Study on friction characterization and wear-resistance properties of Si3N4 ceramic sliding against different high-temperature alloys

被引:53
|
作者
Huang, Changming [1 ,2 ]
Zou, Bin [1 ,2 ]
Liu, Yanan [1 ,2 ]
Zhang, Shuai [1 ,2 ]
Huang, Chuanzhen [1 ,2 ]
Li, Shasha [3 ]
机构
[1] Shandong Univ, Sch Mech Engn, Ctr Adv Jet Engn Technol CaJET, 17923 Jing Shi Rd, Jinan 250061, Peoples R China
[2] Shandong Univ, Minist Educ, Key Lab High Efficiency & Clean Mech Manufacture, Jinan, Peoples R China
[3] Shandong Special Equipment Inspect Inst, Jinan 250013, Peoples R China
基金
中国国家自然科学基金;
关键词
Si3N4; ceramic; Friction coefficient; Wear-resistance; High-temperature alloy; SILICON-NITRIDE; TRIBOLOGICAL BEHAVIOR; STEEL; CONTACT;
D O I
10.1016/j.ceramint.2016.08.013
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ball-on-disc tests were performed to investigate the tribological behaviour of Si3N4 in contact with various high-temperature alloys, under dry sliding conditions, at different sliding speed, load and temperature. The tribological behaviour was characterized in terms of the friction coefficient and wear rate. The friction coefficient of Si3N4 sliding against high-temperature alloys was initially increased to a peak value and then decreased with the further increase of sliding speed. When Si3N4 slides against cobalt based high-temperature alloy (GH605) the friction coefficient and wear rate was the lowest. The smallest friction coefficient was attributed to the powder like wear debris and the formation of a tribo-layer on the worn surface of Si3N4 and GH605. The primary wear mechanism of Si3N4 sliding against iron and cobalt-based high-temperature alloy was adhesion, while a combination of abrasion and adhesion were considered to be the dominant wear mechanisms in the case of sliding against nickel-based high-temperature alloy at room temperature. At high temperature, the friction coefficient and wear rate were decreased with the increase of temperature. An oxide layer was found on the worn surface of Si3N4 after sliding against high-temperature alloys and the oxidative wear was considered to be the main wear mechanism. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:17210 / 17221
页数:12
相关论文
共 50 条
  • [21] UNLUBRICATED SLIDING WEAR MECHANISM OF FINE CERAMIC SI3N4 AGAINST HIGH-CHROMIUM CAST-IRON
    ZHOU, L
    FANG, L
    WANG, NX
    ZHOU, JE
    TRIBOLOGY INTERNATIONAL, 1994, 27 (05) : 349 - 357
  • [22] WEAR PROPERTIES OF SI3N4 IN ROLLING-SLIDING CONTACT
    AKAZAWA, M
    KATO, K
    WEAR, 1988, 124 (02) : 123 - 132
  • [23] Friction and wear properties of SiC and Si3N4 in emulsion lubrication
    Hironaka, S
    Kawamura, D
    Suzuki, M
    JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2003, 48 (06) : 486 - 493
  • [24] Friction and wear behaviors of Si3N4 sliding against M50 bearing steel in vacuum
    Tong Yongxing
    Wang Liqin
    Gu Le
    MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-5, 2010, 97-101 : 1681 - 1684
  • [25] The Friction and Wear Properties of Si3N4 + SiC Gradient Ceramics
    Chen, Bei
    Cheng, Chuan
    SCIENCE OF ADVANCED MATERIALS, 2017, 9 (3-4) : 321 - 325
  • [26] Friction and wear of self-mated SiC and Si3N4 sliding in water
    Chen, M
    Kato, K
    Adachi, K
    WEAR, 2001, 250 (PART 1) : 246 - 255
  • [27] Effects of antiwear additives on the friction and wear of Si3N4/steel sliding contacts
    Zhao, XZ
    Liu, JJ
    Zhu, BL
    Miao, HZ
    Luo, ZB
    WEAR, 1996, 201 (1-2) : 99 - 105
  • [28] TRIBOLOGICAL CHARACTERISTICS OF SI3N4, CERAMIC IN HIGH-TEMPERATURE AND HIGH-PRESSURE WATER
    KITAOKA, S
    TSUJI, T
    KATOH, T
    YAMAGUCHI, Y
    SATO, K
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (02) : 580 - 588
  • [29] Friction and wear characteristics of SiC and Si3N4 ceramics against ZrO2 ceramic under dry friction
    Tian, X
    Lin, B
    Zhang, WL
    HIGH-PERFORMANCE CERAMICS III, PTS 1 AND 2, 2005, 280-283 : 1319 - 1322
  • [30] HIGH-TEMPERATURE CORROSION OF SIC AND SI3N4
    JACOBSON, NS
    SMIALEK, JL
    FOX, DS
    JOURNAL OF METALS, 1987, 39 (10): : A35 - A35