A 3.7 MHz phased array probe using 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 single crystal

被引:59
|
作者
Saitoh, S [1 ]
Takeuchi, T
Kobayashi, T
Harada, K
Shimanuki, S
Yamashita, Y
机构
[1] Toshiba Corp, Ctr Res & Dev, Mat Lab, Kawasaki, Kanagawa 2108582, Japan
[2] Toshiba Corp, Ctr Res & Dev, Device Res Lab, Kawasaki, Kanagawa 2108582, Japan
[3] Toshiba Corp, Nasu Works, Otawara 3248850, Japan
关键词
D O I
10.1109/58.753031
中图分类号
O42 [声学];
学科分类号
070206 ; 082403 ;
摘要
A novel 128-channel phased array probe for echocardiography with a center frequency of 3.7 MHz using 0.91Pb(Zn1/3Nb2/3)O-3-0.09PbTiO(3) (PZN-9%PT) single crystal has been fabricated to realize greater sensitivity and broader bandwidth properties. The echo amplitude of the PZN-9%PT single-crystal probe is about 5 dB higher than that of the conventional lead zirconate titanate (PZT) ceramic probe, and the fractional bandwidth is about 25 percentage points broader. The quality of B mode images obtained by the PZN-9%PT probe satisfies the performance of the two types of conventional PZT ceramic probes that have center frequencies of 2.5 and 3.75 MHz. At the reference frequency of 3 MHz, the Doppler sensitivity of the PZN-9%PT probe is about 5 dB higher than that of the 3.75 MHz PZT probe; the blood flow of a pulmonary vein in a hard-to-image patient is much more clearly imaged than in the case of using the PZT probe. These superior images are attributable to the use of sufficiently large PZN-9%PT single crystals obtained by the serf-flux method.
引用
收藏
页码:414 / 421
页数:8
相关论文
共 50 条
  • [21] Investigation of intrinsic defect structure in 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 single crystal through AC conductivity
    James, AR
    Priya, S
    Uchino, K
    Srinivas, K
    Kiran, VV
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2002, 41 (08): : 5272 - 5276
  • [22] Orientation effects on the bandgap and dispersion behavior of 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 single crystals
    赫崇君
    付信夺
    徐峰
    王吉明
    朱孔军
    杜朝玲
    刘友文
    Chinese Physics B, 2012, 21 (05) : 264 - 268
  • [23] Investigation of intrinsic defect structure in 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 single crystal through AC conductivity
    James, Ajit R.
    Priya, Shashank
    Uchino, Kenji
    Srinivas, Kuchipudi
    Kiran, Vemuri V.
    1600, Japan Society of Applied Physics (41):
  • [24] Double hysteresis loops in 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 near the ferroelectric critical endpoint
    Iwata, Makoto
    Kaiden, Yasutaka
    Takikawa, Yoshinori
    Ishibashi, Yoshihiro
    FERROELECTRICS, 2018, 533 (01) : 139 - 144
  • [25] Irreversible phase transition characteristic of 0.91Pb(Zn1/3Nb2/3) O3-0.09PbTiO3 single crystals by domain observation
    Zhu, Rongfeng
    Zhang, Qihui
    Fang, Bijun
    Ding, Jianning
    Zhao, Xiangyong
    Luo, Haosu
    CURRENT APPLIED PHYSICS, 2016, 16 (12) : 1703 - 1707
  • [26] Tetragonal micro/nanotwins in 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 revealed by reciprocal space mapping
    Chang, W. S.
    Lim, L. C.
    Yang, P.
    Miao, H.
    Tu, C. -S.
    Chen, Qiming
    Soh, A. K.
    APPLIED PHYSICS LETTERS, 2009, 94 (20)
  • [27] SOL-GEL PROCESSING OF 0.91PB(ZN1/3NB2/3)O3-0.09PBTIO3 - STABILIZATION OF THE PEROVSKITE PHASE
    HAYES, JM
    GURURAJA, TR
    GEOFFROY, GL
    CROSS, LE
    MATERIALS LETTERS, 1987, 5 (10) : 396 - 400
  • [28] Study on crystal growth and electrical properties of relaxor-based ferroelectric single crystal 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3
    Fang, BJ
    Luo, HS
    Wu, YJ
    Xu, HQ
    Yin, ZW
    ACTA CHIMICA SINICA, 2001, 59 (09) : 1430 - 1434
  • [29] Fabrication and electrical properties of grain-oriented 0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 ceramics
    Cheng, W. X.
    He, X. Y.
    Sun, D. Z.
    Zheng, X. S.
    Qiu, P. S.
    OPTOELECTRONIC MATERIALS, PTS 1AND 2, 2010, 663-665 : 555 - +
  • [30] Phased array ultrasonic probe using Pb(Zn1/3Nb2/3)O3-PbTiO3 single crystal
    Saitoh, S
    Kobayashi, T
    Harada, K
    Shimanuki, S
    Yamashita, Y
    ULTRASONIC TRANSDUCER ENGINEERING: MEDICAL IMAGING 1998, 1998, 3341 : 264 - 271