www.scientific.net/MSF.667-669.1101
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
An Al-1050 alloy was processed by ECAP and HPT, respectively. Dry sliding wear tests were conducted on the as-received and SPD-processed samples under various sliding conditions. A comparison of wear rate indicated that SPD processing decreased the wear resistance. Two main wear mechanisms were observed. The initial wear stage was dominated by severe platelet wear mechanism and later wear was dominated by an oxidation wear mechanism. The results show the severe wear stage of SPD-processed Al-1050 is much longer than that of the as-received Al-1050, which is attributed to the loss of work hardening capacity after SPD processing.
引用
收藏
页码:1101 / +
页数:2
相关论文
共 50 条
  • [21] Influence of heat treatment on corrosion resistance of Mg-Al-Zn alloy processed by severe plastic deformation
    Zemkova, Maria
    Kral, Robert
    Cizek, Jakub
    Smilauerova, Jana
    Minarik, Peter
    OPEN ENGINEERING, 2018, 8 (01): : 391 - 394
  • [22] Effect of severe plastic deformation on creep behaviour of a Ti-6Al-4V alloy
    Kral, Petr
    Dvorak, Jiri
    Zherebtsov, Sergey
    Salishchev, Gennady
    Kvapilova, Marie
    Sklenicka, Vaclav
    JOURNAL OF MATERIALS SCIENCE, 2013, 48 (13) : 4789 - 4795
  • [23] Microstructure and dislocation density evolutions in MgAlZn alloy processed by severe plastic deformation
    Miloš Janeček
    Jakub Čížek
    Jenő Gubicza
    Jitka Vrátná
    Journal of Materials Science, 2012, 47 : 7860 - 7869
  • [24] Characterization of ultrafine and nano grained magnesium alloy processed by severe plastic deformation
    Fatemi-Varzaneh, S. M.
    Zarei-Hanzaki, A.
    Paul, H.
    MATERIALS CHARACTERIZATION, 2014, 87 : 27 - 35
  • [25] COMMERCIALLY Ti GRADE 2 ALLOY PROCESSED BY SPD (SEVERE PLASTIC DEFORMATION)
    Cinca, Ion
    Petrescu, Mircea Ionut
    METALURGIA INTERNATIONAL, 2013, 18 (04): : 83 - 86
  • [26] Microstructure and dislocation density evolutions in MgAlZn alloy processed by severe plastic deformation
    Janecek, Milos
    Cizek, Jakub
    Gubicza, Jeno
    Vratna, Jitka
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (22) : 7860 - 7869
  • [27] Pitting corrosion resistance of anodized aluminum alloy processed by severe plastic deformation
    Son, In-Joon
    Nakano, Hiroaki
    Oue, Satoshi
    Kobayashi, Shigeo
    Fukushima, Hisaaki
    Horita, Zenji
    MATERIALS TRANSACTIONS, 2007, 48 (01) : 21 - 28
  • [28] Pitting corrosion resistance of anodized aluminum alloy processed by severe plastic deformation
    Son, In-Joon
    Nakano, Hiroaki
    Oue, Satoshi
    Kobayashi, Shigeo
    Fukushima, Hisaaki
    Horita, Zenji
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2006, 70 (07) : 534 - 540
  • [29] Superplasticity of AZ31 magnesium alloy processed by severe plastic deformation
    Xing, Jie
    Yang, Xuyue
    Miura, Hiromi
    Sakai, Taku
    Keikinzoku/Journal of Japan Institute of Light Metals, 2006, 56 (12): : 716 - 720
  • [30] Pitting corrosion resistance of anodized aluminum alloy processed by severe plastic deformation
    Department of Materials Process Engineering, Kyushu University, Fukuoka 819-0395
    不详
    不详
    不详
    Nippon Kinzoku Gakkaishi, 7 (534-540):