Mechanical properties of in situ demineralised human enamel measured by AFM nanoindentation

被引:61
|
作者
Finke, M
Hughes, JA
Parker, DM
Jandt, KD
机构
[1] Univ Bristol, Dept Oral & Dent Sci, Bristol BS1 2LY, Avon, England
[2] Univ Bristol, Biomed Engn & Biomat Sci Sect, Bristol BS1 2LY, Avon, England
[3] Glaxo SmithKline, Consumer Healthcare, Nutr Healthcare R&D, Royal Forest Factory, Coleford GL16 8JB, Glos, England
基金
英国生物技术与生命科学研究理事会;
关键词
atomic force microscopy; surface chemical reaction; surface roughening; surface structure; morphology; roughness; and; topography; polycrystalline surfaces; solid-liquid interfaces;
D O I
10.1016/S0039-6028(01)01311-5
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Diet-induced demineralisation is one of the key factors in surface changes of tooth enamel, with soft drinks being a significant etiological agent. The first step in this dissolution process is characterised by a change in the mechanical properties of the enamel and a roughening of the surface. The objective of this pilot study was to measure early stages of in situ induced hardness changes of polished human enamel surfaces with high accuracy using a nanoindenter attached to an atomic force microscope (AFM). Human unerupted third molars were cleaned. sterilised with sodium hypochlorite, sectioned and embedded in epoxy resin. The outer enamel surface was polished and the samples partly covered with a tape, allowing a 2-mm-wide zone to be exposed to the oral environment. Samples were fitted in an intra-oral appliance, which was worn from 9 a.m. to 5 p.m. for one day. During this time the volunteer sipped 250 ml of a drink over 10 min periods at 9.00, 11.00, 13.00 and 15.00 h. Three different drinks, mineral water, orange juice and the prototype of a blackcurrant drink with low demineralisation potential were used in this study. At the end of the experiment the samples were detached from the appliance, the tape removed and the surfaces chemically cleaned. The surface hardness and reduced Young's modulus of the exposed and unexposed areas of each sample were determined. In addition, high resolution topographical AFM images were obtained. This study shows that by determining the hardness and reduced Young's modulus, the difference in demineralisation caused by the drinks can be detected and quantified before statistically significant changes in surface topography could be observed with the AFM. The maximum decrease in surface hardness and Young's modulus occurred in the samples exposed to orange juice, followed by those exposed to the blackcurrant drink, while exposure to water led to the same values as unexposed areas. A one-way ANOVA showed a statistically significant difference between the changes in hardness for the drinks at a 95% confidence level (p = 0.0000), while a Kruskal-Wallis test proved a statistically significant difference between the changes in the reduced Young's modulus at a 95% confidence level (p = 0.0000). Thus, it was possible to detect differences in demineralisation potential in an in situ study at a very early stage. Further investigations with greater subject numbers and a larger quantity of samples are necessary to fully evaluate the potential of this method. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:456 / 467
页数:12
相关论文
共 50 条
  • [31] Nanoindentation creep behavior of human enamel
    He, Li-Hong
    Swain, Michael V.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2009, 91A (02) : 352 - 359
  • [32] Mechanical Properties of U-Cu Intermetallic Compound Measured by Nanoindentation
    Li, Ruiwen
    Mo, Chuan
    Liao, Yichuan
    MATERIALS, 2018, 11 (11):
  • [33] MICRO-MECHANICAL PROPERTIES OF CEMENT AND SLAG COMPOSITES MEASURED BY NANOINDENTATION
    Nemecek, Jiri
    Nemecek, Jiri
    NANO & MACRO MECHANICS (NMM 2019), 2020, 26 : 45 - 49
  • [34] Mechanical properties of OI type III bone tissue measured by nanoindentation
    Fan, Zaifeng
    Smith, Peter A.
    Eckstein, Eugene C.
    Harris, Gerald F.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2006, 79A (01) : 71 - 77
  • [35] A review on the mechanical properties of cement-based materials measured by nanoindentation
    Hu, Chuanlin
    Li, Zongjin
    CONSTRUCTION AND BUILDING MATERIALS, 2015, 90 : 80 - 90
  • [36] The mechanical properties of float glass surfaces measured by nanoindentation and acoustic microscopy
    Goodman, Oriel
    Derby, Brian
    ACTA MATERIALIA, 2011, 59 (04) : 1790 - 1799
  • [37] Anisotropic properties of human tibial cortical bone as measured by nanoindentation
    Fan, Z
    Swadener, JG
    Rho, JY
    Roy, ME
    Pharr, GM
    JOURNAL OF ORTHOPAEDIC RESEARCH, 2002, 20 (04) : 806 - 810
  • [38] Evaluation of mechanical properties in nanometer scale using AFM-based nanoindentation tester
    Natl. Research Institute for Metals, 1-2-1 Sengen, Ibaraki 305-0047, Japan
    Nanostruct Mater, 5 (1049-1052):
  • [39] Effect of AFM Nanoindentation Loading Rate on the Characterization of Mechanical Properties of Vascular Endothelial Cell
    Wang, Lei
    Tian, Liguo
    Zhang, Wenxiao
    Wang, Zuobin
    Liu, Xianping
    MICROMACHINES, 2020, 11 (06)
  • [40] Mechanical characterisation of human cartilage cells by AFM nanoindentation under different loading frequencies
    Hu, Kexiang
    Sun, Limin
    Wang, Qingkang
    International Journal of Nanomanufacturing, 2014, 10 (5-6) : 500 - 512