Surface Integrity Characteristics in Wire Electrical Discharge Machining of Titanium Alloy during Main cut and Trim cuts

被引:0
|
作者
Arikatla, Siva Prasad [1 ,2 ]
Mannan, K. Tamil [3 ]
Krishnaiah, Arkanti [4 ]
机构
[1] IGNOU, SOET, New Delhi 523001, India
[2] DA Govt Polytechn, Ongole 523001, Andhra Pradesh, India
[3] IGNOU, Sch Engn & Technol, Dept Mech Engn, New Delhi 110028, India
[4] Osmania Univ, Coll Engn, Dept Mech Engn, Hyderabad, Telangana, India
关键词
Wire Electrical Discharge Machining (WEDM); Surface Integrity; Titanium alloy; Trim cut; Scanning Electron Microscopy (SEM); EVOLUTION; EDM;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ti-6Al-4V grade titanium alloy is the most popular alloy and is used for a wide range of applications in aerospace, marine, power generation and offshore industries etc., because of its very good mechanical properties such as high tensile strength, fatigue resistance, highest strength-to-weight ratio, extraordinary corrosion resistance and toughness even at elevated temperatures. Wire Electrical Discharge Machining (WEDM) is extensively used for machining of complex shapes in the field of die and mould making, medical, aerospace and automobile industries for machining of too hard materials. WEDM is essentially a thermal process with a complex metal removal mechanism, involving the formation of a plasma channel between the wire/tool and workpiece, resulting in the material removal, which also leads to surface roughness, work hardness, over cut, white layer, heat effected zone, surface structural changes, metallurgical transformations and cracking. These properties determine the operational behaviour of the material and can be included in one term called surface integrity. In this Investigation multi cutting pass i.e. rough/main cut and trim/finish cut approach was adopted to improve the quality of surface characteristics of WEDM surface of Titanium alloy. The results show that the WEDMed surface topography shows dominant micro voids, thick white layer and heat affected zone and even micro cracks at high pulse on time and pulse current and these are low at low pulse on time and pulse current during trim cuts. Further surface topography and micro structural changes were observed through scanning electron microscopy (SEM) micrographs. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1500 / 1509
页数:10
相关论文
共 50 条
  • [21] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Jain, N.K. (nkjain@iiti.ac.in), 1735, Springer London (72): : 9 - 12
  • [22] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Kapil Gupta
    Neelesh Kumar Jain
    The International Journal of Advanced Manufacturing Technology, 2014, 72 : 1735 - 1745
  • [23] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Gupta, Kapil
    Jain, Neelesh Kumar
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2014, 72 (9-12): : 1735 - 1745
  • [24] Study of the Surface Integrity of AISI 4140 Steel in Wire Electrical Discharge Machining
    Hassan, M. A.
    Mehat, N. S.
    Sharif, S.
    Daud, R.
    Tomadi, S. H.
    Reza, M. S.
    IMECS 2009: INTERNATIONAL MULTI-CONFERENCE OF ENGINEERS AND COMPUTER SCIENTISTS, VOLS I AND II, 2009, : 1666 - +
  • [25] Surface Integrity Evolution of Zirconium-Based Metallic Glass Multi-Cut with Wire Electrical Discharge Machining
    Hou, Yonggang
    Xu, Jinkai
    Lian, Zhongxu
    Pei, Qiangqiang
    Yang, Shen
    Zhai, Changtai
    Yu, Huadong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (05) : 4158 - 4166
  • [26] Surface Integrity Evolution of Zirconium-Based Metallic Glass Multi-Cut with Wire Electrical Discharge Machining
    Yonggang Hou
    Jinkai Xu
    Zhongxu Lian
    Qiangqiang Pei
    Shen Yang
    Changtai Zhai
    Huadong Yu
    Journal of Materials Engineering and Performance, 2022, 31 : 4158 - 4166
  • [27] An Investigation to Achieve Good Surface Integrity in Wire Electrical Discharge Machining of Ti-6242 Super Alloy
    Ezeddini, Sonia
    Rajhi, Wajdi
    Boujelbene, Mohamed
    Bayraktar, Emin
    Ben Salem, Sahbi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (09) : 4523 - 4537
  • [28] Study of surface integrity and machining performance during main/rough cut and trim/finish cut mode of WEDM on Ti-6Al-4V: effects of wire material
    Jadam, Thrinadh
    Datta, Saurav
    Masanta, Manoj
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2019, 41 (03)
  • [29] Wire electric discharge machining characteristics of titanium nickel shape memory alloy
    Manjaiah, M.
    Narendranath, S.
    Basavarajappa, S.
    Gaitonde, V. N.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (10) : 3201 - 3209
  • [30] The machining characteristics and surface integrity of Ni-rich NiTi shape memory alloy using wire electric discharge machining
    Bisaria, Himanshu
    Shandilya, Pragya
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2019, 233 (03) : 1068 - 1078