Corrosion resistance of Ni-50Cr HVOF coatings on 310S alloy substrates in a metal dusting atmosphere

被引:4
|
作者
Saaedi, J. [1 ,2 ]
Arabi, H. [2 ]
Coyle, T. W. [1 ]
Mirdamadi, S. [2 ]
Ghorbani, H. [2 ]
机构
[1] Univ Toronto, Ctr Adv Coating Technol, Dept Mat Sci & Engn, Toronto, ON M5S 3E4, Canada
[2] Iran Univ Sci & Technol, Dept Mat & Met Engn, Tehran, Iran
来源
关键词
NICKEL-BASE ALLOYS; MECHANISMS; OXIDATION; BEHAVIOR; STEEL; CO2;
D O I
10.1002/maco.200905536
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Metal dusting attack has been examined after three 168 h cycles on two Ni-50Cr coatings with different microstructures deposited on 310S alloy substrates by the high velocity oxy-fuel (HVOF) thermal-spray process. Metal dusting in uncoated 310S alloy specimens was found to be still in the initiation stage after 504 h of exposure in the 50H(2):50CO gas environment at 620 degrees C. Dense Ni-50Cr coatings offered suitable resistance to metal dusting. Metal dusting was observed in the 310S substrates adjacent to pores at the interface between the substrate and a porous Ni-50Cr coating. The porosity present in the as-deposited coatings was shown to introduce a large variability into coating performance. Carbon formed by decomposition of the gaseous species accumulated in the surface pores and resulted in the dislodgement of surface splats due to stresses generated by the volume changes. When the corrosive gas atmosphere was able to penetrate through the interconnected pores and reach the coating-substrate interface, the 310S substrate was carburized, metal dusting attack occurred, and the resulting formation of coke in the pores led to local failure of the coating.
引用
收藏
页码:823 / 835
页数:13
相关论文
共 33 条
  • [31] Effect of TiB2 content on the microstructure, corrosion behavior, and wear resistance of (Fe 50 Mn 30 Co 10 Cr 10 ) 0.8-x (TiB2)x Mo 0.2 high-entropy alloy coatings by laser cladding
    Geng, Jiaye
    Yang, Xiaohui
    Wang, Guicheng
    Yin, Ming
    Li, Jucai
    Li, Yan
    SURFACE & COATINGS TECHNOLOGY, 2025, 496
  • [32] GAS-METAL REACTIONS OF A NEW Fe-Ni-Cr-W ALLOY IN HELIUM WITH REACTIVE COMPONENTS AND IN AN H2-CH4-H2S ATMOSPHERE IN THE TEMPERATURE RANGE 700-950 degree C.
    Huchtemann, Bernd
    Schueler, Peter
    1600, (87):
  • [33] Effect of TiB2 content on the microstructure, corrosion behavior, and wear resistance of (Fe50Mn30Co10Cr10)0.8-x (TiB2)x Mo0.2 high-entropy alloy coatings by laser cladding (vol 496, 131662, 2025)
    Geng, Jiaye
    Yang, Xiaohui
    Wang, Guicheng
    Yin, Ming
    Li, Jucai
    Li, Yan
    SURFACE & COATINGS TECHNOLOGY, 2025, 501