Corrosion of Fe-(8.5∼36.9) wt% Cr Alloys at 600∼800°C in (N2, H2S, H2O)-Mixed Gases

被引:4
|
作者
Kim, Min Jung [1 ]
Lee, Dong Bok [1 ]
机构
[1] Sungkyunkwan Univ, Sch Adv Mat Sci & Engn, Suwon 440746, Gyeonggi, South Korea
来源
关键词
alloys; casting; corrosion; scanning electron microscopy (SEM); H2S gas; HIGH-TEMPERATURES; AL ALLOYS; SULFIDATION; STEELS; BEHAVIOR; KINETICS; METALS; SCALES; SULFUR; IRON;
D O I
10.3365/KJMM.2012.50.3.218
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fe-(8.5, 18.5, 28.3, 36.9) wt% Cr alloys were corroded between 600 and soot for up to 70 h in a 1 atm gas mixture that consisted of 0.0242 atm of H2S, 0.031 atm of water vapor, and 0.9448 atm of nitrogen gas. Their corrosion resistance increased with an increment in the Cr content. The Fe-8.5%Cr alloy corroded fast, forming thick, fragile, nonadherent scales that consisted primarily of an outer FeS layer and an inner (Fe, Cr, 0, S)-mixed layer. The outer FeS layer grew into the air by the outward diffusion of Fe2+ ions, whereas the inner mixed layer grew by the inward diffusion of oxygen and sulfur ions. At the interface of the outer and inner scales, voids developed and cracking occurred. The Fe-(18.5, 28.3, 36.9)% Cr alloys displayed much better corrosion resistance than the Fe-8.5Cr alloy, because thin Cr2O3 or Cr2S3 scales formed.
引用
收藏
页码:218 / 223
页数:6
相关论文
共 50 条
  • [31] The Corrosion of Cu–Al Binary Alloys in H2/H2S/H2O Atmospheres at 400–900°C
    W. Kai
    G. W. Fan
    P. C. Chen
    Y. T. Lin
    Oxidation of Metals, 2004, 61 : 439 - 461
  • [32] High temperature corrosion behavior of iron aluminides containing ternary additions in H2/H2S/H2O mixed gases
    Kai, W
    Chu, JP
    Huang, RT
    Lee, PY
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 240 : 859 - 870
  • [33] THE HIGH-TEMPERATURE CORROSION BEHAVIOR OF FE-MO-AL ALLOYS IN H2/H2O/H2S MIXED-GAS ENVIRONMENTS
    KAI, W
    DOUGLASS, DL
    OXIDATION OF METALS, 1993, 39 (3-4): : 281 - 316
  • [34] Corrosion of Multilayered TiAlSiN Films at 800-1000 °C in N2/0.1%H2S Gas
    Hahn, Junhee
    Abro, Muhammad Ali
    Xiao, Xiao
    Lee, Dong Bok
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (09) : 3260 - 3268
  • [35] A new force field for the adsorption of H2, O2, N2, CO, H2O, and H2S gases on alkali doped carbon nanotubes
    Bamdad, Mahdiyeh
    Farrokhpour, Hossein
    Ashrafizaadeh, Mahmud
    Najafi, Bijan
    MOLECULAR PHYSICS, 2016, 114 (22) : 3375 - 3387
  • [36] THE HIGH-TEMPERATURE CORROSION OF FE-NB ALLOYS IN A H2/H2O/H2S GAS-MIXTURE
    KAI, W
    DOUGLASS, DL
    GESMUNDO, F
    OXIDATION OF METALS, 1992, 37 (3-4): : 189 - 215
  • [37] Bridging H2O and H2S homomeric clusters via H2O-H2S mixed clusters: Impact of the changing ratio of H2O and H2S moieties
    Monu
    Oram, Binod Kumar
    Bandyopadhyay, Biman
    COMPUTATIONAL AND THEORETICAL CHEMISTRY, 2022, 1213
  • [38] The corrosion of Cu-Al binary alloys in H2/H2S/H2O atmospheres at 400-900°C
    Kai, W
    Fan, GW
    Chen, PC
    Lin, YT
    OXIDATION OF METALS, 2004, 61 (5-6): : 439 - 461
  • [39] The corrosion of Fe-18Al and Fe-18Al-2Nb in H-2/H2S/H2O mixed-gas environments
    Kai, W
    Huang, RT
    Chu, JP
    Lee, PY
    FUNDAMENTAL ASPECTS OF HIGH TEMPERATURE CORROSION, 1997, 96 (26): : 332 - 343
  • [40] EARLY STAGES OF OXIDATION OF FE-25CR AND FE-25CR-6AL ALLOYS IN H2/H2O/H2S ATMOSPHERES AT 700-DEGREES-C
    VEDULA, K
    BOULOGNE, B
    HUGHES, P
    CHANG, S
    MICHAL, GM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1989, 120 : 259 - 266