Fracture and fatigue behavior of WC-Co and WC-CoNi cemented carbides

被引:56
|
作者
Tarrago, J. M. [1 ,2 ]
Roa, J. J. [1 ,2 ]
Valle, V. [1 ]
Marshall, J. M. [3 ]
Llanes, L. [1 ,2 ]
机构
[1] Univ Politecn Cataluna, CIEFMA, Dept Ciencia Dels Mat & Engn Met, ETSEIB, E-08028 Barcelona, Spain
[2] Univ Politecn Cataluna, CRnE, Ctr Recerca Nanoengn, E-08028 Barcelona, Spain
[3] Sandvik Hyper, Coventry CV4 0XG, W Midlands, England
关键词
Fatigue crack growth; Cemented carbides; Crack deflection; Fractography; Alternative binders; CRACK-GROWTH-BEHAVIOR; HARD METALS; MECHANICAL-PROPERTIES; BINDER PHASE; HARDMETALS; CERMETS; MICROSTRUCTURE; DEFORMATION;
D O I
10.1016/j.ijrmhm.2014.07.027
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The fracture and fatigue characteristics of several cemented carbide grades are investigated as a function of their microstructure. In doing so, the influence of binder chemical nature and content (Co and 76 wt.% Co-24 wt.% Ni), as well as carbide grain size on hardness, flexural strength, fracture toughness and fatigue crack growth (FCG) behavior is evaluated. Mechanical testing is combined with a detailed inspection of crack-microstructure interaction, by means of scanning electron microscopy, in order to evaluate crack-path tortuosity and to discern fracture and fatigue micromechanisms within the metallic binder. Results show that CoNi-base hardmetals exhibit slightly lower hardness but higher toughness values than Co-base grades. Meanwhile, flexural strength is found to be rather independent of the binder chemical nature. Regarding FCG behavior, experimental results indicate that: (1) FCG threshold (K-th) values for coarse-grained grades are higher than those measured for the medium-grained ones; and (2) fatigue sensitivity levels exhibited by CoNi- and Co-base cemented carbides, for a given binder mean free path, are similar. These findings are rationalized on the basis of the increasing relevance of crack deflection mechanisms as microstructure gets coarser and the evidence of similar fatigue degradation phenomena within the binder independent of its chemical nature, respectively. (C) 2014 Elsevier Ltd. All rights reserved.
引用
下载
收藏
页码:184 / 191
页数:8
相关论文
共 50 条
  • [12] GRINDING OF WC-CO CEMENTED CARBIDES
    ZELWER, O
    MALKIN, S
    JOURNAL OF ENGINEERING FOR INDUSTRY-TRANSACTIONS OF THE ASME, 1980, 102 (03): : 209 - 220
  • [13] Complexions in WC-Co cemented carbides
    Liu, Xingwei
    Song, Xiaoyan
    Wang, Haibin
    Liu, Xuemei
    Tang, Fawei
    Lu, Hao
    ACTA MATERIALIA, 2018, 149 : 164 - 178
  • [14] GRINDING OF WC-CO CEMENTED CARBIDES
    ZELWER, O
    MALKIN, S
    INDUSTRIAL DIAMOND REVIEW, 1980, (APR): : 133 - 139
  • [15] Three-point bending fatigue behavior of WC-Co cemented carbides
    Li, Anhai
    Zhao, Jun
    Wang, Dong
    Gao, Xinliang
    Tang, Hongwei
    MATERIALS & DESIGN, 2013, 45 : 271 - 278
  • [16] Mechanisms of fatigue crack growth in WC-Co cemented carbides
    Boo, MH
    Park, CY
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 1120 - 1125
  • [17] Heat treatment of WC-Co cemented carbides
    Liu, Shourong
    Jinshu Rechuli Xuebao/Transactions of Metal Heat Treatment, 1988, 9 (02): : 30 - 36
  • [18] Magnetism Study of WC-Co Cemented Carbides
    刘寿荣
    Rare Metals, 1993, (04) : 305 - 307
  • [19] Evaluation of fatigue crack growth characteristics of WC-Co cemented carbides
    Kanazawa Univ, Kanazawa, Japan
    Zairyo, 7 (726-731):
  • [20] Characteristics and applications of WC-Co cemented carbides
    Usami, H
    JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2004, 49 (07) : 547 - 552