Effect of ageing on the mechanical behaviour of a novel automotive grade Al-Mg-Si alloy

被引:7
|
作者
Ramesh, Raghav [1 ,2 ]
Bhattacharya, R. [2 ,3 ]
Williams, G. [2 ]
机构
[1] Indian Inst Technol, Sch Mech Sci, Bhubaneswar 751013, Orissa, India
[2] Univ Warwick, WMG, Coventry CV4 7AL, W Midlands, England
[3] Univ Strathclyde, Adv Forming Res Ctr, Glasgow PA4 9LJ, Lanark, Scotland
关键词
Aluminium alloys; Age hardening; Hardness measurement; Electron microscopy; Fracture; DEFORMATION-BEHAVIOR; HARDENING BEHAVIOR; PRECIPITATION; AA6111; TEMPERATURE; STRENGTH; FRACTURE;
D O I
10.1016/j.msea.2012.02.013
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The ageing behaviour of a novel Al-Mg-Si alloy AA6014 is studied against AA6111 using hardness and tensile tests. Three conditions were adopted in the tests - natural ageing (T4), artificial ageing (T6) and artificial ageing after pre-natural ageing (T4 followed by T6). The effect of ageing on edge-cracking through hole-expansion test, work hardening potential and fractography has also been studied. The ageing pattern of AA6014 is found to be similar to that of AA6111, but the effect is less severe as observed through lower values of hardness and strength at various ageing conditions. At peak aged condition, the Vickers hardness of AA6014 is 15% less than that of AA6111, whilst the ultimate tensile strength and yield strength of AA6014 are 19% and 13% lower than that of AA6111, respectively. Also, the time taken to attain peak ageing is lower in AA6014 compared to AA6111. The natural ageing prior to artificial ageing is found to have a significant effect on ageing response at shorter ageing times, whilst it is negligible at higher ageing times. The hole-expansion ratio of the two alloys are comparable at higher ageing times, whilst it is higher for AA6014 in as-quenched condition and lower ageing times. The work hardening rate of AA6014 also showed similar pattern as AA6111 and its values, lower than AA6111. The fractography supplemented the tensile test results. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:128 / 134
页数:7
相关论文
共 50 条
  • [21] Annealing on Anisotropy and Mechanical Properties of an Al-Mg-Si Alloy
    Yan, Li-Zhen
    Zhang, Yong-An
    Xiong, Bai-Qing
    Li, Zhi-Hui
    Li, Xi-Wu
    Liu, Hong-Wei
    Huang, Shu-Hui
    Yan, Hong-Wei
    Wen, Kai
    THERMEC 2018: 10TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2018, 941 : 1077 - 1082
  • [22] A study on the mechanical properties of cryorolled Al-Mg-Si alloy
    Panigrahi, Sushanta Kumar
    Jayaganthan, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 480 (1-2): : 299 - 305
  • [23] THE EFFECT OF IRON ON THE PRECIPITATION IN AN AL-MG-SI ALLOY
    SCHMIDT, U
    JOACHIMI, M
    PETZOLD, L
    EICHHORN, F
    CRYSTAL RESEARCH AND TECHNOLOGY, 1984, 19 (07) : 981 - 989
  • [24] Effect of cryorolling on microstructure of Al-Mg-Si alloy
    Panigrahi, Sushanta Kumar
    Jayaganthan, R.
    Chawla, V.
    MATERIALS LETTERS, 2008, 62 (17-18) : 2626 - 2629
  • [25] The effect of pre-ageing and addition of copper on the precipitation behaviour in Al-Mg-Si alloys
    Morley, A. I.
    Zandbergen, M. W.
    Cerezo, A.
    Smith, G. D. W.
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 543 - 548
  • [26] Study on Dynamic Mechanical Behavior of Al-Mg-Si Alloy
    陶小旺
    LIU Jibo
    LIU Xianbin
    CHEN Jianbin
    WANG Yonggang
    汪小锋
    Journal of Wuhan University of Technology(Materials Science), 2024, 39 (02) : 454 - 462
  • [27] Study on Dynamic Mechanical Behavior of Al-Mg-Si Alloy
    Tao, Xiaowang
    Liu, Jibo
    Liu, Xianbin
    Chen, Jianbin
    Wang, Yonggang
    Wang, Xiaofeng
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2024, 39 (02): : 454 - 462
  • [28] Effect of Mg and Si Content on Microstructure and Property of Al-Mg-Si Alloy
    Ren Z.
    Luo B.
    Zheng Y.
    Gao Y.
    He C.
    Cailiao Daobao/Materials Reports, 2019, 33 (09): : 3072 - 3076
  • [29] Dynamic ageing and the mechanical response of Al-Mg-Si alloy through equal channel angular pressing
    Vaseghi, Majid
    Taheri, Ali Karimi
    Hong, Sun Ig
    Kim, Hyoung Seop
    MATERIALS & DESIGN, 2010, 31 (09) : 4076 - 4082
  • [30] Effect of ceramic particles on precipitation in an Al-Mg-Si alloy with silicon excess during ageing
    Meyruey, Gwenaelle
    Massardier, Veronique
    Perez, Michel
    17TH INTERNATIONAL CONFERENCE ON ALUMINIUM ALLOYS 2020 (ICAA17), 2020, 326