摘要
Approximately 500 in of abovegrade 4.5-in. (11.4-cm) outside diameter, welded, type 304 austenitic stainless steel (UNS S30400) water pipeline in a food processing factory experienced severe localized corrosion after 3 months of service. Visual examination showed that corrosion and pitting were evident in the circumferential welds and parent metal of the pipe. An investigation revealed that chloride pitting initiated the attack and sulfate-reducing bacteria and warm temperature (>35degreesC) exacerbated the corrosion process. This article describes the investigation and recommended remedial action.
引用
收藏
页码:54 / 57
页数:4
相关论文
共 50 条
  • [41] Influence of Warm Predeformation Temperature on the Corrosion Property of Type 304 Austenitic Stainless Steel
    Tao, Huimin
    Zhou, Chengshuang
    Hong, Yuanjian
    Zheng, Yuanyuan
    Zhang, Kaiyu
    Zheng, Jinyang
    Zhang, Lin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (07) : 4515 - 4528
  • [42] Influence of Warm Predeformation Temperature on the Corrosion Property of Type 304 Austenitic Stainless Steel
    Huimin Tao
    Chengshuang Zhou
    Yuanjian Hong
    Yuanyuan Zheng
    Kaiyu Zhang
    Jinyang Zheng
    Lin Zhang
    Journal of Materials Engineering and Performance, 2020, 29 : 4515 - 4528
  • [43] Influence of the individual microstructural features on pitting corrosion in type 304 austenitic stainless steel
    Pradhan, S. K.
    Bhuyan, P.
    Mandal, S.
    CORROSION SCIENCE, 2019, 158
  • [44] Corrosion behaviour of borided AISI 304 austenitic stainless steel
    Gunen, Ali
    Karakas, Mustafa Serdar
    Kurt, Bulent
    Calik, Adnan
    ANTI-CORROSION METHODS AND MATERIALS, 2014, 61 (02) : 112 - 118
  • [45] DEFORMATION IN TYPE 304 AUSTENITIC STAINLESS STEEL.
    Anon
    1600,
  • [46] Electrochemical Analysis of the Microbiologically Influenced Corrosion of AISI 304 Stainless Steel by Sulphate Reducing Bacteria Associated with Bacillus Cereus
    Santana, J. J.
    Santana, F. J.
    Gonzalez, J. E.
    Souto, R. M.
    Gonzalez, S.
    Morales, J.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (01): : 711 - 724
  • [47] Salvia officinalis extract mitigates the microbiologically influenced corrosion of 304L stainless steel by Pseudomonas aeruginosa biofilm
    Lekbach, Yassir
    Li, Zhong
    Xu, Dake
    El Abed, Soumya
    Dong, Yucliao
    Liu, Dan
    Gu, Tingyue
    Koraichi, Saad Ibnsouda
    Yang, Ke
    Wang, Fuhui
    BIOELECTROCHEMISTRY, 2019, 128 : 193 - 203
  • [48] Inhibition of Microbiologically Influenced Corrosion of Mild Steel and Stainless Steel 316 by an organic inhibitor
    Sheng, Xiaoxia
    Ting, Yen-Peng
    Pehkonen, Simo Olavi
    BIOHYDROMETALLURY: FROM THE SINGLE CELL TO THE ENVIRONMENT, 2007, 20-21 : 379 - +
  • [49] Study of Microbiologically Influenced Corrosion of the Welded Stainless Steel 316L
    Ahmad Nejad Ababaf
    Esmaeil Jafari
    Journal of Materials Engineering and Performance, 2023, 32 : 8162 - 8173
  • [50] Microbially Induced Pitting Corrosion on an Austenitic Stainless Steel Pipe
    Strobl, S.
    Linhardt, P.
    Haubner, R.
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2019, 56 (10): : 669 - 679